Abstract

Abstract A composition which is curable upon exposure to moisture comprising an organic polymer having at least one silicon bonded hydrolyzable group and an alcohol, wherein the composition is storable for long periods of time without any substantial increase in its viscosity.

Inventors

  • 👤 Yasushi Kato
  • 👤 Hisao Furukawa
  • 👤 Saori Nakatsuka

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 12:56
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/04; C08K5/05

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 172 words
A method of storing a polymer having a silyl group for long periods of time without any substantial amount of increase in the viscosity of said polymer, consisting of mixing 100 parts by weight of said polymer, said polymer having at least one silyl group per molecule having the formula: ##STR2## wherein R.sub., R 2 , R 3 is a hydrogen atom or a monovalent hydrocarbon group selected form alkyl, aryl, or aralkyl group having 1 to 10 carbon atoms, X is a group selected from alkoxy, acryloxy, aminooxy, phenoxy, thioalkyoxy, or amino group, and a is an integer 0, 1 or 2, with about 10 to 50 parts by weight of a stabilizer consisting of one or more aliphatic or aromatic monohydric alcohol having 1 to 10 carbon atoms; and wherein said polymer is a member selected from the group consisting of polyester, polether, ether-ester block copolymer, vinyl polymer, diallyl phthalate monomer or polymer, and a mixture thereof; and wherein said polymer has a molecular weight of between 1,200 and 9,000.
Claim 2
Independent Claim 172 words
A method of storing a polymer having a silyl group for long periods of time without any substantial amount of increase in the viscosity of said polymer, consisting of mixing 100 parts by weight of said polymer, said polymer having at least one silyl group per molecule having the formula: ##STR2## wherein R.sub., R 2 , R 3 is a hydrogen atom or a monovalent hydrocarbon group selected form alkyl, aryl, or aralkyl group having 1 to 10 carbon atoms, X is a group selected from alkoxy, acryloxy, aminooxy, phenoxy, thioalkyoxy, or amino group, and a is an integer 0, 1 or 2, with about 10 to 50 parts by weight of a stabilizer consisting of one or more aliphatic or aromatic monohydric alcohol having 1 to 10 carbon atoms; and wherein said polymer is a member selected from the group consisting of polyester, polether, ether-ester block copolymer, vinyl polymer, diallyl phthalate monomer or polymer, and a mixture thereof; and wherein said polymer has a molecular weight of between 1,200 and 9,000.
Claim 3
Dependent Claim 162 words
A composition consisting of a stabilizer consisting of an alcohol and a polymer having at least one silyl group per molecule of the general formula: ##STR3## wherein R 1 , R 2 , R 3 is a hydrogen atom or a monovalent hydrocarbon group selected from alkyl, aryl or aralkyl group having 1 to 10 carbon atoms, X is a group selected from alkoxy, acyloxy, aminoxy, phenoxy, thioalkoxy or amino group, and a is an integer of 0, 1 or 2; and wherein said alcohol is one or more aliphatic or aromatic monohydric alcohol having 1 to 10 carbon atoms in an amount of from about 10 to 50 parts by weight to 100 parts by weight of said polymer; and wherein said polymer is a member selected from the group consisting of polyester, polyether, ether-ester block copolymer, vinyl polymer, diallyl phthalate monomer or polymer and a mixture thereof; and wherein said polymer has a molecular weight of between 1,200 and 9,000.
Claim 4
Dependent Claim 162 words
A composition consisting of a stabilizer consisting of an alcohol and a polymer having at least one silyl group per molecule of the general formula: ##STR3## wherein R 1 , R 2 , R 3 is a hydrogen atom or a monovalent hydrocarbon group selected from alkyl, aryl or aralkyl group having 1 to 10 carbon atoms, X is a group selected from alkoxy, acyloxy, aminoxy, phenoxy, thioalkoxy or amino group, and a is an integer of 0, 1 or 2; and wherein said alcohol is one or more aliphatic or aromatic monohydric alcohol having 1 to 10 carbon atoms in an amount of from about 10 to 50 parts by weight to 100 parts by weight of said polymer; and wherein said polymer is a member selected from the group consisting of polyester, polyether, ether-ester block copolymer, vinyl polymer, diallyl phthalate monomer or polymer and a mixture thereof; and wherein said polymer has a molecular weight of between 1,200 and 9,000.

References Cited (Backward Citations)

US4157321A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-03-04 1988-09-03 1989-03-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-03-04 1992-09-03 1993-03-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-03-04 1996-09-03 1997-03-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag