Claim 1
Independent Claim
202 words
A method for controlling the dimensions of a hollow plastics product injection molded within the cooling cavity of a mold having a core section and a cavity section defining the cooling cavity therebetween and separated by a parting line comprising stabilizing the core section in the cooling cavity and being characterized by the steps of: (a) injecting a first plastics material into the cooling cavity so that only a part of the cooling cavity is filled and so that the injected first plastics material does not completely cover the parting line; (b) cooling the injected first plastics material in the cooling cavity; (c) injecting subsequent to injecting the first plastics material a second plastics material into the cooling cavity so that the cooled injected first plastics material in said part of the cooling cavity stabilizes the core section by impeding movement of the core section caused by injecting the second plastics material and whereby the injected second plastics material fills the cooling cavity to thereby completely cover the parting line and fuses with the cooled previously injected plastics material; (d) cooling the injected plastics material in the cooling cavity to thereby solidify the fused unit; and (e) ejecting the solidified molded unit.
Claim 2
Independent Claim
202 words
A method for controlling the dimensions of a hollow plastics product injection molded within the cooling cavity of a mold having a core section and a cavity section defining the cooling cavity therebetween and separated by a parting line comprising stabilizing the core section in the cooling cavity and being characterized by the steps of: (a) injecting a first plastics material into the cooling cavity so that only a part of the cooling cavity is filled and so that the injected first plastics material does not completely cover the parting line; (b) cooling the injected first plastics material in the cooling cavity; (c) injecting subsequent to injecting the first plastics material a second plastics material into the cooling cavity so that the cooled injected first plastics material in said part of the cooling cavity stabilizes the core section by impeding movement of the core section caused by injecting the second plastics material and whereby the injected second plastics material fills the cooling cavity to thereby completely cover the parting line and fuses with the cooled previously injected plastics material; (d) cooling the injected plastics material in the cooling cavity to thereby solidify the fused unit; and (e) ejecting the solidified molded unit.
Claim 3
Independent Claim
188 words
A method for controlling the dimensions of a hollow plastics product injection molded within the cooling cavity of a mold having a core section and a cavity section defining the cooling cavity therebetween and separated by a parting line, comprising stabilizing the core section in the cooling cavity, and being characterized by the steps of: (a) injecting a first plastics material into the cooling cavity so that only a part of the cooling cavity is filled; (b) cooling the injected first plastics material in the cooling cavity while discontinuing the filling of the cooling cavity for a period; (c) injecting subsequent to said period a second plastics material into the cooling cavity so that the cooled injected first plastics material in said part of the cooling cavity stabilizes the core section by impeding movement of the core section caused by injecting the second plastics material and whereby the injected second plastics material fills the cooling cavity and fuses with the cooled previously injected plastics material; (d) cooling the injected plastics material in the cooling cavity to thereby solidify the fused unit; and (e) ejecting the solidified molded unit.
Claim 4
Independent Claim
188 words
A method for controlling the dimensions of a hollow plastics product injection molded within the cooling cavity of a mold having a core section and a cavity section defining the cooling cavity therebetween and separated by a parting line, comprising stabilizing the core section in the cooling cavity, and being characterized by the steps of: (a) injecting a first plastics material into the cooling cavity so that only a part of the cooling cavity is filled; (b) cooling the injected first plastics material in the cooling cavity while discontinuing the filling of the cooling cavity for a period; (c) injecting subsequent to said period a second plastics material into the cooling cavity so that the cooled injected first plastics material in said part of the cooling cavity stabilizes the core section by impeding movement of the core section caused by injecting the second plastics material and whereby the injected second plastics material fills the cooling cavity and fuses with the cooled previously injected plastics material; (d) cooling the injected plastics material in the cooling cavity to thereby solidify the fused unit; and (e) ejecting the solidified molded unit.
Claim 5
Dependent Claim
26 words
A method according to claim 1 or 2 wherein the injection pressure of the first plastic is less than the injection pressure of the second plastic.
Claim 6
Dependent Claim
26 words
A method according to claim 1 or 2 wherein the period of injecting the first plastic is less than the period of injecting the second plastic.
Claim 7
Dependent Claim
21 words
A method according to claim 1 or 2 wherein the first plastic has the same chemical composition as the second plastic.
Claim 8
Dependent Claim
25 words
A method according to claim 1 or 2 wherein the injection of the second plastic is started before the injected first plastic is completely solidified.
Claim 9
Dependent Claim
33 words
A method according to claim 1 or 2 wherein a relatively smaller amount of first plastics material is injected into the cooling cavity as compared with the quantity of the second plastics material.
Claim 10
Dependent Claim
25 words
A method according to claim 1 or 2 wherein the first plastic enters the cooling cavity at a lower pressure than the second plastic does.
Claim 11
Dependent Claim
32 words
A method according to claim 1 or 2 wherein the apex of the core section is not at any time during the molding cycle supported from transverse deflection by the cavity section.
Claim 12
Dependent Claim
30 words
A method according to claim 1 or 2 wherein the apex of the core section is not at any time during the molding cycle in contact with the cavity section.
Claim 13
Dependent Claim
44 words
A method according to claim 1 or 2 comprising the additional step of: (f) injecting a third plastics material into the cooling cavity subsequent to beginning the injection of the first plastics material and prior to ending the injection of the second plastics material.
Claim 14
Dependent Claim
23 words
A method according to claim 1 or 2 wherein the first and/or the second plastics material are injected through one or more gates.
Claim 15
Dependent Claim
18 words
A method according to claim 12 wherein the first plastics material is injected through more than one gate.
Claim 16
Dependent Claim
21 words
A method according to claim 12 wherein the first plastics material is injected through different gate/s than the second plastics material.
Claim 17
Dependent Claim
22 words
A method according to claim 12 wherein the first plastic material is injected through the same gate/s as the second plastic material.
Claim 18
Dependent Claim
28 words
A method according to claim 14 wherein the first plastics material is injected through a first gate and the second plastics material is injected through a second gate.
Claim 19
Dependent Claim
47 words
A method according to claim 16 wherein the injection pressure of the first plastic in a first runner is approximately the same as the injection pressure of the second plastic in a second runner, but the first gate has a smaller cross-sectional area than the second gate.
Claim 20
Dependent Claim
46 words
A method according to claim 12 comprising the additional step of: (f) retracting, subsequent to step (a), retractable partition/s of said core and/or cavity sections to provide flow path/s for the second plastics material between the injection gate/s and the unfilled portion of the cooling cavity.
Claim 21
Dependent Claim
23 words
A method according to claim 18 wherein the flow path/s form part of the cooling cavity and remains filled with second plastics material.
Claim 22
Dependent Claim
43 words
A method according to claim 18 wherein at least part of the flow path/s does not form part of the cooling cavity and wherein the retractable portion is extended to define the cooling cavity during or after injection of the second plastics material.
Claim 23
Dependent Claim
17 words
A method according to claim 18 wherein the retractable portion comprises movable part/s of the core section.
Claim 24
Dependent Claim
17 words
A method according to claim 18 wherein the retractable portion comprises the whole of the core section.
Claim 25
Dependent Claim
46 words
A method according to claim 18 wherein step (f) comprises: (g) creating only one flow path and thereby impeding any movement of the core with some of the first quantity of plastic which is located transversely across the apex of the core from the retraction passage.
Claim 26
Dependent Claim
24 words
A method according to claim 18 where the flow path/s (7) partly consist of molten plastics material which has not completely solidified by cooling.
Claim 27
Dependent Claim
17 words
A method according to claim 15 wherein all the injected plastic is injected through a single gate.