Patent US4496313A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4496313A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of calcining minerals containing heat-value components

Assignee: BKMI Industrieanlagen GmbH
•
Filing: 1982-09-24
•
Granted: 1985-01-29
•
Expires: 2002-09-24
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of calcining mineral components such as bituminous limestone in which heat is recovered from the calcining process and is used to liberate volatilizable substances within the mineral matter before the latter is subjected to calcination. The volatilized and pyrolytically decomposed substances form a fuel which is burned to produce the calcining gas mixture.

Inventors

  • 👤 Wolfram Quittkat
  • 👤 Gerhard Reuter
  • 👤 Rudiger Schmidt

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:33
CPC Classifications
C; C04; C04B; C04B2/00; C04B2/10; C04B2/108

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 222 words
A method of calcining mineral matter containing heat value in the form of volatilizable combustible organic substances, comprising the steps of: (a) burning a gas mixture of air and said volatilizable substances from the volatilization thereof and calcining the mineral matter following removal of at least a substantial portion of said volatilizable substances therefrom to form a hot calcined product at a location different from that at which the removal was effected; (b) recovering heat from said hot calcined product; and (c) subjecting the mineral matter containing the volatilizable substances to the recovered heat at a location different from that at which calcination occurs to drive said volatilizable substances from said mineral matter containing same to thereby form a combustible gas mixture from said substances for use in step (a) and a mineral matter from which said substances have been removed for calcination in a repetition of step (a) for the latter mineral matter, said hot product being subjected to cooling with air, said gas mixture in step (a) including cooling air heated by said hot product, the volatilizable substances being driven out of said mineral matter by passing same and a hot gas in codirectional flow in a rotary furnace and thereafter passing the burning gas mixture and said mineral matter for calcination in a codirectional flow through a rotary furnace.
Claim 2
Independent Claim 222 words
A method of calcining mineral matter containing heat value in the form of volatilizable combustible organic substances, comprising the steps of: (a) burning a gas mixture of air and said volatilizable substances from the volatilization thereof and calcining the mineral matter following removal of at least a substantial portion of said volatilizable substances therefrom to form a hot calcined product at a location different from that at which the removal was effected; (b) recovering heat from said hot calcined product; and (c) subjecting the mineral matter containing the volatilizable substances to the recovered heat at a location different from that at which calcination occurs to drive said volatilizable substances from said mineral matter containing same to thereby form a combustible gas mixture from said substances for use in step (a) and a mineral matter from which said substances have been removed for calcination in a repetition of step (a) for the latter mineral matter, said hot product being subjected to cooling with air, said gas mixture in step (a) including cooling air heated by said hot product, the volatilizable substances being driven out of said mineral matter by passing same and a hot gas in codirectional flow in a rotary furnace and thereafter passing the burning gas mixture and said mineral matter for calcination in a codirectional flow through a rotary furnace.
Claim 3
Dependent Claim 62 words
The method defined in claim 1 wherein a hot gas is said air and is introduced by shell blowers into the rotary furnace for the driving out of the volatilizable substances from said mineral matter, the calcination being effected after an ignition of said mixture by dosed air supply in a temperature range slightly above the dissociation temperature of the mineral matter.

References Cited (Backward Citations)

DE1251688B Cited
US3881862A Cited
US3929417A Cited
US3891382A Cited
US4043746A Cited
US4014641A Cited
US4198273A Cited
US4370127A Cited
US4217092A Cited
US4299564A Cited
US4353750A Cited
US4342598A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-01-29 1988-07-30 1989-01-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-01-29 1992-07-30 1993-01-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-01-29 1996-07-30 1997-01-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag