Patent US4675120A successfully refreshed from Google Patents.
US4675120A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Methods of using strong acids modified with acid solutions
Assignee: AN-SON PETROCHEMICAL Inc A CORP OF FL
•
Filing: 1983-07-14
•
Granted: 1987-06-23
•
Expires: 2003-07-14
Abstract
Abstract Acidic compositions comprising mixtures of hydrochloric, phosphoric, oxalic and citric acids, optionally additionally containing oleic, hydrofluoric or sulfuric acid and methods of preparing the acidic mixtures. Uses for certain mixtures of the acids include treating crude oil, in oil recovery processes, for well acidizing, cleaning glass, in batteries, removing corrosion from metals, removing oil residues from oil handling equipment and reactivating wells clogged with asphaltene.
Inventors
- 👤 David J. Martucci
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-05 18:20
CPC Classifications
H; H01; H01M; H01M10/00; H01M10/06; H01M10/08; C; C03; C03C; C03C23/00; C03C23/0075; C09; C09K; C09K8/00; C09K8/54; C09K8/60; C09K8/62; C09K8/72; C10; C10G; C10G17/00; C10G17/02; C10G17/04; C23; C23G; C23G1/00; C23G1/02; E; E21; E21B; E21B37/00; E21B37/06; Y; Y02; Y02E; Y02E60/00; Y02E60/10; Y10; Y10S; Y10S507/00; Y10S507/933
Claims Analysis
Total Claims: 13
Claim 1
Independent Claim
185 words
A method for acidizing wells surrounded by clay or silicate formations, said method comprising the steps of: (a) mixing water and hydrochloric acid with relatively smaller amounts of phosphoric, oxalic and citric acids and urotropine to form a first solution, said hydrochloric acid present in said first solution having a concentration of 1-60 percent by weight of said first solution, said phosphoric acid present in said first solution having a concentration of 0.2 percent by weight of said first solution, said oxalic acid present in said first solution having a concentration of 0.1-10 percent by weight of said first solution and said citric acid present in said first solution having a concentration of 0.1-25 percent by weight of said first solution; (b) forming a second solution by mixing a portion of said first solution with additional hydrochloric acid; (c) forming a third solution by mixing the remaining portion of said first solution with hydroflouric acid; (d) forming a fourth solution by mixing said second and third solutions; and (e) introducing said fourth solution into the well and into contact with the clay or silicate formations.
Claim 2
Independent Claim
185 words
A method for acidizing wells surrounded by clay or silicate formations, said method comprising the steps of: (a) mixing water and hydrochloric acid with relatively smaller amounts of phosphoric, oxalic and citric acids and urotropine to form a first solution, said hydrochloric acid present in said first solution having a concentration of 1-60 percent by weight of said first solution, said phosphoric acid present in said first solution having a concentration of 0.2 percent by weight of said first solution, said oxalic acid present in said first solution having a concentration of 0.1-10 percent by weight of said first solution and said citric acid present in said first solution having a concentration of 0.1-25 percent by weight of said first solution; (b) forming a second solution by mixing a portion of said first solution with additional hydrochloric acid; (c) forming a third solution by mixing the remaining portion of said first solution with hydroflouric acid; (d) forming a fourth solution by mixing said second and third solutions; and (e) introducing said fourth solution into the well and into contact with the clay or silicate formations.
Claim 3
Dependent Claim
32 words
A method as set forth in claim 1, wherein said step of forming said second solution includes mixing equal parts of said portion of said first solution and said additional hydrochloric acid.
Claim 4
Dependent Claim
32 words
A method as set forth in claim 1, wherein said step of forming said third solution includes mixing equal parts of said remaining portion of said first solution and said hydroflouric acid.
Claim 5
Dependent Claim
79 words
A method as set forth in claim 1, wherein said step of forming said first solution includes mixing water at a concentration of 67.25 percent by weight and hydrochloric acid at a concentration of 21 percent by weight with phosphoric acid at a concentration of 5.28 percent by weight, oxalic acid at a concentration of 0.95 percent by weight, citric acid at a concentration of 1.92 percent by weight and urotropine at a concentration of 3.6 percent by weight.
Claim 6
Independent Claim
132 words
A method as set forth in claims 1, 2 or 3, wherein said step of forming said first solution includes the steps of mixing said hydrochloric and phosphoric acids in a first reactor, dissolving said oxalic acid in a portion of said water in a second reactor, combining the contents of said first reactor and said second reactor while simultaneously dissolving said citric acid therein, adding the remaining portion of said water to the combined contents of said first reactor and said second reactor following solubilization of said citric acid, dissolving said urotropine in a portion of the combined contents of said first and second reactors and said solubilized citric acid and adding thereto the remaining portion of the combined contents of said first and second reactors and said solubilized citric acid.
Claim 7
Dependent Claim
32 words
A method as set forth in claim 1 wherein said fourth solution is introduced into the well and into contact with the clay or silicate formations at temperatures below approximately 160° F.
Claim 8
Independent Claim
151 words
A method for acidizing wells surrounded by calcareous formations, said method comprising the steps of: (a) mixing water and hydrochloric acid with relatively smaller amounts of phosphoric, oxalic and citric acids and urotropine to form a first solution, said hydrochloric acid present in said first solution having a concentration of 1-60 percent by weight of said first solution, said phosphoric acid present in said first solution having a concentration of 0.2-60 percent by weight of said first solution, said oxalic acid present in said first solution having a concentration of 0.1-10 percent by weight of said first solution and said citric acid present in said first solution having a concentration of at least 0.1 percent by weight of said first solution; (b) forming a second solution by mixing said first solution with additional hydrochloric acid; and (c) introducing said second solution into the well and into contact with the calcareous formations.
Claim 9
Independent Claim
151 words
A method for acidizing wells surrounded by calcareous formations, said method comprising the steps of: (a) mixing water and hydrochloric acid with relatively smaller amounts of phosphoric, oxalic and citric acids and urotropine to form a first solution, said hydrochloric acid present in said first solution having a concentration of 1-60 percent by weight of said first solution, said phosphoric acid present in said first solution having a concentration of 0.2-60 percent by weight of said first solution, said oxalic acid present in said first solution having a concentration of 0.1-10 percent by weight of said first solution and said citric acid present in said first solution having a concentration of at least 0.1 percent by weight of said first solution; (b) forming a second solution by mixing said first solution with additional hydrochloric acid; and (c) introducing said second solution into the well and into contact with the calcareous formations.
Claim 10
Dependent Claim
34 words
A method as set forth in claim 7, wherein said step of forming said second solution includes mixing said first solution and said additional hydrochloric acid in a ration ranging between 2:8 and 3:7.
Claim 11
Dependent Claim
79 words
A method as set forth in claim 7, wherein said step of forming said first solution includes mixing water at a concentration of 67.25 percent by weight and hydrochloric acid at a concentration of 21 percent by weight with phosphoric acid at a concentration of 5.28 percent by weight, oxalic acid at a concentration of 0.95 percent by weight, citric acid at a concentration of 1.92 percent by weight and urotropine at a concentration of 3.6 percent by weight.
Claim 12
Independent Claim
131 words
A method as set forth in claims 7 or 8, wherein said step of forming said first solution includes the steps of mixing said hydrochloric and phosphoric acids in a first reactor, dissolving said oxalic acid in a portion of said water in a second reactor, combining the contents of said first reactor and said second reactor while simultaneously dissolving said citric acid therein, adding the remaining portion of said water to the combined contents of said first reactor and said second reactor following solubilization of said citric acid, dissolving said urotropine in a portion of the combined contents of said first and second reactors and said solubilized citric acid and adding thereto the remaining portion of the combined contents of said first and second reactors and said solubilized citric acid.
Claim 13
Dependent Claim
30 words
A method as set forth in claim 7 wherein said second solution is introduced into the well and into contact with the calcareous formations at temperatures below approximately 176° F.
References Cited (Backward Citations)
US1990969A
Cited
US3122204A
Cited
US3142335A
Cited
US3505235A
Cited
US3630933A
Cited
US3920566A
Cited
US4101426A
Cited
US4116713A
Cited
US4213866A
Cited
US4371443A
Cited
GB2110744A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1990-06-22 | 1990-12-22 | 1991-06-23 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1994-06-22 | 1994-12-22 | 1995-06-23 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1998-06-22 | 1998-12-22 | 1999-06-23 | $7700.00 | Window Closed / Lapsed |