Abstract

Abstract A method of forming a MIM element for use in liquid crystal displays. The MIM element is formed on a substrate using photolithography with a self-alignment method where one of the metal electrodes forming the MIM element acts as a radiation mask to radiation use in forming the element.

Inventors

  • 👤 Yoichi Ono

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 23:20
CPC Classifications
H; H10; H10N; H10N70/00; G; G02; G02F; G02F1/00; G02F1/01; G02F1/13; G02F1/133; G02F1/136; G02F1/1362; G02F1/1365

Claims Analysis

Total Claims: 29
Claim 1
Independent Claim 146 words
A method of forming a MIM element having a first metal electrode and a second metal electrode with an insulator therebetween in an electro-optic display device having first and second opposed substrates with a liquid crystal material disposed therebetween, said first substrate having at least a first row electrode formed thereon, said second substrate having at least a first column electrode formed thereon, a picture element being defined where said row and column electrodes overlap in top plan view, comprising the step of forming said MIM element having first and second electrodes with an insulator therebetween at the position where said picture element is defined on one of said first and second substrates by a photolithography process using a self-alignment method where the substrate on which said MIM element is formed is exposed from behind with radiation with said first metal electrode acting as a mask.
Claim 2
Independent Claim 146 words
A method of forming a MIM element having a first metal electrode and a second metal electrode with an insulator therebetween in an electro-optic display device having first and second opposed substrates with a liquid crystal material disposed therebetween, said first substrate having at least a first row electrode formed thereon, said second substrate having at least a first column electrode formed thereon, a picture element being defined where said row and column electrodes overlap in top plan view, comprising the step of forming said MIM element having first and second electrodes with an insulator therebetween at the position where said picture element is defined on one of said first and second substrates by a photolithography process using a self-alignment method where the substrate on which said MIM element is formed is exposed from behind with radiation with said first metal electrode acting as a mask.
Claim 3
Dependent Claim 59 words
The method as claimed in claim 1, wherein said second metal electrode is formed by a photolithography process using a self-alignment method in which a negative-type photo resist is coated on said second metal electrode, said substrate on which said MIM element is formed being exposed from behind with radiation with said first metal electrode acting as a mask.
Claim 4
Dependent Claim 17 words
The method as claimed in claim 1, wherein said insulator is formed on said first metal electrode.
Claim 5
Dependent Claim 27 words
The method as claimed in claim 1, wherein said insulator is formed substantially over the entire surface of the substrate on which said MIM element is formed.
Claim 6
Dependent Claim 23 words
The method as claimed in claim 1, wherein said second metal electrode includes a transparent electrode as a picture element electrode formed thereon.
Claim 7
Dependent Claim 21 words
The method as claimed in claim 1, wherein said second metal electrode is transparent to serve as a picture element electrode.
Claim 8
Dependent Claim 38 words
The method as claimed in claim 1, wherein said second metal electrode is formed using a self-alignment method with a photo mask being disposed on the rear surface of the substrate on which said MIM element is formed.
Claim 9
Dependent Claim 49 words
The method as claimed in claim 1, wherein said second metal electrode is formed by a photolithography process using a self-alignment method, said substrate on which said MIM element is formed being exposed from behind with radiation with said first metal electrode acting as a mask through said insulator.
Claim 10
Dependent Claim 30 words
The method as claimed in claim 1, wherein said first electrode includes a side face portion, said MIM element being formed at said side face portion by a self-alignment method.
Claim 11
Dependent Claim 21 words
The method as claimed in claim 1, wherein said MIM element is formed at only one portion of said first electrode.
Claim 12
Dependent Claim 38 words
The method as claimed in claim 5, wherein an electrode in a desired shape and a picture element electrode are simultaneously formed using a self-alignment method with a photomask being disposed on the rear surface of said substrate.
Claim 13
Dependent Claim 22 words
The method as claimed in claim 1, wherein said first metal electrode is formed on one of said row and column electrodes.
Claim 14
Dependent Claim 22 words
The method as claimed in claim 6, wherein said first metal electrode is formed on one of said row and column electrodes.
Claim 15
Independent Claim 97 words
A method of forming a MIM element on a substrate having first and second sides for use in a liquid crystal display device comprising the steps of forming a first electrode metal film in a predetermined pattern on the first side of said substrate, forming an insulator over said first electrode metal film, forming a second electrode metal film over said insulator, applying a photo resist over said second electrode metal film, and exposing said second side of said substrate to radiation, said first electrode metal film acting as a radiation mask when said radiation is applied.
Claim 16
Independent Claim 97 words
A method of forming a MIM element on a substrate having first and second sides for use in a liquid crystal display device comprising the steps of forming a first electrode metal film in a predetermined pattern on the first side of said substrate, forming an insulator over said first electrode metal film, forming a second electrode metal film over said insulator, applying a photo resist over said second electrode metal film, and exposing said second side of said substrate to radiation, said first electrode metal film acting as a radiation mask when said radiation is applied.
Claim 17
Dependent Claim 12 words
The method as claimed in claim 14, wherein said substrate is glass.
Claim 18
Dependent Claim 29 words
The method as claimed in claim 14, wherein said first electrode metal film is formed from a metal selected from the group consisting of Al, Ni, Cr and Ta.
Claim 19
Dependent Claim 24 words
The method as claimed in claim 16, wherein the thickness of said first electrode metal film is substantially in the range of 1000 Å-1μ.
Claim 20
Dependent Claim 19 words
The method as claimed in claim 17, wherein said metal is Al having a thickness of about 2000 Å.
Claim 21
Dependent Claim 23 words
The method as claimed in claim 17, wherein said metal is Ta having a thickness substantially in the range of 3000 Å-6000 Å.
Claim 22
Dependent Claim 36 words
The method as claimed in claim 14, wherein second electrode metal film is formed from a metal selected from the group consisting of Cr, Al, and NiCr having a film thickness less than about 200 Å.
Claim 23
Dependent Claim 21 words
The method as claimed in claim 20, wherein the thickness of said second electrode metal film in less than 100 Å.
Claim 24
Dependent Claim 25 words
The method as claimed in claim 21, wherein the thickness of said second electrode metal film is substantially in the range of 40 Å-60 Å.
Claim 25
Dependent Claim 19 words
The method as claimed in claim 14, wherein said second electrode metal film serves as a picture element electrode.
Claim 26
Dependent Claim 28 words
The method as claimed in claim 23, wherein said second electrode metal film is made from a member of the group consisting of ITO, SnO 2 and ZnO.
Claim 27
Dependent Claim 23 words
The method as claimed in claim 24, wherein said member is ITO having a thickness substantially in the range of 100 Å-2000 Å.
Claim 28
Dependent Claim 21 words
The method as claimed in claim 25, wherein said member has a thickness substantially in the range of 200 Å-800 Å.
Claim 29
Dependent Claim 33 words
The method as claimed in claim 14, wherein said insulator is made from a member of the group consisting of SiO 2 , Cr 2 O 5 and Ta 2 O 5 .

References Cited (Backward Citations)

JPS5734520A Cited
US4523811A Cited
JPS58181023A Cited
JPS58184119A Cited
US4534623A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-07-27 1991-01-26 1991-07-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-07-27 1995-01-26 1995-07-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-07-27 1999-01-26 1999-07-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag