Method of manufacturing electrochemical cell

Assignee: NGK Insulators Ltd
•
Filing: 1985-07-02
•
Granted: 1986-04-15
•
Expires: 2005-07-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of manufacturing an electrochemical cell for determining the cencentration of a component of a measurement gas, which comprises a solid electrolyte body, and a pair of electrodes which are disposed on the solid electrolyte body and spaced apart from each other, such that one of the electrodes is exposed to the measurement gas via a porous ceramic diffusion layer having a predetermined diffusion resistance to the component of the measurement gas, so that an atmosphere adjacent to the above one electrode is controlled by means of reaction of the pair of electrodes by application of an electric current thereto, the method comprising the steps of: preparing an unfired or calcined laminar structure of the electrochemical cell such that an unfired or calcined layer of the above one electrode is covered by an unfired or calcined layer of the porous ceramic diffusion layer; starting a firing process to fire the laminar structure at predetermined elevated temperatures; applying an electric voltage or current to the electrodes; and terminating the firing process when a value of current flowing through the electrodes or a value of voltage present between the electrodes has become equal to a predetermined value at which is obtained a desired rate of diffusion of the gas component to the above one electrode through the porous ceramic diffusion layer.

Inventors

  • 👤 Kazuyoshi Shibata
  • 👤 Yoshihiko Mizutani

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 03:46
CPC Classifications
G; G01; G01N; G01N27/00; G01N27/26; G01N27/403; G01N27/406; G01N27/407; G01N27/4071; G01N27/4065; H; H01; H01M; H01M8/00; H01M8/10; H01M8/12; H01M8/1213; H01M4/00; H01M4/86; H01M4/90; H01M4/9016; H01M4/9025; H01M4/9041; H01M4/905; H01M4/9066; Y; Y02; Y02E; Y02E60/00; Y02E60/30; Y02E60/50; Y02P; Y02P70/00; Y02P70/50

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 247 words
A method of manufacturing an electrochemical cell for determining the concentration of a given component of a measurement gas, which has a solid electrolyte body, and at least one pair of electrodes which are disposed on the solid electrolyte body and spaced apart from each other, such that at least one of said at least one pair of electrodes is exposed to the measurement gas via a porous ceramic diffusion layer having a predetermined diffusion resistance to molecules of said component of the measurement gas, so that an atmosphere adjacent to said at least one electrode is controlled by means of reaction at said at least one pair of electrodes by application of an electric current thereto, comprising the steps of: preparing an unfired or calcined laminar structure of the electrochemical cell such that an unfired or calcined layer of said at least one electrode is covered by an unfired or calcined layer of said porous ceramic diffusion layer; starting a firing process to fire said unfired or calcined laminar structrure at predetermined elevated temperatures; applying an electric voltage or current to said at least one pair of electrodes; and terminating said firing process when a value of current flowing through, or voltage present between, said at least one pair of electrodes has become equal to a predetermined value at which is obtained a desired rate of diffusion of said component of the measurement gas through said porous ceramic diffusion layer to said at least one electrode.
Claim 2
Independent Claim 247 words
A method of manufacturing an electrochemical cell for determining the concentration of a given component of a measurement gas, which has a solid electrolyte body, and at least one pair of electrodes which are disposed on the solid electrolyte body and spaced apart from each other, such that at least one of said at least one pair of electrodes is exposed to the measurement gas via a porous ceramic diffusion layer having a predetermined diffusion resistance to molecules of said component of the measurement gas, so that an atmosphere adjacent to said at least one electrode is controlled by means of reaction at said at least one pair of electrodes by application of an electric current thereto, comprising the steps of: preparing an unfired or calcined laminar structure of the electrochemical cell such that an unfired or calcined layer of said at least one electrode is covered by an unfired or calcined layer of said porous ceramic diffusion layer; starting a firing process to fire said unfired or calcined laminar structrure at predetermined elevated temperatures; applying an electric voltage or current to said at least one pair of electrodes; and terminating said firing process when a value of current flowing through, or voltage present between, said at least one pair of electrodes has become equal to a predetermined value at which is obtained a desired rate of diffusion of said component of the measurement gas through said porous ceramic diffusion layer to said at least one electrode.
Claim 3
Dependent Claim 32 words
A method according to claim 1, wherein said value of current or voltage is detected continuously or intermittently, while said unfired or calcined laminar structure of the electrochemical cell is continuously fired.
Claim 4
Dependent Claim 65 words
A method according to claim 1, wherein said value of current or voltage is detected at least two times at a temperature lower than a firing temperature at which said unfired or calcined laminer structure of the electrochemical cell is fired, each of said at least two times of detection of said value of current or voltage being effected during interruption of said firing process.
Claim 5
Dependent Claim 63 words
A method according to claim 1, wherein said value of current or voltage is detected at least two times, and a point of time at which said predetermined value of the diffusion resistance of the porous ceramic diffusion layer is reached is obtained based on the detected values of current or voltage, said firing process being terminated at the obtained point of time.

References Cited (Backward Citations)

US4136000A Cited
US4169777A Cited
US4186071A Cited
US4294668A Cited
US4514812A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-04-14 1989-10-14 1990-04-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-04-14 1993-10-14 1994-04-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-04-14 1997-10-14 1998-04-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag