Abstract

Abstract An inorganic fiber-reinforced polyester resin composition having an improved mold-release property comprises 5% to 60% by weight of inorganic fibers, 0.01% to 2% by weight of at least one esters of pentaerythritol with saturated aliphatic monocarboxylic acids having 10 to 30 carbon atoms, and a balance of polyethylene terephthalate resin.

Inventors

  • 👤 Tomohiko Yoshida

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 01:24
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/04; C08K5/10; C08K5/101; C08K5/103; C08K13/00; C08K13/04

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 111 words
A polyester resin composition comprising 5% to 60% by weight of inorganic fibers; 0.01% to 2% by weight of at least one ester compound of the formula (I): ##STR2## wherein R 1 , R 2 , R 3 , and R 4 respectively represent, independently from each other, a member selected from the group consisting of a hydrogen atom and alkyl carbonyl radicals of the formula C n H 2n+1 CO-- wherein n represents an integer of from 10 to 30, at least one member of R 1 , R 2 , R 3 , and R 4 representing said alkyl carbonyl radical; and a balance of a polyethylene terephthalate resin.
Claim 2
Dependent Claim 111 words
A polyester resin composition comprising 5% to 60% by weight of inorganic fibers; 0.01% to 2% by weight of at least one ester compound of the formula (I): ##STR2## wherein R 1 , R 2 , R 3 , and R 4 respectively represent, independently from each other, a member selected from the group consisting of a hydrogen atom and alkyl carbonyl radicals of the formula C n H 2n+1 CO-- wherein n represents an integer of from 10 to 30, at least one member of R 1 , R 2 , R 3 , and R 4 representing said alkyl carbonyl radical; and a balance of a polyethylene terephthalate resin.
Claim 3
Dependent Claim 41 words
The composition as claimed in claim 1, wherein said polyethylene terephthalate resin comprises at least one member selected from the group consisting of linear polyethylene terephthalate homopolymers, and polyethylene terephthalate copolymers containing at least 60 molar % of ethylene terephthalate units.
Claim 4
Dependent Claim 47 words
The composition as claimed in claim 1, wherein said polyethylene terephthalate resin has an intrinsic viscosity [η] of from 0.4 to 1.4 determined in a solvent consisting of 50 parts by weight of phenol and 50 parts by weight of tetrachloroethane at a temperature of 25° C.
Claim 5
Dependent Claim 20 words
The composition as claimed in claim 1, wherein said inorganic fibers have a length of from 0.4 to 6 mm.
Claim 6
Dependent Claim 39 words
The composition as claimed in claim 1, wherein said ester compound of the formula (I) is selected from mono-, di-, tri- and tetra-esters of pentaerythritol with at least one saturated aliphatic monocarboxylic acid having 10 to 30 carbon atoms.
Claim 7
Dependent Claim 65 words
The composition as claimed in claim 1, wherein said ester compound of the formula (I) is selected from the group consisting of pentaerythritol mono-, di-, tri-, and tetra-stearates; pentaertyritol mono-, di-, tri-, and tetra-myristates; pentaerythritol mono-, di, tri-, and tetra-palmitates; pentaerythritol mono-, di-, tri-, and tetra-nonadecylates; pentaerythritol mono-, di-, tri-, and tetra-behenates; pentaerythritol mono-, di-, tri-, and tetra-montanates; and pentaerythritol mono-, di-, tri-, and tetra-melissinates.
Claim 8
Dependent Claim 25 words
The composition as claimed in claim 1, wherein said inorganic fibers are selected from the group consisting of glass fibers, carbon fibers, and asbestos fibers.
Claim 9
Independent Claim 133 words
A method for improving the mold release properties of a polyester resin composition containing polyethylene terephthalate resin and 5% to 60% by weight inorganic fibers comprising mixing at the same time together with the resin and the fibers from 0.01% to 2% by weight as a mold release agent at least one ester compound of the formula (I): ##STR3## wherein R 1 , R 2 , R 3 , and R 4 respectively represent, independently from each other, a member selected from the group consisting of a hydrogen atom and alkyl carbonyl radicals of the formula C n H 2n+1 CO-- wherein n represents an integer of from 10 to 30, at least one member of R 1 , R 2 , R 3 , and R 4 represents said alkyl carbonyl radical.
Claim 10
Independent Claim 133 words
A method for improving the mold release properties of a polyester resin composition containing polyethylene terephthalate resin and 5% to 60% by weight inorganic fibers comprising mixing at the same time together with the resin and the fibers from 0.01% to 2% by weight as a mold release agent at least one ester compound of the formula (I): ##STR3## wherein R 1 , R 2 , R 3 , and R 4 respectively represent, independently from each other, a member selected from the group consisting of a hydrogen atom and alkyl carbonyl radicals of the formula C n H 2n+1 CO-- wherein n represents an integer of from 10 to 30, at least one member of R 1 , R 2 , R 3 , and R 4 represents said alkyl carbonyl radical.

References Cited (Backward Citations)

US871008A Cited
US3423347A Cited
UST871008I4 Cited
FR2310403A2 Cited
JPS5373242A Cited
EP0003156A1 Cited
US4274987A Cited
DE3031491A1 Cited
US4419478A Cited
US4408000A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-07-22 1989-01-21 1989-07-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-07-22 1993-01-21 1993-07-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-07-22 1997-01-21 1997-07-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag