Photoresponsive semiconductor device having a double layer anti-reflective coating
Assignee: United Solar Systems Corp
•
Filing: 1984-02-24
•
Granted: 1985-07-09
•
Expires: 2004-02-24
Abstract
Abstract Disclosed is an improved dual layer anti-reflective coating for use in a photoresponsive semiconductor device, and a device incorporating the coating. The coating has a uniformly low parasitic absorbance in the range of about 475 to 600 nanometers. The dual layer has an incident light layer and an intermediate layer. The intermediate layer is formed of a silicon alloy material having at least one band gap widening element incorporated therein. The index of refraction of the intermediate layer has an index of refraction intermediate the indexes of the incident light layer and the underlying photoresponsive semiconductor device.
Inventors
- 👤 John McGill
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-24 14:17
CPC Classifications
H; H10; H10F; H10F77/00; H10F77/30; H10F77/306; H10F77/311; H10F77/315; H10F10/00; H10F10/10; H10F10/17; Y; Y02; Y02E; Y02E10/00; Y02E10/50; Y02E10/548
Claims Analysis
Total Claims: 26
Claim 1
Independent Claim
121 words
An improved p.i.n. type photovoltaic device having a transparent conductive oxide light incident layer thereon and in contact with an outermost layer of n-type conductivity amorphous silicon alloy material of the device, wherein the said outermost layer of n-type conductivity silicon alloy material has an index of refraction intermediate to and substantially equal to the square root of the product of the indices of refraction of the light incident layer and of the subjacent semiconductor body, said alloy material including silicon, hydrogen, fluorine, nitrogen, and phosphorous for substantially reducing the reflection of light and broadening the band width in the optimum operating range of the p.i.n. type photovoltaic device, whereby additional light energy is provided to the p.i.n. type photovoltaic device.
Claim 2
Dependent Claim
121 words
An improved p.i.n. type photovoltaic device having a transparent conductive oxide light incident layer thereon and in contact with an outermost layer of n-type conductivity amorphous silicon alloy material of the device, wherein the said outermost layer of n-type conductivity silicon alloy material has an index of refraction intermediate to and substantially equal to the square root of the product of the indices of refraction of the light incident layer and of the subjacent semiconductor body, said alloy material including silicon, hydrogen, fluorine, nitrogen, and phosphorous for substantially reducing the reflection of light and broadening the band width in the optimum operating range of the p.i.n. type photovoltaic device, whereby additional light energy is provided to the p.i.n. type photovoltaic device.
Claim 3
Dependent Claim
16 words
The p.i.n. type photovoltaic device of claim 1 wherein the light incident layer comprises (indium-tin) oxide.
Claim 4
Dependent Claim
24 words
The p.i.n. type photovoltaic device of claim 1 wherein the light incident layer has an idex of refraction of about 1.8 at 550 nanometers.
Claim 5
Dependent Claim
20 words
The p.i.n. type photovoltaic device of claim 1 wherein the light incident layer is about 450 to 500 Angstroms thick.
Claim 6
Dependent Claim
35 words
The p.i.n. type photovoltaic device of claim 1 wherein the light incident layer is a 450 to 500 Angstroms thick layer of (indium-tin) oxide having an index of refraction of about 1.8 at 550 nanometers.
Claim 7
Dependent Claim
30 words
The p.i.n. type photovoltaic device of claim 1 wherein the outermost n-type conductivity silicon alloy material layer has an index of refraction of about 2.5 to 3.3 at 550 nanometers.
Claim 8
Dependent Claim
28 words
The p.i.n. type photovoltaic device of claim 6 wherein the outermost n-type conductivity silicon alloy material layer has an index of refraction of about 3.0 at 550 nanometers.
Claim 9
Dependent Claim
29 words
The p.i.n. type photovoltaic device of claim 1 wherein the outermost n-type conductivity silicon alloy material layer has an electrical conductivity of at least 10 -5 (ohm-cm) -1 .
Claim 10
Dependent Claim
27 words
The p.i.n. type photovoltaic device coating of claim 1 wherein the outermost n-type conductivity silicon alloy material layer is from about 150 to about 250 Angstroms thick.
Claim 11
Dependent Claim
22 words
The p.i.n. type photovoltaic device of claim 9 wherein the outermost n-type conductivity silicon alloy material layer is about 200 Angstroms thick.
Claim 12
Dependent Claim
27 words
The p.i.n. type photovoltaic device of claim 1 wherein the outermost n-type conductivity silicon alloy material layer has a band gap of 2.0 to 2.4 electron volts.
Claim 13
Dependent Claim
27 words
The p.i.n. type photovoltaic device of claim 11 wherein the outermost layer of n-conductivity type silicon alloy material has a band gap of about 2.2 electron volts.
Claim 14
Dependent Claim
66 words
The p.i.n. type photovoltaic device of claim 1 wherein the outermost n-type conductivity silicon alloy material layer is a 200 Angstrom thick layer of a silicon alloy material comprising silicon, hydrogen, fluorine, nitrogen, and phosphorous, having a band gap of about 2.2 electron volts, an index of refraction of about 3.0 at 550 nanometers, and an electrical conductivity of at least 10 -5 (ohm-cm) -1 .
Claim 15
Dependent Claim
59 words
The p.i.n. type photovoltaic device of claim 1 wherein the light incident layer has an index of refraction of about 1.8, the outermost layer of n-type conductivity silicon alloy material has an index of refraction of about 2.5 to 3.3 at 550 nanometers, and the subjacent semiconductor device has an index of refraction greater than 3.3 at 550 nanometers.
Claim 16
Dependent Claim
25 words
The p.i.n. type photovoltaic device of claim 1 wherein the anti-reflective coating has a substantially low, uniform, parasitic light absorbance between 475 and 600 nanometers.
Claim 17
Independent Claim
147 words
A method of forming a photoresponsive semiconductor device comprising the steps of: (a) forming a photoresponsive semiconductor layer; (b) depositing an amorphous silicon alloy n-type conductivity semiconductor material layer, from a deposition gas comprising SiF 4 , H 2 , N 2 , and PH 3 , the silicon alloy material having a band gap widening element therein to provide a wider band gap than the responsive semiconductor layer, the silicon alloy material having a lower refractive index than the photoresponsive semiconductor layer; and (c) depositing a light incident layer atop the silicon alloy material, the light incident layer having a lower index of refraction than the silicon alloy material, the index of refraction of the n-type conductivity silicon alloy material layer being approximately equal to the square root of the product of the indices of refraction of the light incident layer and the photoresponsive semiconductor layer.
Claim 18
Independent Claim
147 words
A method of forming a photoresponsive semiconductor device comprising the steps of: (a) forming a photoresponsive semiconductor layer; (b) depositing an amorphous silicon alloy n-type conductivity semiconductor material layer, from a deposition gas comprising SiF 4 , H 2 , N 2 , and PH 3 , the silicon alloy material having a band gap widening element therein to provide a wider band gap than the responsive semiconductor layer, the silicon alloy material having a lower refractive index than the photoresponsive semiconductor layer; and (c) depositing a light incident layer atop the silicon alloy material, the light incident layer having a lower index of refraction than the silicon alloy material, the index of refraction of the n-type conductivity silicon alloy material layer being approximately equal to the square root of the product of the indices of refraction of the light incident layer and the photoresponsive semiconductor layer.
Claim 19
Dependent Claim
24 words
The method of claim 16 wherein the silicon alloy material has an index of refraction of from about 2.5 to 3.3 at 550 nanometers.
Claim 20
Dependent Claim
22 words
The method of claim 16 wherein the silicon alloy material has an electrical conductivity of at least 10 -5 (ohm-cm) -1 .
Claim 21
Dependent Claim
21 words
The method of claim 16 wherein the silicon alloy material has a band gap of about 2.0 to 2.4 electron volts.
Claim 22
Dependent Claim
18 words
The method of claim 16 comprising depositing the silicon alloy material to a thickness of about 200 angstroms.
Claim 23
Dependent Claim
75 words
The method of claim 16 comprising depositing the silicon alloy material from a gas stream containing SiF 4 , H 2 , N 2 , and PH 3 whereby to form a deposit of silicon alloy material at least 200 angstroms thick having a band gap of 2.0 to 2.4 volts, an index of refraction of about 2.5 to 3.3. at 550 nanometers, and an electrical conductivity of at least 10 -5 (ohm-cm) -1 .
Claim 24
Dependent Claim
22 words
The method of claim 16 comprising depositing a light incident layer of a transparent conductive oxide atop the silicon alloy material layer.
Claim 25
Dependent Claim
13 words
The method of claim 22 wherein the transparent conductive oxide is (indium-tin) oxide.
Claim 26
Dependent Claim
20 words
The method of claim 16 comprising depositing the light incident layer to a thickness of about 450 to 500 angstroms.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1988-07-08 | 1989-01-07 | 1989-07-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1992-07-08 | 1993-01-07 | 1993-07-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1996-07-08 | 1997-01-07 | 1997-07-09 | $7700.00 | Window Closed / Lapsed |