Abstract

Abstract Poly(heteroaromatics) are prepared by electrochemical polymerization, in particular anodic oxidation, of a monomeric heteroaromatic compound in an aqueous electrolyte solvent in which the monomeric heteroaromatic compound is dispersed, in the presence of a conductive salt and a dispersant. The films obtained by the process have good mechanical properties and high electrical conductivities.

Inventors

  • 👤 Gerhard Wegner
  • 👤 Wolfgang Wernet

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 06:19
CPC Classifications
C; C08; C08G; C08G73/00; C08G73/06; C08G61/00; C08G61/12; C08G61/122; C08G61/123; H; H01; H01B; H01B1/00; H01B1/06; H01B1/12; H01B1/124; H01B1/128; H01M; H01M4/00; H01M4/02; H01M4/36; H01M4/60; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 184 words
In an electrochemical process for preparing a poly(heteroaromatic) film wherein heteroaromatic compounds are polymerized by an anodic oxidation carried out in an electrolyte solvent in the presence of a conductive salt with the electrolyte solvent consisting essentially of a polar organic compound, and wherein the resulting polymer deposits in the form of a film on the surface of the anode, the improvement which comprises: dispersing said monomeric heteroaromatic compounds in an aqueous electrolyte solvent consisting of at least 80 percent by weight of water and to which has been added a water soluble dispersant selected from the group consisting of a neutral emulsifier, an anionic emulsifier or a mixture thereof together with the further addition of a conductive salt, with the proviso that a conductive salt need not be present when an anionic emulsifier is employed as the sole dispersant, introducing the resulting composition into an electrolytic cell and subjecting said monomeric compounds dispersed therein to an anodic oxidation to effect a polymerization thereof and deposition of the resulting polymer in the form of a film onto the anode surface of said electrolytic cell.
Claim 2
Dependent Claim 184 words
In an electrochemical process for preparing a poly(heteroaromatic) film wherein heteroaromatic compounds are polymerized by an anodic oxidation carried out in an electrolyte solvent in the presence of a conductive salt with the electrolyte solvent consisting essentially of a polar organic compound, and wherein the resulting polymer deposits in the form of a film on the surface of the anode, the improvement which comprises: dispersing said monomeric heteroaromatic compounds in an aqueous electrolyte solvent consisting of at least 80 percent by weight of water and to which has been added a water soluble dispersant selected from the group consisting of a neutral emulsifier, an anionic emulsifier or a mixture thereof together with the further addition of a conductive salt, with the proviso that a conductive salt need not be present when an anionic emulsifier is employed as the sole dispersant, introducing the resulting composition into an electrolytic cell and subjecting said monomeric compounds dispersed therein to an anodic oxidation to effect a polymerization thereof and deposition of the resulting polymer in the form of a film onto the anode surface of said electrolytic cell.
Claim 3
Dependent Claim 22 words
A process in accordance with claim 1, wherein the electrolyte solvent consists of from 90 to 100 percent by weight of water.
Claim 4
Dependent Claim 26 words
A process as claimed in claim 1, wherein the dispersant is used in an amount of from 0.001 to 1 mole per liter of electrolyte solvent.
Claim 5
Dependent Claim 29 words
A process as claimed in claim 1, wherein, in the electrolyte solvent, from 0.001 to 1 mole of a soluble conductive salt is used per liter of electrolyte solvent.
Claim 6
Dependent Claim 28 words
A process as claimed in claim 1, wherein the monomeric heteroaromatic compound is used in a concentration of from 0.001 to 5 moles per liter of electrolyte solvent.
Claim 7
Dependent Claim 35 words
A process as claimed in claim 1, wherein the electrochemical polymerization is carried out using a voltage of from 1 to 10 volt and a current density of from 0.05 to 50 mA/cm 2 .

References Cited (Backward Citations)

US3574072A Cited
US4401545A Cited
US4468291A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-08-19 1989-02-18 1989-08-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-08-19 1993-02-18 1993-08-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-08-19 1997-02-18 1997-08-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag