US4638555A Expired / Lapsed US ⏱️ 0.0 years remaining

Sodium sulphur cells and their manufacture

Assignee: Ionotec Ltd
•
Filing: 1985-06-26
•
Granted: 1987-01-27
•
Expires: 2005-06-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An alkali metal energy conversion device, particularly a sodium sulphur cell has a cylindrical outer casing (18) containing a tubular solid electrolyte (10) of beta alumina. An outer cathode region between the electrolyte (10) and the casing (18) contains sulphur, and an inner anode region in the electrolyte tube contains sodium. An alpha alumina lid (12) closes the tube (10) and holds a current collector (15). The cathode region is sealed by an annular metal element (23) which is thermocompression bonded about its inner periphery to the lid (12) and is welded about its outer periphery to the casing (18). A second annular metal element (26) is thermocompression bonded to the lid (12) wholly inside the first annular element (23) and is welded to the current collector. The metal elements (23, 26) are bonded to the lid (12) before the lid is glazed to the electrolyte tube (10) and before the first element (23) is welded to the casing (18).

Inventors

  • 👤 Stuart MacLachlan
  • 👤 Christopher O'Neill Bell

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 09:32
CPC Classifications
H; H01; H01M; H01M50/00; H01M50/10; H01M50/147; H01M50/148; H01M50/1535; H01M10/00; H01M10/36; H01M10/39; H01M10/3909; Y; Y02; Y02E; Y02E60/00; Y02E60/10; Y02P; Y02P70/00; Y02P70/50; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49108

Claims Analysis

Total Claims: 20
Claim 1
Independent Claim 79 words
A method of constructing an alkali metal energy conversion device having an external casing, a solid electrolyte element dividing the interior of the casing into two electrode regions, an electrically insulating ceramic element joined to the electrolyte element, and at least one metal member sealed to the insulating element, which method includes the steps of securing the metal member directly to the insulating ceramic element by thermocompression bonding before joining the insulating element to the electrolyte element by glazing.
Claim 2
Independent Claim 79 words
A method of constructing an alkali metal energy conversion device having an external casing, a solid electrolyte element dividing the interior of the casing into two electrode regions, an electrically insulating ceramic element joined to the electrolyte element, and at least one metal member sealed to the insulating element, which method includes the steps of securing the metal member directly to the insulating ceramic element by thermocompression bonding before joining the insulating element to the electrolyte element by glazing.
Claim 3
Dependent Claim 35 words
A method as claimed in claim 1 wherein after the metal member is thermocompression bonded to the insulating element the member is joined to the external casing to seal off one of said electrode regions.
Claim 4
Dependent Claim 57 words
A method as claimed in claim 2 wherein each of the metal member and the insulating ceramic element are substantially flat and a plurality of said metal members are bonded to respective said insulating ceramic elements simultaneously by stacking pairs of said metal members and said ceramic elements and applying bonding pressure and heat to the stack.
Claim 5
Dependent Claim 22 words
A method as claimed in claim 1 wherein the metal member is formed of an iron based or a nickel based alloy.
Claim 6
Dependent Claim 13 words
A method as claim 4 wherein the metal member is Inconel 600 alloy.
Claim 7
Dependent Claim 14 words
A method as claimed in claim 4 wherein the metal member is Fecralloy A.
Claim 8
Dependent Claim 15 words
A method as claimed in claim 1 wherein the electrolyte element is of beta alumina.
Claim 9
Dependent Claim 40 words
A method as claimed in claim 7 wherein the external casing is cylindrical, the electrolyte element is tubular, and the metal member is annular having a central opening through which extends, insulatingly spaced from the metal member, a current collector.
Claim 10
Dependent Claim 38 words
A method as claimed in claim 8 wherein said annular metal member is secured, by thermocompression bonding, to the insulating ceramic element in a narrow annular region at or near the inner periphery of the annular metal member.
Claim 11
Dependent Claim 31 words
A method as claimed in claim 8 wherein the pressure to produce bonding is applied through an annular metal washer of a material which becomes bonded to said annular metal member.
Claim 12
Dependent Claim 50 words
A method as claimed in claim 8 wherein, after the annular metal member has been secured to the insulating ceramic element and the electrolyte element has subsequently been joined to the ceramic element, the external casing is welded around its periphery at one end thereof to the annular metal member.
Claim 13
Dependent Claim 62 words
A method as claimed in claim 8 wherein the insulating ceramic element is a disc shaped lid for the tubular electrolyte element and an inner metal element is secured to the lid by thermocompression bonding to provide a metal element for sealing around the current collector which is subsequently inserted through the inner metal element and through an aperture in the lid.
Claim 14
Dependent Claim 27 words
A method as claimed in claim 12 wherein the inner metal element is bonded to the lid at the same time as the aforesaid annular metal member.
Claim 15
Dependent Claim 40 words
A method as claimed in claim 12 wherein the pressure to produce bonding of said inner metal element to the lid is applied through an annular metal backing element of a material which becomes bonded to said inner metal member.
Claim 16
Dependent Claim 52 words
A method as claimed in claim 12 wherein said inner metal element is formed as a flat annular sheet having an outer diameter which is less than the inner diameter of the aforesaid annular metal member and the inner metal element is thermocompression bonded to the lid about its outer periphery only.
Claim 17
Dependent Claim 58 words
A method as claimed in claim 15 wherein a metal strengthening washer is bonded to the inner metal element adjacent its inner periphery, the outer diameter of the washer being less than the diameter at which the inner metal element is sealed to the lid, and the current collector is sealed in electrical connection to the strengthening washer.
Claim 18
Dependent Claim 19 words
A method as claim 1 in any preceding claim wherein the insulating ceramic element is formed of alpha alumina.
Claim 19
Independent Claim 112 words
A method of constructing a cylindrical sodium sulphur cell having a beta alumina electrolyte element with an alpha alumina insulating element glazed to one end of the electrolyte element and with an annular metal member welded to an external casing surrounding the electrolyte tube and sealed to the alpha alumina around a central aperture therethrough which method includes the steps of forming the annular metal member of an iron based or nickel based alloy resistant to chemical attack by sodium and by hot sulphur/sodium polysulphides and securing this annular member directly to the alpha alumina element by thermocompression bonding in a vacuum before glazing the electrolyte tube to the alpha alumina element.
Claim 20
Independent Claim 112 words
A method of constructing a cylindrical sodium sulphur cell having a beta alumina electrolyte element with an alpha alumina insulating element glazed to one end of the electrolyte element and with an annular metal member welded to an external casing surrounding the electrolyte tube and sealed to the alpha alumina around a central aperture therethrough which method includes the steps of forming the annular metal member of an iron based or nickel based alloy resistant to chemical attack by sodium and by hot sulphur/sodium polysulphides and securing this annular member directly to the alpha alumina element by thermocompression bonding in a vacuum before glazing the electrolyte tube to the alpha alumina element.

References Cited (Backward Citations)

DE64656C Cited
US3833422A Cited
US4419418A Cited
US4473624A Cited
US4452871A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-01-26 1990-07-28 1991-01-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-01-26 1994-07-28 1995-01-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-01-26 1998-07-28 1999-01-27 $7700.00 Window Closed / Lapsed