Abstract A composition and method for inhibiting ferrous metal corrosion in aqueous systems consisting essentially of (A) a copolymer of styrene sulfonic acid and maleic anhydride or maleic acid, and (B), water-soluble salts of said copolymer; and (C) a blend of two phosphonates consisting of (1) 2-phosphonobutane-1,2,4-tricarboxylic acid and (2) one member of the group consisting of (a) aminotrimethylene phosphonic acid and (b) hydroxy ethylidene diphosphonic acid. A preferred dosage, based on the active ingredient, is 7.5 ppm of styrene sulfonic acid/maleic anhydride copolymer and 6.0 ppm of phosphonate (1) and either 3.5 ppm of phosphonate (2a) of 4.2 ppm of phosphonate (2b). This relationship can be maintained during a total dosage of 0.01 to 500 ppm.
Inventors
👤 Alan M. Yeoman
Bibliographic Details
Application Number—
JurisdictionUS
Data Sourcegoogle_patents
Last Synchronized2026-11-03 20:25
CPC Classifications
C; C23; C23F; C23F11/00; C23F11/08; C23F11/10
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
118 words
A composition for inhibiting ferrous metal corrosion in an aqueous system consisting essentially of a copolymer of styrene sulfonic acid and maleic anhydride or maleic acid and water-soluble salts of said copolymer; and a blend of two phosphonates consisting of (1) 2-phosphonobutane-1,2,4-tricarboxylic acid and (2) one member of the group consisting of (a) aminotrimethylene phosphonic acid, and (b) hydroxyethylidene 1,1-diphosphonic acid, with the copolymer being combined with the blend of phosphonates so as to provide in the aqueous system to be treated: I. 7.5-15 ppm of the copolymers, and II. 9.5-10.4 ppm of the blend of phosphonates, with the dosage of the blend of phosphonates being 6-12 ppm of (1) and 3.5-8.4 ppm of either 2(a) or 2(b).
Claim 2
Dependent Claim
118 words
A composition for inhibiting ferrous metal corrosion in an aqueous system consisting essentially of a copolymer of styrene sulfonic acid and maleic anhydride or maleic acid and water-soluble salts of said copolymer; and a blend of two phosphonates consisting of (1) 2-phosphonobutane-1,2,4-tricarboxylic acid and (2) one member of the group consisting of (a) aminotrimethylene phosphonic acid, and (b) hydroxyethylidene 1,1-diphosphonic acid, with the copolymer being combined with the blend of phosphonates so as to provide in the aqueous system to be treated: I. 7.5-15 ppm of the copolymers, and II. 9.5-10.4 ppm of the blend of phosphonates, with the dosage of the blend of phosphonates being 6-12 ppm of (1) and 3.5-8.4 ppm of either 2(a) or 2(b).
Claim 3
Dependent Claim
26 words
The composition according to claim 1 which contains additionally an effective dispersing amount of a water soluble surfactant formed by condensing propylene oxide with propylene glycol.
Claim 4
Dependent Claim
29 words
A composition according to claim 1 wherein in the copolymer, the styrene sulfonic acid moiety is 25-95 weight percent and the molecular weight of the copolymer is about 1500-20,000.