Claims Analysis
Total Claims: 21
Claim 1
Independent Claim
214 words
A process for hydrocracking a hydrocarbon feed comprising contacting said feed at an elevated temperature of at least about 100° C. and in the presence of hydrogen with a catalyst comprising a supported mixture of a sulfide of (i) trivalent chromium, (ii) a metal selected from the group consisting of Mo, W and mixture thereof, and (iii) at least one promoter metal selected from the group consisting of (I) Ni, Co, Mn, Cu, Zn and mixture thereof and (II) mixtures of Fe with at least one metal selected from the group consisting of Ni, Co, Mn, Cu, Zn and mixture thereof, wherein said catalyst is formed by heating at an elevated temperature of at least about 200° C., in the presence of sulfur or sulfur bearing compound and under oxygen-free conditions, a composite of (a) a pre-selected quantity of inorganic refractory oxide support material, (b) a hydrated oxide of trivalent chromium and (c) one or more salts containing a thiometallate anion of Mo, W or mixture thereof and a cation containing at least one of said promoter metals wherein said promoter metal in said cation is divalent and is chelated by at least one neutral, nitrogen-containing polydentate ligand, said contacting occurring for a time sufficient to hydrocrack at least a portion of said feed.
Claim 2
Dependent Claim
214 words
A process for hydrocracking a hydrocarbon feed comprising contacting said feed at an elevated temperature of at least about 100° C. and in the presence of hydrogen with a catalyst comprising a supported mixture of a sulfide of (i) trivalent chromium, (ii) a metal selected from the group consisting of Mo, W and mixture thereof, and (iii) at least one promoter metal selected from the group consisting of (I) Ni, Co, Mn, Cu, Zn and mixture thereof and (II) mixtures of Fe with at least one metal selected from the group consisting of Ni, Co, Mn, Cu, Zn and mixture thereof, wherein said catalyst is formed by heating at an elevated temperature of at least about 200° C., in the presence of sulfur or sulfur bearing compound and under oxygen-free conditions, a composite of (a) a pre-selected quantity of inorganic refractory oxide support material, (b) a hydrated oxide of trivalent chromium and (c) one or more salts containing a thiometallate anion of Mo, W or mixture thereof and a cation containing at least one of said promoter metals wherein said promoter metal in said cation is divalent and is chelated by at least one neutral, nitrogen-containing polydentate ligand, said contacting occurring for a time sufficient to hydrocrack at least a portion of said feed.
Claim 3
Dependent Claim
64 words
The process of claim 1 wherein said thiometallate salt is of the general formula (ML)(Mo y W 1-y S 4 ) wherein M is one or more of said promoter metals in divalent form, wherein y is any value ranging from 0 to 1 and wherein L is one or more neutral, nitrogen-containing ligands at least one of which is a chelating polydentate ligand.
Claim 4
Dependent Claim
22 words
The process of claim 2 wherein said precursor salt is formed in the presence of a slurry of particles of support material.
Claim 5
Dependent Claim
28 words
The process of any of claims 1, 2 or 3 wherein L is selected from the group consisting of alkyl amines, aryl amines, nitrogen heterocycles and mixtures thereof.
Claim 6
Dependent Claim
12 words
The process of claim 4 wherein ligand L comprises an alkyl amine.
Claim 7
Dependent Claim
215 words
A process for hydrotreating a hydrocarbon feed which comprises contacting said feed at an elevated temperature of at least about 150° C. in the presence of hydrocarbon with a catalyst comprising a supported mixture of a sulfide of (i) trivalent chromium, (ii) a metal selected from the group consisting of Mo, W and mixture thereof, and (iii) at least one promoter metal selected from the group consisting of (I) Ni, Co, Mn, Cu, Zn and mixture thereof and (II) a mixture of Fe with at least one metal selected from the group consisting of Ni, Co, Mn, Cu, Zn and mixture thereof, wherein said catalyst is formed by heating, at an elevated temperature of at least about 200° C., in the presence of sulfur or sulfur bearing compound and under oxygen-free conditions, a composite of (a) a pre-selected quantity of inorganic refractory oxide support material, (b) a hydrated oxide of trivalent chromium and (c) one or more salts containing a thiometallate anion of Mo, W or mixture thereof and a cation containing at least one of said promoter metals wherein said promoter metal in said cation is divalent and is chelated by at least one neutral, nitrogen-containing polydentate ligand, said contacting occurring for a time sufficient to hydrotreat at least a portion of said feed.
Claim 8
Dependent Claim
215 words
A process for hydrotreating a hydrocarbon feed which comprises contacting said feed at an elevated temperature of at least about 150° C. in the presence of hydrocarbon with a catalyst comprising a supported mixture of a sulfide of (i) trivalent chromium, (ii) a metal selected from the group consisting of Mo, W and mixture thereof, and (iii) at least one promoter metal selected from the group consisting of (I) Ni, Co, Mn, Cu, Zn and mixture thereof and (II) a mixture of Fe with at least one metal selected from the group consisting of Ni, Co, Mn, Cu, Zn and mixture thereof, wherein said catalyst is formed by heating, at an elevated temperature of at least about 200° C., in the presence of sulfur or sulfur bearing compound and under oxygen-free conditions, a composite of (a) a pre-selected quantity of inorganic refractory oxide support material, (b) a hydrated oxide of trivalent chromium and (c) one or more salts containing a thiometallate anion of Mo, W or mixture thereof and a cation containing at least one of said promoter metals wherein said promoter metal in said cation is divalent and is chelated by at least one neutral, nitrogen-containing polydentate ligand, said contacting occurring for a time sufficient to hydrotreat at least a portion of said feed.
Claim 9
Dependent Claim
22 words
The process of claim 6 wherein said precursor salt is formed in the presence of a slurry of particles of support material.
Claim 10
Dependent Claim
64 words
The process of claim 7 wherein said thiometallate salt is of the general formula (ML)(Mo y W 1-y S 4 ) wherein M is one or more of said promoter metals in divalent form, wherein y is any value ranging from 0 to 1 and wherein L is one or more neutral, nitrogen-containing ligands at least one of which is a chelating polydentate ligand.
Claim 11
Dependent Claim
28 words
The process of either of claims 6, 7 or 8 wherein L is selected from the group consisting of alkyl amines, aryl amines, nitrogen heterocycles and mixtures thereof.
Claim 12
Dependent Claim
16 words
The process of claim 9 wherein said catalyst is formed in the presence of excess sulfur.
Claim 13
Dependent Claim
13 words
The process of claim 6 wherein said feed is a lube oil fraction.
Claim 14
Dependent Claim
13 words
The process of claim 10 wherein said feed is a lube oil fraction.
Claim 15
Dependent Claim
232 words
A process for removing nitrogen from a nitrogen-containing hydrocarbon feed which comprises contacting said feed at an elevated temperature of at least about 150° C. and in the presence of hydrogen with a catalyst comprising a supported mixture of a sulfide of (i) trivalent chromium, (ii) Mo, W or mixture thereof and (iii) at least one promoter metal selected from the group consisting of (I) Ni, Co, Mn, Cu, Zn and mixture thereof and (II) a mixture of Fe with at least one metal selected from the group consisting of Ni, Co, Mn, Cu, Zn and mixture thereof, wherein said catalyst has been prepared by compositing a pre-selected quantity of inorganic refractory oxide support material with (a) a hydrated oxide of trivalent chromium and (b) one or more catalyst precursor salts containing a thiometallate anion of Mo, W or mixture thereof and a cation containing at least one of said promoter metals wherein said promoter metal in said cation is divalent and is chelated by at least one neutral, nitrogen-containing polydentate ligand and heating said composite at an elevated temperature of at least about 200° C., in the presence of sulfur or sulfur bearing compound and under oxygen-free conditions for a time sufficient to form said catalyst, and wherein said feed is contacted with said catalyst for a time sufficient to remove at least a portion of said nitrogen from said feed.
Claim 16
Dependent Claim
232 words
A process for removing nitrogen from a nitrogen-containing hydrocarbon feed which comprises contacting said feed at an elevated temperature of at least about 150° C. and in the presence of hydrogen with a catalyst comprising a supported mixture of a sulfide of (i) trivalent chromium, (ii) Mo, W or mixture thereof and (iii) at least one promoter metal selected from the group consisting of (I) Ni, Co, Mn, Cu, Zn and mixture thereof and (II) a mixture of Fe with at least one metal selected from the group consisting of Ni, Co, Mn, Cu, Zn and mixture thereof, wherein said catalyst has been prepared by compositing a pre-selected quantity of inorganic refractory oxide support material with (a) a hydrated oxide of trivalent chromium and (b) one or more catalyst precursor salts containing a thiometallate anion of Mo, W or mixture thereof and a cation containing at least one of said promoter metals wherein said promoter metal in said cation is divalent and is chelated by at least one neutral, nitrogen-containing polydentate ligand and heating said composite at an elevated temperature of at least about 200° C., in the presence of sulfur or sulfur bearing compound and under oxygen-free conditions for a time sufficient to form said catalyst, and wherein said feed is contacted with said catalyst for a time sufficient to remove at least a portion of said nitrogen from said feed.
Claim 17
Dependent Claim
64 words
The process of claim 13 wherein said thiometallate salt is of the general formula (ML)(Mo y W 1-y S 4 ) wherein M is one or more of said promoter metals in divalent form, wherein y is any value ranging from 0 to 1 and wherein L is one or more neutral, nitrogen-containing ligands at least one of which is a chelating polydentate ligand.
Claim 18
Dependent Claim
40 words
The process of claim 14 wherein said precursor salt is formed in the presence of a slurry of support material and wherein ligand L is selected from the group consisting of alkyl amines, aryl amines, nitrogen heterocycles and mixtures thereof.
Claim 19
Dependent Claim
13 words
The process of claim 15 wherein said feed is a lube oil fraction.
Claim 20
Dependent Claim
206 words
A process for improving the oxidation stability of a nitrogen and sulfur containing lube oil feed which comprises contacting said feed at an elevated temperature of at least about 150° C. and in the presence of hydrogen with a catalyst comprising a support mixture of a sulfide of (i) trivalent chromium, (ii) Mo, W or mixture thereof and (iii) at least one promoter metal selected from the group consisting of Ni, Co, Mn, Cu, Zn and mixture thereof and mixture thereof with Fe wherein said catalyst has been prepared by compositing a pre-selected quantity of inorganic refractory oxide support material with (a) a hydrated oxide of trivalent chromium and (b) one or more catalyst precursor salts containing a thiometallate anion of Mo, W or mixture thereof and a cation containing at least one of said promoter metals wherein said promoter metal in said cation is divalent and is chelated by at least one neutral, nitrogen-containing polydentate ligand and heating said composite at elevated temperature, in the presence of sulfur or sulfur bearing compound and under oxygen-free conditions for a time sufficient to form said catalyst, said contacting of said feed with said catalyst occurring for a time sufficient to improve the oxidation stability of said oil.
Claim 21
Dependent Claim
206 words
A process for improving the oxidation stability of a nitrogen and sulfur containing lube oil feed which comprises contacting said feed at an elevated temperature of at least about 150° C. and in the presence of hydrogen with a catalyst comprising a support mixture of a sulfide of (i) trivalent chromium, (ii) Mo, W or mixture thereof and (iii) at least one promoter metal selected from the group consisting of Ni, Co, Mn, Cu, Zn and mixture thereof and mixture thereof with Fe wherein said catalyst has been prepared by compositing a pre-selected quantity of inorganic refractory oxide support material with (a) a hydrated oxide of trivalent chromium and (b) one or more catalyst precursor salts containing a thiometallate anion of Mo, W or mixture thereof and a cation containing at least one of said promoter metals wherein said promoter metal in said cation is divalent and is chelated by at least one neutral, nitrogen-containing polydentate ligand and heating said composite at elevated temperature, in the presence of sulfur or sulfur bearing compound and under oxygen-free conditions for a time sufficient to form said catalyst, said contacting of said feed with said catalyst occurring for a time sufficient to improve the oxidation stability of said oil.