Method of manufacturing carbon electrode

Assignee: Nikku Industry Co Ltd
•
Filing: 1983-10-11
•
Granted: 1985-08-20
•
Expires: 2003-10-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The present invention provides a method of manufacturing improved carbon electrodes. According to this method, the raw material for the carbon electrodes is pulverized and then kneaded with a binder. The kneaded mixture thus obtained is compressed under reduced pressure and thereafter extrusion-molded. This molded product is baked to obtain the desired carbon electrodes.

Inventors

  • 👤 Torata Tanaka

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 18:46
CPC Classifications
B; B30; B30B; B30B11/00; B30B11/22; B30B11/26; C; C04; C04B; C04B35/00; C04B35/515; C04B35/52; C04B35/528; C04B35/532; C25; C25C; C25C3/00; C25C3/06; C25C3/08; C25C3/12; C25C3/125; H; H05; H05B; H05B7/00; H05B7/02; H05B7/06; H05B7/08; H05B7/085

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 161 words
A method of manufacturing carbon electrodes, which comprises the steps of: kneading 100 parts of regular coke with 25 to 50 parts of a binder selected from the group consisting of coal tar pitch, coal tar and a synthetic resin at a temperature of 140° to 170° C., dividing the resultant kneaded mixture into a plurality of portions, compressing sequentially portion by portion the divided portions of the kneaded mixture at a pressure of 1500 to 3000 tons while being subjected to a vacuum below 300 Torr in a manner such that when a first divided portion is compressed, a second portion is supplied on top of the first compressed portion and compressed at the same pressure under the same vacuum, extrusion-molding the compressed mixture as a whole, after the whole of the divided portions of the mixture is thus compressed, baking the resultant extrudate, filling the baked product with an impregnator, and subjecting the resultant product to a secondary baking.
Claim 2
Independent Claim 161 words
A method of manufacturing carbon electrodes, which comprises the steps of: kneading 100 parts of regular coke with 25 to 50 parts of a binder selected from the group consisting of coal tar pitch, coal tar and a synthetic resin at a temperature of 140° to 170° C., dividing the resultant kneaded mixture into a plurality of portions, compressing sequentially portion by portion the divided portions of the kneaded mixture at a pressure of 1500 to 3000 tons while being subjected to a vacuum below 300 Torr in a manner such that when a first divided portion is compressed, a second portion is supplied on top of the first compressed portion and compressed at the same pressure under the same vacuum, extrusion-molding the compressed mixture as a whole, after the whole of the divided portions of the mixture is thus compressed, baking the resultant extrudate, filling the baked product with an impregnator, and subjecting the resultant product to a secondary baking.

References Cited (Backward Citations)

US1654046A Cited
US2269880A Cited
GB506728A Cited
US2960726A Cited
SU624796A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-08-19 1989-02-18 1989-08-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-08-19 1993-02-18 1993-08-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-08-19 1997-02-18 1997-08-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag