Amorphous silicon photovoltaic device including a two-layer transparent electrode

Assignee: Kanegafuchi Chemical Industry Co Ltd
•
Filing: 1983-11-17
•
Granted: 1985-01-01
•
Expires: 2003-11-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An amorphous silicon semiconductor of the general formula: a-Si.sub.(1-x-y) C x N y containing hydrogen and/or fluorine, which provides an amorphous silicon PIN junction photovoltaic device having an improved conversion efficiency when it is used as a P-type or N-type semiconductor in the layer on the light impinging side of the PIN junction photovoltaic device. Also, the conversion efficiency of an amorphous silicon PIN junction photovoltaic device is improved by using a film of ITO and SnO 2 two layer structure as a transparent electrode for the photovoltaic device with the SnO 2 layer contacting the P or N layer, and the improvement is particularly marked in the heterojunction photovoltaic device.

Inventors

  • 👤 Yoshihiro Hamakawa
  • 👤 Yoshihisa Tawada

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 11:44
CPC Classifications
H; H10; H10F; H10F71/00; H10F71/10; H10F71/103; H10F10/00; H10F10/10; H10F10/17; H10F77/00; H10F77/10; H10F77/16; H10F77/162; H10F77/166; H10F77/20; H10F77/244; H10F77/247; Y; Y02; Y02E; Y02E10/00; Y02E10/50; Y02E10/548; Y02P; Y02P70/00; Y02P70/50; Y10; Y10S; Y10S420/00; Y10S420/903

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 47 words
In an amorphous silicon derivative PIN junction photovoltaic device, the improvement comprising a two-layer transparent electrode consisting of ITO and SnO 2 layers that are provided on the P or N layer so that the SnO 2 layer is in contact with said P or N layer.
Claim 2
Dependent Claim 47 words
In an amorphous silicon derivative PIN junction photovoltaic device, the improvement comprising a two-layer transparent electrode consisting of ITO and SnO 2 layers that are provided on the P or N layer so that the SnO 2 layer is in contact with said P or N layer.
Claim 3
Dependent Claim 22 words
The photovoltaic device of claim 1, wherein said SnO 2 layer has a thickness of between about 30 to about 500 angstroms.
Claim 4
Dependent Claim 67 words
The photovoltaic device of claim 1, wherein the amorphous semiconductor of said P or N layer which contacts the SnO 2 layer is a member selected from the group consisting of an amorphous semiconductor of the general formula: a-Si.sub.(1-x) C x , an amorphous semiconductor of the general formula: a-Si.sub.(1-y) N y , and an amorphous semiconductor of the general formula: a-Si.sub.(1-x-y) C x N y .
Claim 5
Dependent Claim 30 words
The photovoltaic device of claim 1, wherein at least one of the P or N layers is an amorphous semiconductor of the general formula: a-Si.sub.(1-x-y) C x N y .
Claim 6
Dependent Claim 28 words
The photovoltaic device of claim 1, comprising an amorphous silicon semiconductor which is doped with a P-type or an N-type impurity to form the P or N layer.
Claim 7
Dependent Claim 24 words
The photovoltaic device of claim 5, comprising a doped amorphous semiconductor having an electric conductivity of not less than 10 -8 (Ω·cm) -1 .
Claim 8
Dependent Claim 26 words
The photovoltaic device of claim 6, wherein said doped amorphous semiconductor is an amorphous silicon semiconductor of the general formula: a-Si.sub.(1-x-y) C x N y .
Claim 9
Dependent Claim 24 words
The photovoltaic device of claim 7, wherein the values, x and y, in the general formula satisfy the following equations: 0.05≦x≦0.75; 0.05≦y≦0.75; and 0.05≦x+y≦0.80.
Claim 10
Dependent Claim 10 words
The photovoltaic device of claim 1 including a PIN heterojunction.
Claim 11
Dependent Claim 25 words
The photovoltaic device of claim 9, wherein at least one of the P, I and N layers contains at least one of hydrogen and fluorine.
Claim 12
Dependent Claim 23 words
The photovoltaic device of claim 10 in which the P or N layer is located on a light impinging side of the device.

References Cited (Backward Citations)

JPS5529154A Cited
JPS57204182A Cited
EP0070509A2 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-01-01 1988-07-02 1989-01-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-01-01 1992-07-02 1993-01-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-01-01 1996-07-02 1997-01-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag