Abstract

Abstract A method of recovering gold and silver efficiently and almost completely from an aqueous solution containing cyanic compounds of gold and silver and which comprises adjusting the pH of the aqueous solution containing cyanic compounds of gold and silver to 6.0 or less, preferably to pH 3.0-5.0, by adding mineral acid, such as sulfuric acid or hydrochloric acid, preferably together with a small amount of active carbon, and subsequently passing the aqueous solution through an active carbon bed, preferably pretreated with mineral acid.

Inventors

  • 👤 Tadayoshi Ogasa
  • 👤 Fumio Kondo

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 22:29
CPC Classifications
C; C22; C22B; C22B11/00; C22B11/08; C01; C01G; C01G5/00; C01G5/003; C01G7/00; C01G7/003; C22B3/00; C22B3/20; C22B3/22; C22B3/24; C22B3/42; Y; Y02; Y02P; Y02P10/00; Y02P10/20

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 125 words
A method of preferentially recovering gold and silver from an aqueous solution containing cyanic compounds of gold, silver, and metals selected from the group consisting of copper, nickel, cobalt, zinc and iron, said solution containing between about 0.5 to 30 mg/l of gold, about 0.5 to 30 mg/l of silver, about 5 to 20 mg/l of the metals selected from the group consisting of copper, nickel, cobalt, zinc and iron, and 5 to 50 mg/l of free cyan selected from the group consisting of sodium cyanide and potassium cyanide, said method comprising the steps of (a) adding a mineral acid to said aqueous solution to reduce its pH to 6.0 or less, and (b) passing said acidified aqueous solution through a bed of active carbon.
Claim 2
Independent Claim 125 words
A method of preferentially recovering gold and silver from an aqueous solution containing cyanic compounds of gold, silver, and metals selected from the group consisting of copper, nickel, cobalt, zinc and iron, said solution containing between about 0.5 to 30 mg/l of gold, about 0.5 to 30 mg/l of silver, about 5 to 20 mg/l of the metals selected from the group consisting of copper, nickel, cobalt, zinc and iron, and 5 to 50 mg/l of free cyan selected from the group consisting of sodium cyanide and potassium cyanide, said method comprising the steps of (a) adding a mineral acid to said aqueous solution to reduce its pH to 6.0 or less, and (b) passing said acidified aqueous solution through a bed of active carbon.
Claim 3
Dependent Claim 27 words
A method according to claim 1, wherein in step (a) a small amount of active carbon is added to said aqueous solution together with said mineral acid.
Claim 4
Dependent Claim 26 words
A method according to claim 1, wherein the mineral acid added in step (a) is selected from the group consisting of sulfuric acid and hydrochloric acid.
Claim 5
Dependent Claim 29 words
A method according to claim 1, including the step of pretreating the bed of active carbon with mineral acid before passing the acidified aqueous solution therethrough in step (b).
Claim 6
Dependent Claim 29 words
A method according to claim 1, wherein the bed of active carbon used in step (b) is composed of active carbon particles having sizes of 0.3 to 3 mm.
Claim 7
Dependent Claim 33 words
A method according to claim 1, wherein in step (b) the acidified aqueous solution is passed through the bed of active carbon at a space velocity of 5 to 20 hrs -1 .
Claim 8
Dependent Claim 19 words
A method according to claim 1, wherein in step (a) the pH is reduced to between 3 and 5.

References Cited (Backward Citations)

US3970737A Cited
JPS5518501A Cited
CA1125033A Cited
EP0010367A1 Cited
US4289532A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-06-16 1989-12-16 1990-06-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-06-16 1993-12-16 1994-06-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-06-16 1997-12-16 1998-06-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag