Patent US4585583A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4585583A Expired / Lapsed US ⏱️ 0.0 years remaining

In situ solidification of ion exchange beads

Assignee: Dow Chemical Co
•
Filing: 1982-05-24
•
Granted: 1986-04-29
•
Expires: 2002-05-24
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method is disclosed for encapsulating and solidifying spent ion exchange beads contained in a container to form an ion exchange bed with a solidification resin without the necessity for applying shear in the bed by an external force such as by a mixing impeller. A solidification resin is flowed through the ion exchange bed by plug flow to intermix with and encapsulate each ion exchange bead therein. The resin is cured to form a uniform, solidified monolith of said ion exchange beads in said container. When the ion exchange bed contains free water, the process also effects the removal of substantial portions of the free water and also emulsifies and solidifies free water remaining in the bed.

Inventors

  • 👤 Keith Roberson
  • 👤 Don L. Stevens
  • 👤 Harold E. Filter

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 13:32
CPC Classifications
G; G21; G21F; G21F9/00; G21F9/28; G21F9/30; G21F9/301; G21F9/307

Claims Analysis

Total Claims: 26
Claim 1
Independent Claim 120 words
A method of solidifying an ion exchange bed composed of ion exchange beads which has been employed to remove ionic species from an aqueous solution which comprises: (a) introducing into and through the ion exchange bed contained in a container a sufficient quantity of a liquid solidification resin comprising a vinyl ester resin, an unsaturated polyester or a mixture of the two, and a suitable catalyst to cause the resin to cure, to intermix with and encapsulate said ion exchange beads in said container, said resin mixture being flowed through the bed in plug flow, and (b) curing said resin in situ in said container to thereby form a uniform solidified mixture of said beads and resin in said container.
Claim 2
Independent Claim 120 words
A method of solidifying an ion exchange bed composed of ion exchange beads which has been employed to remove ionic species from an aqueous solution which comprises: (a) introducing into and through the ion exchange bed contained in a container a sufficient quantity of a liquid solidification resin comprising a vinyl ester resin, an unsaturated polyester or a mixture of the two, and a suitable catalyst to cause the resin to cure, to intermix with and encapsulate said ion exchange beads in said container, said resin mixture being flowed through the bed in plug flow, and (b) curing said resin in situ in said container to thereby form a uniform solidified mixture of said beads and resin in said container.
Claim 3
Dependent Claim 39 words
The method of claim 1 wherein the ion exchange bed contains free water and a sufficient quantity of resin is introduced into and through said bed to force a substantial portion of said free water out of the bed.
Claim 4
Dependent Claim 13 words
The method of claim 1 wherein the ion exchange bed contains radioactive ions.
Claim 5
Dependent Claim 58 words
The method of claim 1 wherein the resin comprises a vinylester resin prepared by reacting about equivalent amounts of an unsaturated monocarboxylic acid and a polyepoxide resin, said vinyl ester resin containing ##STR2## linkage groups and terminal vinylidene groups attached to the ester end of said linkage, and said catalyst consists of a peroxide or a hydroperoxide catalyst.
Claim 6
Dependent Claim 29 words
The method of claim 1 wherein the ion exchange bed initially contains free water and the liquid precatalyzed resin has a viscosity of about 40 to about 1000 centipoise.
Claim 7
Dependent Claim 23 words
The method of claim 4 wherein the solidification resin includes in addition a promoter which functions to initiate the cure of said resin.
Claim 8
Dependent Claim 23 words
The method of claim 1 wherein the presolidification resin includes in addition a promoter which functions to initiate the cure of said resin.
Claim 9
Dependent Claim 12 words
The method of claim 1 wherein the resin is an unsaturated polyester.
Claim 10
Dependent Claim 10 words
The method of claim 1 wherein the container is rectangular.
Claim 11
Dependent Claim 25 words
The method of claim 1 wherein the solidification resin includes in addition from about 60 to about 30 percent by weight of a copolymerizable monomer.
Claim 12
Dependent Claim 11 words
The method of claim 10 wherein the copolymerizable monomer is styrene.
Claim 13
Dependent Claim 30 words
The method of claim 11 wherein the ion exchange bed initially contains free water and the liquid solidification resin has a viscosity of from about 40 to about 1000 centipoise.
Claim 14
Independent Claim 160 words
A method of solidifying an ion exchange bed composed of ion exchange beads contained in a container which has been employed to remove radioactive ions from an aqueous solution which comprises: (a) introducing into said container and through said ion exchange bed in plug flow a liquid solidification resin comprising a vinyl ester resin, an unsaturated polyester or a mixture of said two resins, from about 30 to about 60 percent of a monomer which is polymerizable with said resin, a sufficient quantity of a catalyst which causes the resin to cure to a solid monolith after said bed has been encapsulated by said resin, and a sufficient quantity of a promoter which functions to initiate the cure of said resin, said solidification resin being employed in an amount sufficient to encapsulate the entire bed; and (b) curing said resin in situ in said containter to form a uniform solidified mixture of said beads and said resin in said container.
Claim 15
Independent Claim 160 words
A method of solidifying an ion exchange bed composed of ion exchange beads contained in a container which has been employed to remove radioactive ions from an aqueous solution which comprises: (a) introducing into said container and through said ion exchange bed in plug flow a liquid solidification resin comprising a vinyl ester resin, an unsaturated polyester or a mixture of said two resins, from about 30 to about 60 percent of a monomer which is polymerizable with said resin, a sufficient quantity of a catalyst which causes the resin to cure to a solid monolith after said bed has been encapsulated by said resin, and a sufficient quantity of a promoter which functions to initiate the cure of said resin, said solidification resin being employed in an amount sufficient to encapsulate the entire bed; and (b) curing said resin in situ in said containter to form a uniform solidified mixture of said beads and said resin in said container.
Claim 16
Dependent Claim 23 words
The method of claim 13 wherein the liquid solidification resin has a viscosity at room temperature of about 40 to about 1000 centipoise.
Claim 17
Dependent Claim 10 words
The method of claim 13 wherein the container is rectangular.
Claim 18
Dependent Claim 42 words
The method of claim 13 wherein the resin is a thermosetting vinylester resin, the copolymerizable monomer is styrene, the catalyst is a peroxide or hydroperoxide, and the promoter is selected from the group consisting of lead naphthenate, cobalt naphthenate, dimethylaniline or N,N-dimethyl-p-toluidine.
Claim 19
Dependent Claim 44 words
The method of claim 13 wherein the resin is a thermosetting unsaturated polyester, the monomer copolymerizable therewith is styrene, the catalyst is a peroxide or a hydroperoxide and the promoter is selected from the group consisting of lead naphthenate, cobalt naphthenate, dimethylaniline or N,N-dimethyl-p-toluidine.
Claim 20
Independent Claim 120 words
A method of removing free water from a spent ion exchange bed composed of ion exchange beads and solidifying said bed, said bed being contained in a container, which comprises: (a) introducing into and through the ion exchange bed in plug flow a sufficient quantity of a liquid solidification resin comprising a vinyl ester resin, an unsaturated polyester or a mixture of the two and a catalyst to cause the resin to cure, to force free water from the bed and intermix with and encapsulate said ion exchange beads with said resin in said container; and (b) curing said resin in situ in said container to thereby form a uniform solidified mixture of said beads and resin in said container.
Claim 21
Independent Claim 120 words
A method of removing free water from a spent ion exchange bed composed of ion exchange beads and solidifying said bed, said bed being contained in a container, which comprises: (a) introducing into and through the ion exchange bed in plug flow a sufficient quantity of a liquid solidification resin comprising a vinyl ester resin, an unsaturated polyester or a mixture of the two and a catalyst to cause the resin to cure, to force free water from the bed and intermix with and encapsulate said ion exchange beads with said resin in said container; and (b) curing said resin in situ in said container to thereby form a uniform solidified mixture of said beads and resin in said container.
Claim 22
Dependent Claim 10 words
The method of claim 18 wherein the container is rectangular.
Claim 23
Dependent Claim 29 words
The method of claim 18 wherein said resin is a vinyl ester resin in admixture with from about 30 to about 60 percent by weight of a copolymerizable monomer.
Claim 24
Dependent Claim 11 words
The method of claim 20 wherein the copolymerizable monomer is styrene.
Claim 25
Dependent Claim 28 words
The method of claim 18 wherein the resin is an unsaturated polyester in admixture with from about 30 to about 60 percent by weight of a copolymerizable monomer.
Claim 26
Dependent Claim 11 words
The method of claim 22 wherein the copolymerizable monomer is styrene.

References Cited (Backward Citations)

US3658179A Cited
US4131563A Cited
US4077901A Cited
US4122048A Cited
US4107044A Cited
US4436655A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-04-28 1989-10-28 1990-04-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-04-28 1993-10-28 1994-04-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-04-28 1997-10-28 1998-04-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag