Method for fusion splicing optical fiber
Assignee: TELEPHONE LABORATORIES INCORPORATED A NY CORP
•
Filing: 1984-01-24
•
Granted: 1986-08-05
•
Expires: 2004-01-24
Abstract
Abstract High-strength, low-loss splices of optical fiber can be produced by fusion splicing the fiber with a D2-O2 flame. According to the invention, the deuterium concentration in the gas mixture used to produce the flame is at least 10% by volume of the reducing gas present in the mixture. Preferably, substantially all of the reducing gas in the mixture is deuterium, with oxygen the oxidizing gas species.
Inventors
- 👤 Jane F. Kuhl
- 👤 William A. Vicory
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 07:41
CPC Classifications
G; G02; G02B; G02B6/00; G02B6/24; G02B6/255; G02B6/2551
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
107 words
Method for producing a composite optical fiber by end-to-end fusing a first optical fiber to a second optical fiber, the method comprising (a) aligning an end of the first optical fiber with an end of the second optical fiber, (b) heating the aligned fiber ends to a fusion temperature by exposing the aligned fiber ends to a flame produced by combustion of a gas mixture comprising at least one species of oxidizing gas and at least one species of reducing gas, with at least 10% by volume of the total amount of reducing gas present in the mixture being deuterium, and (c) fusing the aligned fiber ends.
Claim 2
Dependent Claim
107 words
Method for producing a composite optical fiber by end-to-end fusing a first optical fiber to a second optical fiber, the method comprising (a) aligning an end of the first optical fiber with an end of the second optical fiber, (b) heating the aligned fiber ends to a fusion temperature by exposing the aligned fiber ends to a flame produced by combustion of a gas mixture comprising at least one species of oxidizing gas and at least one species of reducing gas, with at least 10% by volume of the total amount of reducing gas present in the mixture being deuterium, and (c) fusing the aligned fiber ends.
Claim 3
Dependent Claim
15 words
Method of claim 1, wherein the oxidizing gas in the mixture consists substantially of oxygen.
Claim 4
Dependent Claim
15 words
Method of claim 2, wherein the reducing gas in the mixture consists substantially of deuterium.
Claim 5
Dependent Claim
18 words
Method of claim 1, wherein the first optical fiber and the second optical fiber are silica-based optical fibers.
Claim 6
Dependent Claim
13 words
Method of claim 4, wherein the optical fibers are single mode optical fibers.
Claim 7
Dependent Claim
214 words
Method for producing a composite optical fiber by end-to-end fusion splicing a first silica-based single mode optical fiber to a second silica-based single mode optical fiber, the method comprising (a) coupling electromagnetic radiation into the first optical fiber, at least part of the coupled-in radiation being guided to a first end of the first optical fiber and being radiated from the first end of the first optical fiber, (b) coupling at least part of the radiation radiated from the first end of the first optical fiber into a first end of the second optical fiber, (c) adjusting the position of at least one of said optical fibers to substantially maximize the amount of radiation coupled into the first end of the second optical fiber, (d) heating the first end of the first optical fiber and the first end of the second optical fiber by exposing the first ends of the first and second optical fibers, respectively, to a flame produced by combustion of a gas mixture comprising oxygen and at least one reducing gas species, with at least 10% by volume of the total amount of reducing gas present in the mixture being deuterium, and (e) fusing the first end of the first optical fiber to the first end of the second optical fiber.
Claim 8
Dependent Claim
214 words
Method for producing a composite optical fiber by end-to-end fusion splicing a first silica-based single mode optical fiber to a second silica-based single mode optical fiber, the method comprising (a) coupling electromagnetic radiation into the first optical fiber, at least part of the coupled-in radiation being guided to a first end of the first optical fiber and being radiated from the first end of the first optical fiber, (b) coupling at least part of the radiation radiated from the first end of the first optical fiber into a first end of the second optical fiber, (c) adjusting the position of at least one of said optical fibers to substantially maximize the amount of radiation coupled into the first end of the second optical fiber, (d) heating the first end of the first optical fiber and the first end of the second optical fiber by exposing the first ends of the first and second optical fibers, respectively, to a flame produced by combustion of a gas mixture comprising oxygen and at least one reducing gas species, with at least 10% by volume of the total amount of reducing gas present in the mixture being deuterium, and (e) fusing the first end of the first optical fiber to the first end of the second optical fiber.
Claim 9
Dependent Claim
15 words
Method of claim 6, wherein the reducing gas in the mixture consists substantially of deuterium.
References Cited (Backward Citations)
US3791714A
Cited
US4118618A
Cited
US4326870A
Cited
US4389230A
Cited
JPS5792533A
Cited
US4372768A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1989-08-04 | 1990-02-03 | 1990-08-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1993-08-04 | 1994-02-03 | 1994-08-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1997-08-04 | 1998-02-03 | 1998-08-05 | $7700.00 | Window Closed / Lapsed |