Insulating seal for electrochemical cells

Assignee: Venture Technology Ltd
•
Filing: 1985-06-05
•
Granted: 1986-01-28
•
Expires: 2005-06-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An electrochemical cell (2) including at least two electrically conductive parts (8,14) which are sealed together by an organic polymer adhesive (16) but electrically insulated from each other by a layer (10) comprising aluminum oxide which is formed on a surface of one of the parts.

Inventors

  • 👤 Alexander Gilmour

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 12:39
CPC Classifications
H; H01; H01M; H01M50/00; H01M50/10; H01M50/147; H01M50/172; H01M50/174; H01M50/179; H01M50/183; H01M50/19; H01M50/193; Y; Y02; Y02E; Y02E60/00; Y02E60/10; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49108; Y10T29/4911; Y10T29/49114

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 42 words
An electrochemical cell including at least two electrically conductive parts which are sealed together by an organic polymer adhesive but electrically insulated from each other by a layer comprising aluminium oxide which is formed on a surface of one of the parts.
Claim 2
Dependent Claim 42 words
An electrochemical cell including at least two electrically conductive parts which are sealed together by an organic polymer adhesive but electrically insulated from each other by a layer comprising aluminium oxide which is formed on a surface of one of the parts.
Claim 3
Dependent Claim 39 words
An electrochemical cell according to claim 1, wherein the said one of the parts is composed of aluminium or an aluminium alloy and the aluminium oxide layer is formed by oxidation of the surface of the said one part.
Claim 4
Dependent Claim 18 words
An electrochemical cell according to claim 2, wherein the aluminium oxide layer is formed by an anodising process.
Claim 5
Dependent Claim 20 words
An electrochemical cell according to claim 1, wherein the layer has a thickness of from 0.1 microns to 25 microns.
Claim 6
Dependent Claim 23 words
An electrochemical cell according to claim 1, wherein the said two parts are each connected to a respective electrode of the electrochemical cell.
Claim 7
Dependent Claim 78 words
An electrochemical cell according to claim 1, wherein one of the said two parts is a terminal for the cell and is comprised of a laminar member comprising a layer of a first metal which is suitable as an electrical contact and is superposed on a layer of aluminium, the said aluminium oxide layer being formed on the aluminium layer, and the other of the said two parts constituting a container for the electrochemical components of the cell.
Claim 8
Dependent Claim 17 words
An electrochemical cell according to claim 1, wherein the organic polymer adhesive is a hot melt adhesive.
Claim 9
Independent Claim 63 words
A method of sealing together electrically conductive parts of an electrochemical cell while retaining the said parts electrically insulated from each other, the method comprising the steps of forming a layer comprising aluminium oxide on a surface of one of the parts and adhering the parts together by an organic polymer adhesive so that the layer electrically insulates the parts from each other.
Claim 10
Independent Claim 63 words
A method of sealing together electrically conductive parts of an electrochemical cell while retaining the said parts electrically insulated from each other, the method comprising the steps of forming a layer comprising aluminium oxide on a surface of one of the parts and adhering the parts together by an organic polymer adhesive so that the layer electrically insulates the parts from each other.
Claim 11
Dependent Claim 38 words
A method according to claim 8, wherein the said one of the parts is composed of aluminium or an aluminium alloy and the aluminium oxide layer is formed by oxidation of the surface of the said one part.
Claim 12
Dependent Claim 17 words
A method according to claim 9, wherein the aluminium oxide layer is formed by an anodising process.
Claim 13
Dependent Claim 19 words
A method according to claim 8, wherein the layer has a thickness of from 0.1 microns to 25 microns.
Claim 14
Dependent Claim 22 words
A method according to claim 8, wherein the said two parts are each connected to a respective electrode of the electrochemical cell.
Claim 15
Dependent Claim 77 words
A method according to claim 8, wherein one of the said two parts is a terminal for the cell and is comprised of a laminar member comprising a layer of a first metal which is suitable as an electrical contact and is superposed on a layer of aluminium, the said aluminium oxide layer being formed on the aluminium layer, and the other of the said two parts constituting a container for the electrochemical components of the cell.
Claim 16
Dependent Claim 16 words
A method according to claim 8, wherein the organic polymer adhesive is a hot melt adhesive.

References Cited (Backward Citations)

US4419418A Cited
US4508797A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-01-27 1989-07-29 1990-01-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-01-27 1993-07-29 1994-01-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-01-27 1997-07-29 1998-01-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag