Abstract

Abstract A semiconductor wafer shape which when subjected to a simultaneous polishing of both wafer surfaces produces a wafer of superior flatness and surface finish, the said wafer having a diametral cross-sectional shape like that of a "dogbone" wherein the wafer is thinner in its medial region than it is in the peripheral region and has rounded edges, this shape resulting from a chemical thinning operation.

Inventors

  • 👤 James R. Hause
  • 👤 Eric Mendel

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 15:35
CPC Classifications
H; H10; H10P; H10P90/00; H10P90/12; H10P90/18; H10D; H10D62/00; H10D62/10; H10D62/117; H10P50/00; H10P50/60; H10P50/64; H10P50/642; H10P90/126; H10W; H10W46/00; H10W46/201; Y; Y10; Y10T; Y10T428/00; Y10T428/21; Y10T428/219; Y10T428/24; Y10T428/24942; Y10T428/2495

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 102 words
An improved semiconductor wafer shape, which when subjected to a subsequent polishing operation, in which both surfaces are simultaneously free-polished, produces a finished wafer having improved surface flatness and parallelism for the fabrication of very large scale integrated circuit devices, characterized by; The said wafer has a diametral cross-sectional shape wherein (a) The thickness of the wafer varies smoothly from a thin portion in the medial region of the wafer to a thicker portion at the peripheral region of the wafer, and; (b) The edges of the wafer are rounded whereby the cross-section can be visualized as having a "dogbone" like shape.
Claim 2
Dependent Claim 102 words
An improved semiconductor wafer shape, which when subjected to a subsequent polishing operation, in which both surfaces are simultaneously free-polished, produces a finished wafer having improved surface flatness and parallelism for the fabrication of very large scale integrated circuit devices, characterized by; The said wafer has a diametral cross-sectional shape wherein (a) The thickness of the wafer varies smoothly from a thin portion in the medial region of the wafer to a thicker portion at the peripheral region of the wafer, and; (b) The edges of the wafer are rounded whereby the cross-section can be visualized as having a "dogbone" like shape.
Claim 3
Dependent Claim 54 words
The wafer shape as claimed in claim 1 wherein; The difference in thickness (ΔT) between the thinner medial region and the thicker peripheral region satisfies the following relationship: ΔT=aD wherein ΔT=the difference between the respective thicknesses D=the diameter of the wafer a=a dimensionless constant within the range from 5×10 -6 to 1×10 -4 .
Claim 4
Dependent Claim 51 words
The wafer shape as claimed in claims 1 or 2 wherein; the edges of the wafer are rounded with a radius of curvature (R) satisfying the following relationship: R=b(T) wherein R=radius of curvature of the rounded edge T=thickness of the wafer b=a dimensionless constant within the range of 0.01 to 0.15.
Claim 5
Dependent Claim 18 words
The wafer shape as claimed in claim 1 wherein the shape is produced by a chemical thinning operation.
Claim 6
Dependent Claim 112 words
The wafer shape as claimed in claim 4 wherein the chemical thinning comprises the steps of: (a) Including the wafer coaxially among a nest of spaced apart wafers wherein the spacing (S) between the wafers has a dimension equal to S=bD wherein S=the linear distance separating adjacent wafers D=diameter of the wafers b=dimensionless constant within the range of 0.016 to 0.200. (b) Immersing the thus-nested wafers in an etching solution having an etch rate for the semiconductor material in the range from 0.10 to 0.53 microns per second. (c) and rotating the thus-immersed wafers at a speed of from 50 RPM to 110 RPM for a time between 2 and 5 minutes.
Claim 7
Dependent Claim 24 words
The wafer shape as claimed in claim 5 wherein the preferred spacing between wafers having a nominal diameter of 3 inches is 3 mm.
Claim 8
Dependent Claim 24 words
The wafer shape as claimed in claim 5 wherein the preferred spacing between wafers having a nominal diameter of 5 inches is 7 mm.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-03-31 1989-09-30 1990-04-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-03-31 1993-09-30 1994-04-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-03-31 1997-09-30 1998-04-01 $7700.00 Window Closed / Lapsed