Patent US4564715A successfully refreshed from Google Patents.
US4564715A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Preparation of monoalkylene glycols in two stages
Assignee: Union Carbide Corp
•
Filing: 1984-10-23
•
Granted: 1986-01-14
•
Expires: 2004-10-23
Abstract
Abstract High selectivity to monoalkylene glycol is obtained by contacting in an associated moiety-forming zone alkylene oxide and a selectivity enhancing, dissociatable metalate anion under conditions sufficient to associate at least a portion of the alkylene oxide with metalate anion, and then contacting the associated moiety with water in a glycol-forming zone to form alkylene glycol. The alkylene glycol can be separated from metalate anion. Desirably, the metalate anion can be recycled to the associated moiety-forming zone.
Inventors
- 👤 John R. Briggs
- 👤 George L. O'Connor
- 👤 John H. Robson
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-09 09:15
CPC Classifications
C; C07; C07C; C07C29/00; C07C29/09; C07C29/10; C07C29/103; C07C29/106
Claims Analysis
Total Claims: 23
Claim 1
Independent Claim
67 words
A process for making alkylene glycols comprising contacting alkylene oxide with a selectivity enhancing, dissociatable, metalate anion-containing material under conditions sufficient to associate at least a portion of the alkylene oxide with the metalate anion, said contacting being in the substantial absence of polyglycol forming amounts of water; and then contacting with water the metalate anion associated with alkylene oxide under conditions sufficient to form alkylene glycol.
Claim 2
Dependent Claim
67 words
A process for making alkylene glycols comprising contacting alkylene oxide with a selectivity enhancing, dissociatable, metalate anion-containing material under conditions sufficient to associate at least a portion of the alkylene oxide with the metalate anion, said contacting being in the substantial absence of polyglycol forming amounts of water; and then contacting with water the metalate anion associated with alkylene oxide under conditions sufficient to form alkylene glycol.
Claim 3
Dependent Claim
51 words
The process of claim 1 wherein the metalate anion has the formula [(A) q M(O)] a where M is a polyvalent metal having a functional positive oxidation state; A represents one or more substituents to fill the remaining valencies (q) of M, and a is the negative charge of the anion.
Claim 4
Dependent Claim
23 words
The process of claim 1 wherein the metalate anion is selected from the group consisting of molybdate, tungstate, metavanadate, pyrovanadate and hydrogen pyrovanadate.
Claim 5
Dependent Claim
106 words
The process of claim 3 wherein the alkylene oxide has the formula ##STR3## wherein each of R 1 , R 2 , R 3 and R 4 are the same or different and are hydrogen, alkyl of between 1 and about 10 carbons, monocyclic or bicyclic aryl having up to about 12 carbons, alkaryl having 7 to about 10 carbons, monocyclic or bicyclic aralkyl having 7 to about 15 carbons, alkenyl having 2 to 3 carbons, cycloalkyl having 3 to about 8 carbons, and cyclic structures joining two of R 1 , R 2 , R 3 and R 4 having 3 to about 8 carbons.
Claim 6
Dependent Claim
12 words
The process of claim 4 wherein the alkylene oxide is ethylene oxide.
Claim 7
Dependent Claim
21 words
The process of claim 1 wherein the mole ratio of alkylene oxide to metalate anion is between about 20:1 to 1:20.
Claim 8
Dependent Claim
21 words
The process of claim 5 wherein the mole ratio of ethylene oxide to metalate anion is between about 20:1 to 1:20.
Claim 9
Dependent Claim
35 words
The process of claim 7 wherein at least a portion of the unassociated ethylene oxide is removed from the liquid medium prior to the contacting of water with the metalate anion associated with ethylene oxide.
Claim 10
Dependent Claim
32 words
The process of claim 6 wherein about 5 to about 90 percent of the alkylene oxide is unassociated with the metalate and is passed with the liquid medium for contact with water.
Claim 11
Dependent Claim
27 words
The process of claim 5 wherein the liquid medium contains less than about 5 weight percent water during the contacting step between ethylene oxide and metalate anion.
Claim 12
Dependent Claim
27 words
The process of claim 10 wherein the liquid medium contains less than about 0.5 weight percent water during the contacting step between ethylene oxide and metalate anion.
Claim 13
Dependent Claim
16 words
The process of claim 6 wherein the liquid medium comprises an organic solvent for the metalate.
Claim 14
Dependent Claim
20 words
The process of claim 12 wherein the weight ratio of solvent to alkylene oxide is between about 20:1 to 1:5.
Claim 15
Dependent Claim
13 words
The process of claim 12 wherein the solvent is substantially immiscible with water.
Claim 16
Dependent Claim
25 words
The process of claim 14 wherein the solvent comprises at least one member selected from the group consisting of benzene, toluene, xylene, dichloromethane and 1,1,2-trichloroethane.
Claim 17
Dependent Claim
17 words
The process of claim 14 wherein the metalate anion is provided with at least one organo-containing cation.
Claim 18
Dependent Claim
30 words
The process of claim 16 wherein the organo-containing carbon has sufficient carbon atoms to render the metalate preferentially soluble in the organic solvent as compared to water at 25° C.
Claim 19
Dependent Claim
148 words
The process of claim 17 wherein the organic-containing cation is represented by the formula [(R.sup.0).sub.m Y.sub.n ].sup.x+ wherein Y is a polyvalent element which is an ionic charge carrying center; R 0 is hydrogen or hydrocarbyl-containing substituent with the proviso that Y has at least one R 0 which contains a hydrocarbyl substituent; m is the average number of electron pairs shared by Y with the total R 0 groups; and n is the number of charge carrying centers, wherein m, n and x are related by the equation x=n(V-m) in which V is the average functional oxidation state of Y wherein each electron pair used by each Y in bonding to R is given the value of 1 and the formal oxidation state of Y is the sum of the electron pairs bonding to R 0 and x/n, and x is an integer of 1 or 2.
Claim 20
Dependent Claim
12 words
The process of claim 18 wherein the organic-containing cation comprises ammonium cation.
Claim 21
Dependent Claim
13 words
The process of claim 19 wherein the ammonium cation comprises tetraalkyl ammonium cation.
Claim 22
Dependent Claim
13 words
The process of claim 18 wherein the organic-containing cation comprises quaternary phosphonium cation.
Claim 23
Dependent Claim
12 words
The process of claim 18 wherein the organic-containing cation comprises bis(trisubstituted-phosphine)iminium cation.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1989-01-13 | 1989-07-15 | 1990-01-14 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1993-01-13 | 1993-07-15 | 1994-01-14 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1997-01-13 | 1997-07-15 | 1998-01-14 | $7700.00 | Window Closed / Lapsed |