Abstract

Abstract Automotive ignition wire with a high temperature rating, excellent electrical insulating properties, heat resistance, oil resistance and abrasion resistance is described. The wire utilizes a conductor made up of a glass fiber-cotton fiber braid on a graphite impregnated glass layer. Overcoating the conductor is an adhesion promoting polymer layer, an extruded thermosetting semiconducting polymer layer overcoated with a glass braid layer and a polymer jacket material. The polymer jacket material comprises a polymeric mixture of ethylene vinyl acetate and ethylene-propylene-diene monomer stabilized with a mixture of a phenolic antioxidant and a metal salt antioxidant.

Inventors

  • 👤 Ronald J. Coffey
  • 👤 Christo M. Wassouf

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 18:12
CPC Classifications
H; H01; H01B; H01B7/00; H01B7/0063; H01B7/17; H01B7/29

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 75 words
Electrically conductive ignition wire comprising a graphite impregnated glass fiber core overbraided with a glass and cotton fiber braid, which is overcoated with an adhesion promoting polymer layer, an extruded layer of thermosetting semiconducting polymer, and a polymer jacket layer extruded over the thermosetting semiconducting polymer layer, the polymer jacket comprising a mixture of ethylene-propylene-diene monomer containing polymer with ethylene vinyl acetate stabilized with a mixture of a phenolic antioxidant and a metal salt antioxidant.
Claim 2
Dependent Claim 75 words
Electrically conductive ignition wire comprising a graphite impregnated glass fiber core overbraided with a glass and cotton fiber braid, which is overcoated with an adhesion promoting polymer layer, an extruded layer of thermosetting semiconducting polymer, and a polymer jacket layer extruded over the thermosetting semiconducting polymer layer, the polymer jacket comprising a mixture of ethylene-propylene-diene monomer containing polymer with ethylene vinyl acetate stabilized with a mixture of a phenolic antioxidant and a metal salt antioxidant.
Claim 3
Dependent Claim 45 words
The wire of claim 1 wherein the ethylene vinyl acetate polymer contains 40% by weight vinyl acetate and the antioxidant mixture is present in an amount of about 3.5% by weight and the weight ratio of phenolic antioxidant to metal salt antioxidant is about 1:2.
Claim 4
Dependent Claim 16 words
The wire of claim 2 wherein the thermosetting semiconducting polymer layer is a methyl vinyl silicone.
Claim 5
Independent Claim 82 words
The method of making electrically conductive ignition wire comprising overbrading a graphite impregnated glass fiber core with a glass and cotton fiber braid, overcoating the braid with an adhesion promoting polymer layer, extruding a layer of thermosetting semiconducting polymer on the adhesion promoting polymer layer, extruding a polymer jacket layer over the thermosetting semiconducting polymer layer, the polymer jacket comprising a mixture of ethylene-propylene-diene-monomer containing polymer with ethylene vinyl acetate stabilized with a mixture of phenolic antioxidant and a metal salt antioxidant.
Claim 6
Independent Claim 82 words
The method of making electrically conductive ignition wire comprising overbrading a graphite impregnated glass fiber core with a glass and cotton fiber braid, overcoating the braid with an adhesion promoting polymer layer, extruding a layer of thermosetting semiconducting polymer on the adhesion promoting polymer layer, extruding a polymer jacket layer over the thermosetting semiconducting polymer layer, the polymer jacket comprising a mixture of ethylene-propylene-diene-monomer containing polymer with ethylene vinyl acetate stabilized with a mixture of phenolic antioxidant and a metal salt antioxidant.
Claim 7
Dependent Claim 45 words
The method of claim 4 wherein the ethylene vinyl acetate polymer contains 40% by weight vinyl acetate and the antioxidant mixture is present in an amount of about 3.5% by weight and the weight ratio of phenolic antioxidant to metal salt antioxidant is about 1:2.
Claim 8
Dependent Claim 16 words
The method of claim 5 wherein the thermosetting semiconducting polymer layer is a methyl vinyl silicone.

References Cited (Backward Citations)

US3284751A Cited
US3692925A Cited
US3680027A Cited
US3697670A Cited
US3818412A Cited
US3870987A Cited
US4209425A Cited
US4342880A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-11-02 1991-05-04 1991-11-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-11-02 1995-05-04 1995-11-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-11-02 1999-05-04 1999-11-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag