US4463083A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Thermal recording elements
Assignee: Fujifilm Holdings Corp
•
Filing: 1982-05-11
•
Granted: 1984-07-31
•
Expires: 2002-05-11
Abstract
Abstract A thermal recording element comprising a support having formed thereon a recording layer, a first protective layer comprising an organic high molecular weight material having a softening point below about 70° C. formed on the recording layer, and a second protective layer comprising an organic high molecular weight material having high mechanical strength.
Inventors
- 👤 Masao Kitajima
- 👤 Osamu Seshimoto
- 👤 Tomizo Namiki
- 👤 Fumiaki Shinozaki
- 👤 Tomoaki Ikeda
- 👤 Yuzo Mizobuchi
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 13:08
CPC Classifications
G; G11; G11B; G11B7/00; G11B7/24; G11B7/241; G11B7/252; G11B7/257; G11B7/2572; G11B7/2575; G11B7/254; G11B7/2542; G11B7/242; G11B7/243; G11B2007/24302; G11B2007/2431; G11B2007/24312; G11B2007/24318; G11B2007/24324; G11B2007/24326; G11B7/253; G11B7/2533; G11B7/2535; Y; Y10; Y10S; Y10S430/00; Y10S430/146; Y10S430/151; Y10S430/162; Y10S430/165
Claims Analysis
Total Claims: 13
Claim 1
Independent Claim
125 words
A thermal recording element for recording information by thermally deforming a recording layer comprising a metal using a high intensity radiation and recording information by the change in the light transmitting and reflecting properties of the recording layer, comprising a support having formed thereon the recording layer, a first protective layer having a thickness of about 1 to 10 μm formed by coating a polymer having a softening point lower than about 70° C. on the recording layer, and a second protective layer having a thickness of about 1 to 10 μm formed by coating a polymer material having high mechanical strength on the first protective layer, said first protective layer minimizing decrease in sensitivity of the recording layer due to the second protective layer.
Claim 2
Dependent Claim
125 words
A thermal recording element for recording information by thermally deforming a recording layer comprising a metal using a high intensity radiation and recording information by the change in the light transmitting and reflecting properties of the recording layer, comprising a support having formed thereon the recording layer, a first protective layer having a thickness of about 1 to 10 μm formed by coating a polymer having a softening point lower than about 70° C. on the recording layer, and a second protective layer having a thickness of about 1 to 10 μm formed by coating a polymer material having high mechanical strength on the first protective layer, said first protective layer minimizing decrease in sensitivity of the recording layer due to the second protective layer.
Claim 3
Dependent Claim
13 words
The thermal recording element of claim 1, wherein said support is polyethylene terephthalate.
Claim 4
Dependent Claim
19 words
The thermal recording element of claim 1, wherein said recording layer is a layer of Sn, Bi or In.
Claim 5
Dependent Claim
47 words
The thermal recording element of claim 1, wherein said recording layer is composed of a mixture of Sn, Bi or In and Ges, SnS or PbI 2 or composed of a layer of Sn, Bi or In and a layer of GeS, SnS or PbI 2 .
Claim 6
Dependent Claim
20 words
The thermal recording element of claim 1, wherein the thickness of said recording layer is about 300 to 1,500 Å.
Claim 7
Dependent Claim
35 words
The thermal recording element of claim 1, wherein said polymer has a softening point of lower than 70° C. is an ethylene-vinyl acetate copolymer containing more than 10 wt. % vinyl acetate, or polychlorosulfonated polyethylene.
Claim 8
Dependent Claim
59 words
The thermal recording element of claim 1, wherein the polymer used for the second protective layer is a copolymer of vinyl chloride and vinyl acetate, polyvinyl chloride, acetyl cellulose, polyethylene terephthalate, polyimide, polyurethane, polyvinylidene fluoride, polyvinyl butyral, polyvinyl formal, polyvinyl alcohol, polyvinylidene chloride, polyethylene, polyvinyl pyrrolidone, polyvinyl acrylamide, nylon, polycarbonate, polypropylene, polystyrene, polybutene, polyethylene trifluorochloride, or poly(metha)acrylic acid ester.
Claim 9
Dependent Claim
20 words
The thermal recording element of claim 1, wherein said element has further an overcoat layer on the second protective layer.
Claim 10
Dependent Claim
23 words
The thermal recording element of claim 8, wherein said overcoat is composed of a higher fatty acid or a higher fatty acid amide.
Claim 11
Dependent Claim
33 words
The thermal recording element of claim 1, wherein the thickness of said first protective layer is 2 to 6 μm and the thickness of said second protective layer is 2 to 6 μm.
Claim 12
Dependent Claim
23 words
The thermal recording element of claim 10, wherein the combined thickness of said first and second protective layers is less than 10 μm.
Claim 13
Dependent Claim
59 words
The thermal recording element of claim 1, wherein said polymer used for the first protective layer is an ethylene-vinyl acetate copolymer containing more than 10 wt. % of vinyl acetate or polychlorosulfonated polyethylene, and said polymer used for the second protective layer is vinyl chloride-vinyl acetate copolymer, alcohol-soluble nylon, polyvinyl butyral, polyurethane, polyvinylidene choride, polyacrylate, ethyl cellulose or polyethylene.
References Cited (Backward Citations)
US4069487A
Cited
US4112013A
Cited
US4237468A
Cited
US4101907A
Cited
US4170683A
Cited
US4282534A
Cited
US4309713A
Cited
US4268575A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-07-31 | 1988-01-30 | 1988-07-31 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-07-31 | 1992-01-30 | 1992-07-31 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-07-31 | 1996-01-30 | 1996-07-31 | $7700.00 | Window Closed / Lapsed |