← Back to Patent Explorer
US4552267A Expired / Lapsed US ⏱️ 0.0 years remaining

Ceramic semiconductor package chip prevention structure and method

Assignee: National Semiconductor Corp
•
Filing: 1985-03-11
•
Granted: 1985-11-12
•
Expires: 2005-03-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A hermetic ceramic semiconductor package is provided with impact absorbing bumpers by applying a composition of sealing glass loaded with malleable metal particles to the ceramic package. The bumpers are applied to the ceramic parts when they are being coated with sealing glass. When the hermetic package seal is formed the bumpers will form a metal loaded matrix that will absorb impacts and thereby avoid chipping of the ceramic package due to impacts during handling.

Inventors

  • 👤 Francis W. Layher

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 17:04
CPC Classifications
H; H05; H05K; H05K13/00; H05K13/0084

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 92 words
In a ceramic package made up of parts sealed together to house an electronic device, which is to be handled in plural numbers pursuant to testing and using, wherein such handling may act to impact the devices and thereby chip said ceramic and a heat-resistant, non-absorbent, resilient coating material is located on said package to absorb said impact whereby the incidence of chipping of said ceramic is reduced, the improvement comprising: said coating being composed of a glass loaded with malleable metal particles and fused to the surface of said ceramic package.
Claim 2
Dependent Claim 92 words
In a ceramic package made up of parts sealed together to house an electronic device, which is to be handled in plural numbers pursuant to testing and using, wherein such handling may act to impact the devices and thereby chip said ceramic and a heat-resistant, non-absorbent, resilient coating material is located on said package to absorb said impact whereby the incidence of chipping of said ceramic is reduced, the improvement comprising: said coating being composed of a glass loaded with malleable metal particles and fused to the surface of said ceramic package.
Claim 3
Dependent Claim 22 words
The package of claim 1 wherein said malleable metal is selected from the group consisting of silver, copper, aluminum and alloys thereof.
Claim 4
Dependent Claim 24 words
The package of claim 1 wherein said coating is in the form of a bump located on said package where said impact will occur.
Claim 5
Dependent Claim 29 words
The package of claim 1 wherein said package parts are sealed together with glass and the glass in said coating is the material employed in forming the package seal.
Claim 6
Dependent Claim 12 words
The package of claim 4 wherein said glass is a solder glass.
Claim 7
Dependent Claim 87 words
An improved method for manufacturing an electronic device housed in a ceramic package wherein said package is formed of parts that are sealed together to form a ceramic package that is to be handled in plural numbers pursuant to testing and using and wherein such handling may act to impact the packages and thereby chip said ceramic, said improved method comprising the step of: applying a coating comprising malleable metal particles in a glass matrix to said package to render it resistant to mechanical shock and impact.
Claim 8
Dependent Claim 87 words
An improved method for manufacturing an electronic device housed in a ceramic package wherein said package is formed of parts that are sealed together to form a ceramic package that is to be handled in plural numbers pursuant to testing and using and wherein such handling may act to impact the packages and thereby chip said ceramic, said improved method comprising the step of: applying a coating comprising malleable metal particles in a glass matrix to said package to render it resistant to mechanical shock and impact.
Claim 9
Dependent Claim 20 words
The improved method of claim 6 wherein said coating is applied to said ceramic prior to forming said package seal.
Claim 10
Dependent Claim 26 words
The improved method of claim 6 wherein said coating is applied to said package in the form of bumps located where the mechanical impact will occur.
Claim 11
Dependent Claim 29 words
The improved method of claim 6 wherein said package is assembled using a sealing glass and said glass matrix in said coating is the same as said sealing glass.
Claim 12
Dependent Claim 24 words
The improved method of claim 6 wherein said malleable metal particles are selected from the group consisting of silver, copper, aluminum and alloys thereof.
Claim 13
Dependent Claim 14 words
The improved method of claim 10 wherein said metal particles are formed into flakes.

References Cited (Backward Citations)

US2951612A Cited
US4171049A Cited
US4231901A Cited
US4470507A Cited
US4463851A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-11-11 1989-05-13 1989-11-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-11-11 1993-05-13 1993-11-12 $3760.00 Window Closed / Lapsed