Abstract An optical fiber coating comprising a thermoplastic rubber block copolymer reduces microbending losses over a wide service temperature range, typically down to at least -40 degrees Celsius, while obtaining an upper temperature limit of typically at least 90 degrees Celsius. The processing properties, including shelf life, cure rate, and toughness, are superior to typical prior art materials, such as silicones. The inventive coating can be used as the inner coating of a dual-layer coated fiber or as an outer or single coating layer.

Inventors

  • 👤 Alvin C. Levy

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 18:54
CPC Classifications
G; G02; G02B; G02B1/00; G02B1/04; G02B1/045; G02B1/048; G02B6/00; G02B6/02; G02B6/02395

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 183 words
A coated optical fiber comprising an optical fiber and one or more coated layers thereon, characterized in that at least one coated layer comprises a mixture of: (X) An ASTM type 103, 104A, 104B, or mixture thereof, napthenic or paraffinic oil, with a wax optionally substituted for a portion of said oil; (Y) a styrene-rubber-styrene block copolymer having a styrene-rubber ratio of 0.2 to 0.5; and optionally (Z) a coumarone-indene copolymer or vinyl toluene -α methyl styrene copolymer; and further comprises a thermal oxidative stabilizer, wherein the ingredients X, Y, and Z have relative proportions by weight falling within the shaded area bounded by A'B'C'D' of FIG. 2 for a styrene-rubber-styrene block copolymer having a viscosity of 1190 cps and with the acceptable proportions of said block copolymer adjusted corresponding to a reduction by 3 parts for block copolymer material having a viscosity of 1800 cps, and to an increase by 6 parts for block copolymer material having a viscosity of 500 cps, with said viscosity being measured for a solution of 20 weight percent block copolymer in toluene at 25 degrees Celsius.
Claim 2
Dependent Claim 183 words
A coated optical fiber comprising an optical fiber and one or more coated layers thereon, characterized in that at least one coated layer comprises a mixture of: (X) An ASTM type 103, 104A, 104B, or mixture thereof, napthenic or paraffinic oil, with a wax optionally substituted for a portion of said oil; (Y) a styrene-rubber-styrene block copolymer having a styrene-rubber ratio of 0.2 to 0.5; and optionally (Z) a coumarone-indene copolymer or vinyl toluene -α methyl styrene copolymer; and further comprises a thermal oxidative stabilizer, wherein the ingredients X, Y, and Z have relative proportions by weight falling within the shaded area bounded by A'B'C'D' of FIG. 2 for a styrene-rubber-styrene block copolymer having a viscosity of 1190 cps and with the acceptable proportions of said block copolymer adjusted corresponding to a reduction by 3 parts for block copolymer material having a viscosity of 1800 cps, and to an increase by 6 parts for block copolymer material having a viscosity of 500 cps, with said viscosity being measured for a solution of 20 weight percent block copolymer in toluene at 25 degrees Celsius.
Claim 3
Dependent Claim 31 words
The coated optical fiber of claim 1 wherein 0 to 12 percent microcrystalline wax substitutes for 0 to 12 percent of said oil, based on total weight percentage of said mixture.
Claim 4
Dependent Claim 22 words
The coated fiber of claim 1 wherein said at least one coated layer is the inner layer of a dual-layer coated fiber.
Claim 5
Dependent Claim 144 words
A coated optical fiber comprising an optical fiber and one or more coated layers thereon, characterized in that at least one coated layer comprises a mixture of: (X) an ASTM type 103, 104A, 104B, or mixture thereof, napthenic or paraffinic oil, with a wax optionally substituted for a portion of said oil; (Y) a styrene-rubber-styrene block copolymer having a styrene-rubber ratio of 0.2 to 0.5; and optionally (Z) a coumarone-indene copolymer; and further comprises a thermal oxidative stabilizer; and wherein said at least one coated layer is the inner layer of a dual-layer coated fiber, and wherein said mixture comprises by weight 59 to 61 percent of said oil; 24 to 26 percent of said styrene-ethylene butylene-styrene block copolymer; 4 to 6 percent of said coumarone-indene copolymer; 8 to 10 percent of said wax; and 0.5 to 1.5 percent of said thermal oxidative stabilizer.
Claim 6
Dependent Claim 144 words
A coated optical fiber comprising an optical fiber and one or more coated layers thereon, characterized in that at least one coated layer comprises a mixture of: (X) an ASTM type 103, 104A, 104B, or mixture thereof, napthenic or paraffinic oil, with a wax optionally substituted for a portion of said oil; (Y) a styrene-rubber-styrene block copolymer having a styrene-rubber ratio of 0.2 to 0.5; and optionally (Z) a coumarone-indene copolymer; and further comprises a thermal oxidative stabilizer; and wherein said at least one coated layer is the inner layer of a dual-layer coated fiber, and wherein said mixture comprises by weight 59 to 61 percent of said oil; 24 to 26 percent of said styrene-ethylene butylene-styrene block copolymer; 4 to 6 percent of said coumarone-indene copolymer; 8 to 10 percent of said wax; and 0.5 to 1.5 percent of said thermal oxidative stabilizer.

References Cited (Backward Citations)

US3464850A Cited
US3876405A Cited
US4167305A Cited
US4198121A Cited
US4042555A Cited
US4147407A Cited
US4105284A Cited
US4114981A Cited
US4259540A Cited
US4286019A Cited
US4432607A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-01-08 1988-07-09 1989-01-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-01-08 1992-07-09 1993-01-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-01-08 1996-07-09 1997-01-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag