Patent US2531835A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4555293A Expired / Lapsed US ⏱️ 0.0 years remaining

Method and apparatus for thermo-bonding seams in thermoplastic material

Assignee: BODIGARD TECHNOLOGIES Inc A CORP OF DE
•
Filing: 1983-07-26
•
Granted: 1985-11-26
•
Expires: 2003-07-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Method for thermobonding thermoplastic material. A support plate supports sheets of the thermoplastic material, and heat element means is provided adjacent thereto. Pressure plate means mates with the support plate and may include recess means for receiving the heat element means. Melt zone means are formed between the heat element means and the pressure plate means (or the recess means) when they are in mating relationship. The melt zone means serves to confine the melted thermoplastic means to form a good seal by relieving stress between the seal and the seal-material interface. The heat element means and recess means are manufactured as interchangeable dies in different sizes and shapes for different materials. The heat element means may be formed into different shapes, such as a glove for manufacturing gloves.

Inventors

  • 👤 Robert C. French

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 19:02
CPC Classifications
B; B29; B29C; B29C66/00; B29C66/01; B29C66/05; B29C66/20; B29C66/21; B29C65/00; B29C65/02; B29C65/18; B29C65/22; B29C65/221; B29C65/222; B29C65/223; B29C65/224; B29C65/226; B29C65/74; B29C65/743; B29C65/7433; B29C65/7441; B29C66/10; B29C66/11; B29C66/112; B29C66/1122; B29C66/13; B29C66/137; B29C66/24; B29C66/244; B29C66/40; B29C66/41; B29C66/43; B29C66/70; B29C66/73; B29C66/739; B29C66/7392; B29C66/73921; B29C66/80; B29C66/81; B29C66/814; B29C66/8141; B29C66/81427; B29C66/81431; B29C66/818; B29C66/8181; B29C66/81811; B29C66/83; B29C66/832; B29C66/8322; B29C66/90; B29C66/95; B29C66/953; B29C66/9534; B29C65/229; B29C66/23; B29C66/232; B29C66/71; B29C66/81411; B29C66/81421; B29C66/81422; B29C66/81423; B29C66/9532; B29L; B29L2031/00; B29L2031/48; B29L2031/4842; B29L2031/4864

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 220 words
A method of sealing thermoplastic material which comprises the steps of: providing a support for the thermoplastic material to be sealed; providing a pressure means for applying pressure on the thermoplastic material to be sealed; providing a heat element in the configuration of a desired seam to be formed; at least one of said pressure means and said heat element having a recessed wall configured to define a confined melt zone volume between said pressure means and said heat element; providing said confined melt zone volume between the pressure means and the heat element when the pressure means and heat element are in mating relationship and are operating with the thermoplastic material; introducing the thermoplastic material to be sealed between the pressure means and the heat element; applying pressure on one side of the thermoplastic material by the pressure means while the heat element on the opposite side of the thermoplastic material is operating to provide heat to the thermoplastic material to melt the thermoplastic material in the configuration of the desired seam and force the melted thermoplastic to flow into and be confined within the melt zone volume; and maintaining said confined melt zone volume between the pressure means and the heat element throughout the time that the heat element is operating to provide heat to the thermoplastic material.
Claim 2
Independent Claim 220 words
A method of sealing thermoplastic material which comprises the steps of: providing a support for the thermoplastic material to be sealed; providing a pressure means for applying pressure on the thermoplastic material to be sealed; providing a heat element in the configuration of a desired seam to be formed; at least one of said pressure means and said heat element having a recessed wall configured to define a confined melt zone volume between said pressure means and said heat element; providing said confined melt zone volume between the pressure means and the heat element when the pressure means and heat element are in mating relationship and are operating with the thermoplastic material; introducing the thermoplastic material to be sealed between the pressure means and the heat element; applying pressure on one side of the thermoplastic material by the pressure means while the heat element on the opposite side of the thermoplastic material is operating to provide heat to the thermoplastic material to melt the thermoplastic material in the configuration of the desired seam and force the melted thermoplastic to flow into and be confined within the melt zone volume; and maintaining said confined melt zone volume between the pressure means and the heat element throughout the time that the heat element is operating to provide heat to the thermoplastic material.
Claim 3
Dependent Claim 32 words
A method as described in claim 1, said thermoplastic material comprising a material selected from the group consisting of spunbound olefin fiber sheet, spunbound polyethylene fiber sheet, polypropylene sheet and rayon acrylic.
Claim 4
Dependent Claim 132 words
A method as described in claim 1, including the steps of providing a work station and controlling the humidity (H) of the work station to between about 27 percent and about 52 percent; pressure (P) applied by said pressure means between about 20 p.s.i. and about 60 p.s.i., the normal temperature setting (T) of said heat element between about 58 degrees Fahrenheit and about 72 degrees Fahrenheit, raising the temperature of said heat element to a range between a high (t h ) of about 340 degrees Fahrenheit and low (t 1 ) of about 125 degrees Fahrenheit, applying said raise in temperature for a time period (h t ) between about 0.38 seconds and about 5.51 seconds and a dwell time (d) of between about 0.53 seconds and about 14.01 seconds.
Claim 5
Dependent Claim 84 words
A method as described in claim 1, said pressure applying step comprising introducing, to said one side of the thermoplastic material, said recessed wall in alignment with the heat element that is on the other side of the thermoplastic material, with a portion of said recessed wall and a portion of the heat element applying a crimping pressure on the thermoplastic material and simultaneously leaving a void between other portions of the recessed wall and the heat element to form the melt zone volume.
Claim 6
Dependent Claim 20 words
A method as described in claim 1, including the step of providing the heat element with a curvilinear cross-sectional configuration.
Claim 7
Dependent Claim 24 words
A method as described in claim 1, including the step of providing a layer of insulating material on said pressure means and said support.
Claim 8
Independent Claim 219 words
A method of forming a garment or glove from thermoplastic material which comprises the steps of: providing a support for the thermoplastic material; providing a pressure means for applying pressure on the thermoplastic material; providing a heat element in the configuration of a desired garment or glove to be formed; at least one of said pressure means and said heat element having a recessed wall configured to define a melt zone volume between said pressure means and said heat element; providing said confined melt zone volume between the pressure means and the heat element when the pressure means and heat element are in mating relationship and are operating with the thermoplastic material; introducing the thermoplastic material between the pressure means and the heat element; applying pressure on one side of the thermoplastic material by the pressure means while the heat element on the opposite side of the thermoplastic material is operating to provide heat to the thermoplastic material to melt the thermoplastic material in the configuration of the desired garment or glove and force the melted thermoplastic to flow into and be confined within the melt zone volume; and maintaining said confined melt zone volume between the pressure means and the heat element throughout the time that the heat element is operating to provide heat to the thermoplastic material.
Claim 9
Independent Claim 219 words
A method of forming a garment or glove from thermoplastic material which comprises the steps of: providing a support for the thermoplastic material; providing a pressure means for applying pressure on the thermoplastic material; providing a heat element in the configuration of a desired garment or glove to be formed; at least one of said pressure means and said heat element having a recessed wall configured to define a melt zone volume between said pressure means and said heat element; providing said confined melt zone volume between the pressure means and the heat element when the pressure means and heat element are in mating relationship and are operating with the thermoplastic material; introducing the thermoplastic material between the pressure means and the heat element; applying pressure on one side of the thermoplastic material by the pressure means while the heat element on the opposite side of the thermoplastic material is operating to provide heat to the thermoplastic material to melt the thermoplastic material in the configuration of the desired garment or glove and force the melted thermoplastic to flow into and be confined within the melt zone volume; and maintaining said confined melt zone volume between the pressure means and the heat element throughout the time that the heat element is operating to provide heat to the thermoplastic material.
Claim 10
Dependent Claim 122 words
A method as described in claim 7, including the steps of providing a work station and controlling the humidity (H) of the work station to between about 27 percent and about 52 percent; pressure (P) applied by said pressure means between about 20 p.s.i. and about 60 p.s.i., the normal temperature setting (T) of said heat element between about 58 degrees Fahrenheit and about 72 degrees Fahrenheit, raising the temperature of said heat element to a range between a high (t h ) of about 340 degrees Fahrenheit, applying said raise in temperature for a time period (h t ) between about 0.38 seconds and about 5.51 seconds and a dwell time (d) of between about 0.53 seconds and about 14.01 seconds.
Claim 11
Dependent Claim 84 words
A method as described in claim 7, said pressure applying step comprising introducing, to said one side of the thermoplastic material, said recessed wall in alignment with the heat element that is on the other side of the thermoplastic material, with a portion of said recessed wall and a portion of the heat element applying a crimping pressure on the thermoplastic material and simultaneously leaving a void between other portions of the recessed wall and the heat element to form the melt zone volume.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-11-25 1989-05-27 1989-11-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-11-25 1993-05-27 1993-11-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-11-25 1997-05-27 1997-11-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags