Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
197 words
A substituted pyrrole polymer ("polypyrrole") linked through N-adjacent carbon atoms of the pyrrole nucleus, said polymer being represented by the structure: ##STR14## wherein, n' is an integer in the range from 2 to about 100, and more preferably in the range from about 20 to about 80; n is an integer in the range from 3 to about 5, so that at least one C atom in the polymethylene ring is distally located relative to the 3- and 4-C atoms on the pyrrole ring; R 1 and R 2 , if present, are independently selected from phenyl, hydroxyphenyl, cycloalkyl having from 4 to about 7 carbon atoms, lower alkyl, alkoxy and hydroxyalkyl each having from 1 to about 6 carbon atoms, and each substituent may be on the same C atom, or different C atoms, distally located from the 3- and 4-C atoms of the pyrrole ring; and, X, if present, is selected from the group consisting of ##STR15## either of which may be substituted, and which are connected to the alkylene ring with a single bond; and, ##STR16## any of which may be substituted, and which are connected to the alkylene ring with a double bond.
Claim 2
Dependent Claim
197 words
A substituted pyrrole polymer ("polypyrrole") linked through N-adjacent carbon atoms of the pyrrole nucleus, said polymer being represented by the structure: ##STR14## wherein, n' is an integer in the range from 2 to about 100, and more preferably in the range from about 20 to about 80; n is an integer in the range from 3 to about 5, so that at least one C atom in the polymethylene ring is distally located relative to the 3- and 4-C atoms on the pyrrole ring; R 1 and R 2 , if present, are independently selected from phenyl, hydroxyphenyl, cycloalkyl having from 4 to about 7 carbon atoms, lower alkyl, alkoxy and hydroxyalkyl each having from 1 to about 6 carbon atoms, and each substituent may be on the same C atom, or different C atoms, distally located from the 3- and 4-C atoms of the pyrrole ring; and, X, if present, is selected from the group consisting of ##STR15## either of which may be substituted, and which are connected to the alkylene ring with a single bond; and, ##STR16## any of which may be substituted, and which are connected to the alkylene ring with a double bond.
Claim 3
Dependent Claim
57 words
The polypyrrole of claim 1 obtained by the electrodeposition of a monomer from a solvent for it, in the presence of an electrolyte which generates an acid ion, said monomer having the structure: ##STR17## wherein, n, and each R 1 , R 2 and X, if any is present, have the same connotation as in claim 1.
Claim 4
Dependent Claim
17 words
The polypyrrole of claim 2 obtained as a powdery deposit which is compactable into a shaped article.
Claim 5
Dependent Claim
34 words
The polypyrrole of claim 3 wherein said electrolyte is an alkylammonium salt, and said polymer has a conductivity in the range from about 10 -5 to about 10 2 ohm -1 cm -1 (S/cm).
Claim 6
Dependent Claim
20 words
The polypyrrole of claim 4, including: poly[1-azabicyclo[3,3,0]octa-2,4-diene]; poly[1-azabicyclo[3,4,0]nona-2,4-diene]; poly[7-phenyl-1-azabicyclo[3,3,0]octa-2,4 -diene]; poly[7-methoxy-8-methyl-1-azabicyclo[3,3,0]octa-2,4-diene]; poly[7-dimethyl-1-azabicyclo[3,3,0]octa-2,4-diene]; poly[7-benzyl-8-methyl-1-azabicyclo[3,3,0]octa-2,4-diene]; poly[7-methyl-8-benzyl-1-azabicyclo[3,4,0]nona-2,4-diene]; poly[7-(4-pyridylmethyl)-1-azabicylo[3,3,0]octa-2,4-diene]; poly[bis[7,8-benzylidene]-1-azabicyclo[3,4,0]nona-2,4-diene]; poly[7-propylidene-1-azabicyclo[3,3,0]octa-2,4-diene]; poly[7-(2,4,7-trinitro-9-fluorenylidene)-1-azabicyclo[3,3,0]octa-2,4-diene]; and, poly[7-(2-thiophenemethylene)-1-azabicyclo[3,3,0]octa-2,4-diene].
Claim 7
Dependent Claim
219 words
A process for polymerizing a substituted pyrrole monomer, comprising, (a) forming a solution of said monomer and an electrolyte which generates an acid ion in a mutual solvent, said monomer having the structure ##STR18## wherein, n is an integer in the range from 3 to about 5, so that at least one C atom in the polymethylene ring is distally located relative to the 3- and 4-C atoms on the pyrrole ring; R 1 and R 2 , if present, are independently selected from phenyl, hydroxyphenyl, cycloalkyl having from 4 to about 7 carbon atoms, lower alkyl, alkoxy and hydroxyalkyl each having from 1 to about 6 carbon atoms, and each substituent may be on the same C atom, or different C atoms, distally located from the 3- and 4-C atoms of the pyrrole ring; and, X, if present, is selected from the group consisting of ##STR19## either of which may be substituted, and which are connected to the alkylene ring with a single bond; and, ##STR20## any of which may be substituted, and which are connected to the alkylene ring with a double bond; (b) passing electrical current between electrodes placed in said solution at an applied voltage and intensity sufficient to deposit a polymer on the anode; and, (c) recovering a compactable powdery deposit of said polymer.
Claim 8
Dependent Claim
219 words
A process for polymerizing a substituted pyrrole monomer, comprising, (a) forming a solution of said monomer and an electrolyte which generates an acid ion in a mutual solvent, said monomer having the structure ##STR18## wherein, n is an integer in the range from 3 to about 5, so that at least one C atom in the polymethylene ring is distally located relative to the 3- and 4-C atoms on the pyrrole ring; R 1 and R 2 , if present, are independently selected from phenyl, hydroxyphenyl, cycloalkyl having from 4 to about 7 carbon atoms, lower alkyl, alkoxy and hydroxyalkyl each having from 1 to about 6 carbon atoms, and each substituent may be on the same C atom, or different C atoms, distally located from the 3- and 4-C atoms of the pyrrole ring; and, X, if present, is selected from the group consisting of ##STR19## either of which may be substituted, and which are connected to the alkylene ring with a single bond; and, ##STR20## any of which may be substituted, and which are connected to the alkylene ring with a double bond; (b) passing electrical current between electrodes placed in said solution at an applied voltage and intensity sufficient to deposit a polymer on the anode; and, (c) recovering a compactable powdery deposit of said polymer.