Abstract

Abstract A thermoplastic resin composition having excellent heat resistance, impact resistance, moldability and platability, which comprises: (i) from 10 to 90% by weight of a thermoplastic polycarbonate; (ii) from 10 to 90% by weight of a graft copolymer obtained by firstly polymerizing a monomer mixture comprising more than 30 and not more than 50% by weight of acrylonitrile and at least 50 and less than 70% by weight of styrene, as monomers for the first stage of graft polymerization, in the presence of a rubber-like polymer, and then polymerizing a monomer mixture comprising from 15 to 40% by weight of acrylonitrile and from 60 to 85% by weight of alpha -methylstyrene, as monomers for the second stage of graft polymerization, in the presence of the polymer obtained in the first stage; and (iii) from 0 to 60% by weight of a copolymer obtained by co-polymerizing from 50 to 80% by weight of an aromatic vinyl monomer and from 20 to 50% by weight of a vinyl cyanide monomer; the total amount of components (i), (ii) and (iii) being 100% by weight. The composition is useful for making molded products having excellent heat resistance, impact resistance and platability.

Inventors

  • 👤 Kazuo Kishida
  • 👤 Hiroshi Kawasaki
  • 👤 Hideyuki Shigemitsu

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 01:18
CPC Classifications
C; C08; C08L; C08L51/00; C08L25/00; C08L25/02; C08L25/04; C08L25/08; C08L25/12; C08L69/00

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 193 words
A thermoplastic resin composition having excellent heat resistance, impact resistance, moldability and platability, which comprises: (i) from 10 to 90% by weight of an aromatic polycarbonate; (ii) from 10 to 90% by weight of a graft copolymer obtained by firstly polymerizing a monomer mixture comprising more than 30 and not more than 50% by weight of acrylonitrile and at least 50 and less than 70% by weight of styrene, as monomers for the first stage of graft polymerization, in the presence of a diene rubber selected from the group consisting of polybutadiene, a butadiene-styrene copolymer and a butadiene-acrylonitrile copolymer, and then polymerizing a monomer mixture comprising from 15 to 40% by weight of acrylonitrile and from 60 to 85% by weight of α-methylstyrene, as monomers for the second stage of graft polymerization, in the presence of the polymer obtained in the first stage; and (iii) from 0 to 60% by weight of a copolymer obtained by co-polymerizing from 50 to 80% by weight of an aromatic vinyl monomer and from 20 to 50% by weight of a vinyl cyanide monomer; the total amount of components (i), (ii), and (iii) being 100% by weight.
Claim 2
Dependent Claim 193 words
A thermoplastic resin composition having excellent heat resistance, impact resistance, moldability and platability, which comprises: (i) from 10 to 90% by weight of an aromatic polycarbonate; (ii) from 10 to 90% by weight of a graft copolymer obtained by firstly polymerizing a monomer mixture comprising more than 30 and not more than 50% by weight of acrylonitrile and at least 50 and less than 70% by weight of styrene, as monomers for the first stage of graft polymerization, in the presence of a diene rubber selected from the group consisting of polybutadiene, a butadiene-styrene copolymer and a butadiene-acrylonitrile copolymer, and then polymerizing a monomer mixture comprising from 15 to 40% by weight of acrylonitrile and from 60 to 85% by weight of α-methylstyrene, as monomers for the second stage of graft polymerization, in the presence of the polymer obtained in the first stage; and (iii) from 0 to 60% by weight of a copolymer obtained by co-polymerizing from 50 to 80% by weight of an aromatic vinyl monomer and from 20 to 50% by weight of a vinyl cyanide monomer; the total amount of components (i), (ii), and (iii) being 100% by weight.
Claim 3
Dependent Claim 23 words
The thermoplastic resin composition according to claim 1, wherein the graft copolymer contains from 10 to 80% by weight of the diene rubber.
Claim 4
Dependent Claim 23 words
The thermoplastic resin composition according to claim 1, wherein the graft copolymer contains from 10 to 70% by weight of the diene rubber.
Claim 5
Dependent Claim 25 words
The thermoplastic resin composition according to claim 1, wherein said component (iii) is from 10 to 60% by weight based on the total resin composition.

References Cited (Backward Citations)

GB1253226A Cited
EP0051336A1 Cited
US4560725A Cited
EP0108350A1 Cited
US4518742A Cited
US4564654A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-05-11 1990-11-10 1991-05-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-05-11 1994-11-10 1995-05-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-05-11 1998-11-10 1999-05-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag