Patent US4485163A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4485163A Expired / Lapsed US ⏱️ 0.0 years remaining

One-component magnetic dry developer comprises triiron tetroxide having specified coercive force and vinyl aromatic polymer and process of use

Assignee: Kyocera Mita Industrial Co Ltd
•
Filing: 1982-06-02
•
Granted: 1984-11-27
•
Expires: 2002-06-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A one-component magnetic dry developer for use in development of positively charged images and transfer of developed images, comprises particles of a composition comprising a vinyl aromatic polymer, an aliphatic carboxylic acid having at least 14 carbon atoms, inclusive of the carbon atom of the carboxyl group, per carboxyl group or its metal salt and a finely divided magnetic material having a coercive force not larger than 120 Oe and a bulk density of at least 0.45 g/ml. This magnetic developer provides an excellent transferred image having high image density and image sharpness on a plain paper as a transfer sheet without fogging or broadening of the contour of the image.

Inventors

  • 👤 Nobuhiro Miyakawa

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 20:18
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/083; G03G9/0837; G03G9/0835; G03G9/0836; G03G9/097; G03G9/09733; G03G9/09783; G03G9/09791; Y; Y10; Y10S; Y10S430/00; Y10S430/001; Y10S430/104

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 188 words
An electrostatic photographic reproduction process which comprises contacting a selenium photoconductive substrate carrying a positively charged electrostatic image with a magnetic brush of a one-component magnetic dry developer to effect development of the latent image and electrostatically transfer the formed image of the developer onto a transfer sheet, wherein the one-component magnetic dry developer consists essentially of particles of a composition comprising (A) a finely divided magnetic material composed of triiron tetroxide having a coercive force not larger than 120 Oe, a bulk density of at least 0.45 g/ml and a shape anisotropic characteristic, as defined as the longest size/shortest size ratio, in the range of from 1.0 to 5.5, (B) 0.2 to 4% by weight, based on the amount of the finely divided magnetic material, of an aliphatic carboxylic acid having at least 14 carbon atoms, inclusive of the carbon atom of the carboxyl group, per carboxyl group or a metal salt thereof, and (C) 45 to 95% by weight, based on the amount of the finely divided magnetic material, of a vinyl aromatic polymer containing at least 25% by weight of a vinyl aromatic monomer component.
Claim 2
Dependent Claim 188 words
An electrostatic photographic reproduction process which comprises contacting a selenium photoconductive substrate carrying a positively charged electrostatic image with a magnetic brush of a one-component magnetic dry developer to effect development of the latent image and electrostatically transfer the formed image of the developer onto a transfer sheet, wherein the one-component magnetic dry developer consists essentially of particles of a composition comprising (A) a finely divided magnetic material composed of triiron tetroxide having a coercive force not larger than 120 Oe, a bulk density of at least 0.45 g/ml and a shape anisotropic characteristic, as defined as the longest size/shortest size ratio, in the range of from 1.0 to 5.5, (B) 0.2 to 4% by weight, based on the amount of the finely divided magnetic material, of an aliphatic carboxylic acid having at least 14 carbon atoms, inclusive of the carbon atom of the carboxyl group, per carboxyl group or a metal salt thereof, and (C) 45 to 95% by weight, based on the amount of the finely divided magnetic material, of a vinyl aromatic polymer containing at least 25% by weight of a vinyl aromatic monomer component.
Claim 3
Dependent Claim 33 words
A process according to claim 1, wherein the finely divided magnetic material is triiron tetroxide of an isometric system or rounded amorphous triiron tetroxide having a particle size of 0.3 to 1 micron.
Claim 4
Dependent Claim 23 words
A process according to claim 1, wherein the aliphatic carboxylic acid or its salt has a melting point of at least 45° C.
Claim 5
Dependent Claim 21 words
A process according to claim 1, wherein the metal salt of the aliphatic carboxylic acid is a water-insoluble polyvalent metal salt.
Claim 6
Independent Claim 324 words
A method for developing and transferring a positively charged electrostatic latent image carried on a selenium photoconductive substrate which comprises contacting the latent image with a magnetic brush of a friction-chargeable one-component magnetic dry developer consisting essentially of particles of a composition comprising (A) from about 50 to 60% by weight, based on the total weight of the composition, of a finely divided magnetic material composed of triiron tetroxide of an isometric system or rounded amorphous triiron tetroxide having a particle size of 0.3 to 1 micron, a shape anisotropic characteristic, as defined as the longest size/shortest size ratio, in the range of from 1.0 to 5.5, a coercive force not larger than 120 Oe, and a bulk density of at least 0.45 g/ml, (B) 0.2 to 0.4% by weight, based on the amount of the finely divided magnetic material (A), of an aliphatic monocarboxylic acid having at least 18 carbon atoms, inclusive of the carbon atom of the carboxyl group, per carboxyl group, or a metal salt thereof and (C) 45 to 95% by weight, based on the amount of the finely divided magnetic material (A) of a vinyl aromatic polymer containing at least 25% by weight of a vinyl aromatic monomer component represented by the following formula: ##STR4## wherein R 1 stands for a hydrogen atom, a lower alkyl group having up to 4 carbon atoms or a halogen atom, R 2 stands for a substituent such as a lower alkyl group or a halogen atom, and n is an integer or 0, 1 or 2, wherein the developer particles become stably negatively charged by frictional contact without subjecting the magnetic brush to a corona discharge, whereby the latent image is developed by the developed particles, and electrostatically transferring the developed latent image onto a plain paper transfer sheet whereby a transferred image having high image density and image sharpness without fogging or broadening of the contour of the image is obtained.
Claim 7
Independent Claim 324 words
A method for developing and transferring a positively charged electrostatic latent image carried on a selenium photoconductive substrate which comprises contacting the latent image with a magnetic brush of a friction-chargeable one-component magnetic dry developer consisting essentially of particles of a composition comprising (A) from about 50 to 60% by weight, based on the total weight of the composition, of a finely divided magnetic material composed of triiron tetroxide of an isometric system or rounded amorphous triiron tetroxide having a particle size of 0.3 to 1 micron, a shape anisotropic characteristic, as defined as the longest size/shortest size ratio, in the range of from 1.0 to 5.5, a coercive force not larger than 120 Oe, and a bulk density of at least 0.45 g/ml, (B) 0.2 to 0.4% by weight, based on the amount of the finely divided magnetic material (A), of an aliphatic monocarboxylic acid having at least 18 carbon atoms, inclusive of the carbon atom of the carboxyl group, per carboxyl group, or a metal salt thereof and (C) 45 to 95% by weight, based on the amount of the finely divided magnetic material (A) of a vinyl aromatic polymer containing at least 25% by weight of a vinyl aromatic monomer component represented by the following formula: ##STR4## wherein R 1 stands for a hydrogen atom, a lower alkyl group having up to 4 carbon atoms or a halogen atom, R 2 stands for a substituent such as a lower alkyl group or a halogen atom, and n is an integer or 0, 1 or 2, wherein the developer particles become stably negatively charged by frictional contact without subjecting the magnetic brush to a corona discharge, whereby the latent image is developed by the developed particles, and electrostatically transferring the developed latent image onto a plain paper transfer sheet whereby a transferred image having high image density and image sharpness without fogging or broadening of the contour of the image is obtained.

References Cited (Backward Citations)

US3510338A Cited
US3577345A Cited
US3645770A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-11-27 1988-05-28 1988-11-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-11-27 1992-05-28 1992-11-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-11-27 1996-05-28 1996-11-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag