Patent US4713105A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4713105A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for glass fiber splicing by flame fusion

Assignee: Nokia Bell Labs
•
Filing: 1986-11-25
•
Granted: 1987-12-15
•
Expires: 2006-11-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In the interest of producing high-strength splice connections between silica-based glass fibers a method of using a tri-particle flow of gases for flame fusion is disclosed. An outer relatively high-velocity flow of oxygen surrounds an intermediate, lower-velocity flow of chlorine or oxygen which in turn surrounds a central flow of H 2 , D 2 , NH 3 , or ND 3 . Particularly high strengths are achieved when a central flow of hydrogen or deuterium and an intermediate flow of chlorine are used in such a fashion as to heat fiber ends to be spliced to temperatures of 500 degrees C. and beyond only after these ends have been enveloped by chlorine.

Inventors

  • 👤 John T. Krause
  • 👤 Charles R. Kurkjian
  • 👤 Un-Chul Paek

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 17:17
CPC Classifications
G; G02; G02B; G02B6/00; G02B6/24; G02B6/255; G02B6/2551

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 264 words
Method for making a glass fiber which here is designated as a spliced fiber, said method comprising a step of connecting at least a first glass fiber and a second glass fiber, said first and said second glass fibers comprising respective surface portions which consist of at least 95 weight percent silica, said step of connecting comprising heating an end portion of said first fiber and an end portion of said second fiber while said end portion of said first fiber is in contact and essentially aligned with said end portion of said second fiber, said heating being in a flame which results upon combustion in a flow of gases, said flow comprising an outer flow portion, an intermediate flow portion which is interior to said outer flow portion, and central flow portion which is interior to said intermediate flow portion, said outer flow portion comprising at least 50 percent by volume oxygen, said intermediate flow portion consisting essentially of chlorine, said central flow portion consisting essentially of hydrogen or deuterium, the velocity of the flow of said outer flow portion being greater than the velocity of the flow of said intermediate flow portion so as to render said flame more narrow and so as to cool the fiber away from said end portions, and central flow being kept low during placement of fiber such that fiber end temperature is less than or equal to 500 degrees C. up until fiber ends are within said intermediate flow, whereby said spliced fiber has a tensile strength which is at least 95 percent of pristine strength.
Claim 2
Dependent Claim 264 words
Method for making a glass fiber which here is designated as a spliced fiber, said method comprising a step of connecting at least a first glass fiber and a second glass fiber, said first and said second glass fibers comprising respective surface portions which consist of at least 95 weight percent silica, said step of connecting comprising heating an end portion of said first fiber and an end portion of said second fiber while said end portion of said first fiber is in contact and essentially aligned with said end portion of said second fiber, said heating being in a flame which results upon combustion in a flow of gases, said flow comprising an outer flow portion, an intermediate flow portion which is interior to said outer flow portion, and central flow portion which is interior to said intermediate flow portion, said outer flow portion comprising at least 50 percent by volume oxygen, said intermediate flow portion consisting essentially of chlorine, said central flow portion consisting essentially of hydrogen or deuterium, the velocity of the flow of said outer flow portion being greater than the velocity of the flow of said intermediate flow portion so as to render said flame more narrow and so as to cool the fiber away from said end portions, and central flow being kept low during placement of fiber such that fiber end temperature is less than or equal to 500 degrees C. up until fiber ends are within said intermediate flow, whereby said spliced fiber has a tensile strength which is at least 95 percent of pristine strength.
Claim 3
Dependent Claim 30 words
Method of claim 1 in which the velocity of the flow of said outer flow portion is at least twice the velocity of the flow of said intermediate flow portion.
Claim 4
Dependent Claim 27 words
Method of claim 1 in which a flow rate is achieved in said outer flow portion which is greater than or equal to 5 meters per second.
Claim 5
Dependent Claim 27 words
Method of claim 1 in which a flow rate is achieved in said intermediate flow portion which is greater than or equal to 0.1 meters per second.
Claim 6
Dependent Claim 27 words
Method of claim 4 in which a flow rate is achieved in said intermediate flow portion which is less than or equal to 1 meter per second.
Claim 7
Dependent Claim 38 words
Method of claim 1 in which flow rate in said central flow portion is adjusted such that the temperature of said first end portion and said second end portion is less than or equal to 1800 degrees C.

References Cited (Backward Citations)

US3791714A Cited
US4118618A Cited
US4345137A Cited
GB2054553A Cited
US4326870A Cited
US4604119A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-12-14 1991-06-15 1991-12-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-12-14 1995-06-15 1995-12-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-12-14 1999-06-15 1999-12-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag