Patent US4516982A successfully refreshed from Google Patents.
US4516982A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Antimisting system for hydrocarbon fluids
Assignee: ExxonMobil Technology and Engineering Co
•
Filing: 1983-11-02
•
Granted: 1985-05-14
•
Expires: 2003-11-02
Abstract
Abstract The present invention relates to hydrocarbon, and specifically jet fuels, solutions having dilatant properties in which the hydrocarbon solution contains a polymer complex which is the interaction product of a sulfonate containing polymer and an amine containing copolymer.
Inventors
- 👤 Ilan Duvdevani
- 👤 Dennis G. Peiffer
- 👤 John A. Eckert
- 👤 Robert D. Lundberg
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 03:16
CPC Classifications
B; B05; B05D; B05D5/00; B05D5/08; C; C10; C10L; C10L1/00; C10L1/10; C10L1/14; C10L1/146; C10L1/22; C10L1/234; C10L1/236; C10L1/2368; C10L1/24; C10L1/2462
Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
167 words
An antimisting hydrocarbon solution comprising a jet fuel and a polymer complex, wherein the concentration of said polymer complex in said solution is about 0.01 to about 2 grams per 100 ml of said solution and said polymer complex comprises the interaction product of a metal neutralized sulfonated polymer and an amine containing polymer which has a vinyl pyridine comonomer incorporated therein, said metal neutralized sulfonated polymer having a polymer backbone which has a solubility parameter of less than about 10.5 and a crystallinity of less than about 25%, said metal neutralized sulfonated polymer containing about 4 to about 200 meq. of metal neutralized sulfonate groups per 100 gram of polymer, said metal neutralized sulfonate groups being neutralized with a metal ion selected from the groups consisting of zinc, copper, iron, nickel, cobalt, antimony and lead, the nitrogen content of the amine containing polymer is about 4 meq. to about 500 meq. per 100 gram of polymer, said amine containing polymer being soluble in said jet fuel.
Claim 2
Dependent Claim
167 words
An antimisting hydrocarbon solution comprising a jet fuel and a polymer complex, wherein the concentration of said polymer complex in said solution is about 0.01 to about 2 grams per 100 ml of said solution and said polymer complex comprises the interaction product of a metal neutralized sulfonated polymer and an amine containing polymer which has a vinyl pyridine comonomer incorporated therein, said metal neutralized sulfonated polymer having a polymer backbone which has a solubility parameter of less than about 10.5 and a crystallinity of less than about 25%, said metal neutralized sulfonated polymer containing about 4 to about 200 meq. of metal neutralized sulfonate groups per 100 gram of polymer, said metal neutralized sulfonate groups being neutralized with a metal ion selected from the groups consisting of zinc, copper, iron, nickel, cobalt, antimony and lead, the nitrogen content of the amine containing polymer is about 4 meq. to about 500 meq. per 100 gram of polymer, said amine containing polymer being soluble in said jet fuel.
Claim 3
Dependent Claim
40 words
A process for reducing antimisting according to claim 1, further including the addition of about 1000 ppm to about 10 weight percent of a polar cosolvent to the solution, said polar cosolvent having a solubility parameter of at least 10.0.
Claim 4
Dependent Claim
15 words
The solution of claim 1, wherein the neutralized sulfonated polymer contains zinc as the counterions.
Claim 5
Dependent Claim
15 words
The solution of claim 1, wherein said sulfonated polymer is derived from an EPDM terpolymer.
Claim 6
Dependent Claim
19 words
The solution of claim 1, wherein the amine containing polymer is a copolymer of t-butyl styrene and vinyl pyridine.
Claim 7
Dependent Claim
17 words
The solution of claim 1, wherein said sulfonated polymer is in excess of said amine containing polymer.
Claim 8
Dependent Claim
17 words
The solution of claim 1, wherein said amine containing polymer is in excess of said sulfonated polymer.
Claim 9
Dependent Claim
44 words
The solution of claim 2, wherein said sulfonated polymer is selected from the group consisting of sulfonated polyethylene, sulfonated polypropylene, sulfonated ethylene-polypropylene copolymers and terpolymers, wherein the third monomer is a nonconjugated diene hydrocarbon having from 5 to 15 carbon atoms and sulfonated polystyrene.
Claim 10
Dependent Claim
19 words
The solution of claim 2, wherein said polar cosolvent is selected from the group consisting of alcohols and amines.
Claim 11
Dependent Claim
18 words
The solution of claim 9, wherein said polar cosolvent has a boiling point of at least 50° C.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1988-05-13 | 1988-11-12 | 1989-05-14 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1992-05-13 | 1992-11-12 | 1993-05-14 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1996-05-13 | 1996-11-12 | 1997-05-14 | $7700.00 | Window Closed / Lapsed |