Claims Analysis
Total Claims: 17
Claim 1
Independent Claim
232 words
Method of producing light olefinic hydrocarbons having 2-5 carbons from methanol, in particular unsaturated hydrocarbons, in the presence of a zeolitic mordenite catalyst, wherein gasified methanol introduced into a carrier gas, the concentration of the methanol in an entering mixture being between 5 and 60% by volume, is passed through a catalytic bed based on dealuminised synthetic mordenite whose Si/Al ratio (atomic) is higher than 80, the methanol flow rate being between 1 and 5 liters of liquid methanol per liter of catalyst and per hour, the reaction being carried out at a temperature between 350° and 550° C., under a pressure which can reach 20 bars; said synthetic mordenite having been de-aluminised by subjecting the mordenite to a series of alternate acid and hydrothermic treatments; during the acid treatment phase, subjecting the mordenite to treatment in a concentrated acid medium, at a temperature between 60° and 90° C., with stirring for some hours; in the hydrothermic treatment phase, bringing the mordenite to a temperature between 550° and 680° C. for some hours, at atmospheric pressure, in an air-steam mixture of which the air-steam flow rate under normal conditions of temperature and pressure is between 500 and 1250 l/h for a weight of catalyst of 1 kg, the steam concentration by volume being between 2.5 and 60%; the series of treatments commencing with an acid treatment and terminating with an acid treatment.
Claim 2
Dependent Claim
232 words
Method of producing light olefinic hydrocarbons having 2-5 carbons from methanol, in particular unsaturated hydrocarbons, in the presence of a zeolitic mordenite catalyst, wherein gasified methanol introduced into a carrier gas, the concentration of the methanol in an entering mixture being between 5 and 60% by volume, is passed through a catalytic bed based on dealuminised synthetic mordenite whose Si/Al ratio (atomic) is higher than 80, the methanol flow rate being between 1 and 5 liters of liquid methanol per liter of catalyst and per hour, the reaction being carried out at a temperature between 350° and 550° C., under a pressure which can reach 20 bars; said synthetic mordenite having been de-aluminised by subjecting the mordenite to a series of alternate acid and hydrothermic treatments; during the acid treatment phase, subjecting the mordenite to treatment in a concentrated acid medium, at a temperature between 60° and 90° C., with stirring for some hours; in the hydrothermic treatment phase, bringing the mordenite to a temperature between 550° and 680° C. for some hours, at atmospheric pressure, in an air-steam mixture of which the air-steam flow rate under normal conditions of temperature and pressure is between 500 and 1250 l/h for a weight of catalyst of 1 kg, the steam concentration by volume being between 2.5 and 60%; the series of treatments commencing with an acid treatment and terminating with an acid treatment.
Claim 3
Dependent Claim
19 words
Method of producing hydrocarbons from methanol, according to claim 1, wherein said Si/Al ratio is between 100 and 150.
Claim 4
Dependent Claim
26 words
Method of producing hydrocarbons from methanol, according to claim 1 or 2, wherein the concentration of the entering methanol is between 30 and 50% by volume.
Claim 5
Dependent Claim
25 words
Method of producing hydrocarbons from methanol, according to claim 1 or 2, wherein unconverted methanol is recycled, possibly conjointly with the dimethylether formed, also recycled.
Claim 6
Dependent Claim
24 words
Method of producing hydrocarbons from methanol according to claim 3, wherein unconverted methanol is recycled, if necessary conjointly with a dimethylether formed, also recycled.
Claim 7
Dependent Claim
89 words
Method of producing hydrocarbons from methanol according to claim 1 or 2, wherein the method is applied with periodic regeneration of the catalyst by combustion in oxygen diluted with an inert gas, at a temperature between 450° and 600° C. for some hours, the hourly volumetric speed under normal conditions of temperature and pressure being between 5,000 and 15,000 h -1 , the oxygen content being of the order of 2% by volume at the start of the regeneration, with gradual increase without exceeding the temperature of 600° C.
Claim 8
Dependent Claim
87 words
Process of producing hydrocarbons from methanol according to claim 3, wherein the method is applied with periodic regeneration of the catalyst by combustion in oxygen diluted with an inert gas, at a temperature between 450° and 600° C. for some hours, the hourly volumetric speed under normal conditions of temperature and pressure being between 5,000 and 15,000 h -1 , the oxygen content being of the order of 2% by volume at the start of the regeneration, with gradual increase without exceeding the temperature of 600° C.
Claim 9
Dependent Claim
100 words
Method of producing hydrocarbons from methanol according to claim 3, wherein unconverted methanol is recycled, if necessary conjointly with dimethylether formed, also recycled, and the method is applied with periodic regeneration of the catalyst by combustion in oxygen diluted with an inert gas, at a temperature between 450° and 600° C. for some hours, the hourly volumetric speed under normal conditions of temperature and pressure being between 5,000 and 15,000 h -1 , the oxygen content being of the order of 2% by volume at the start of the regeneration, with gradual increase without exceeding the temperature of 600° C.
Claim 10
Dependent Claim
126 words
Method for the hydrothermic de-aluminisation of mordenite, comprising subjecting the mordenite to a series of alternate acid and hydrothermic treatments; during the acid treatment phase, subjecting the mordenite to treatment in a concentrated acid medium, at a temperature between 60° and 90° C., with stirring for some hours; in the hydrothermic treatment phase, bringing the mordenite to a temperature between 550° and 680° C. for some hours, at atmospheric pressure, in an air-steam mixture of which the air-steam flow rate under normal conditions of temperature and pressure is between 500 and 1250 l/h for a weight of catalyst of 1 kg, the steam concentration by volume being between 2.5 and 60%; the series of treatments commencing with an acid treatment and terminating by an acid treatment.
Claim 11
Dependent Claim
126 words
Method for the hydrothermic de-aluminisation of mordenite, comprising subjecting the mordenite to a series of alternate acid and hydrothermic treatments; during the acid treatment phase, subjecting the mordenite to treatment in a concentrated acid medium, at a temperature between 60° and 90° C., with stirring for some hours; in the hydrothermic treatment phase, bringing the mordenite to a temperature between 550° and 680° C. for some hours, at atmospheric pressure, in an air-steam mixture of which the air-steam flow rate under normal conditions of temperature and pressure is between 500 and 1250 l/h for a weight of catalyst of 1 kg, the steam concentration by volume being between 2.5 and 60%; the series of treatments commencing with an acid treatment and terminating by an acid treatment.
Claim 12
Dependent Claim
23 words
Method of hydrothermic de-aluminisation of mordenite, according to claim 9, wherein the concentrated acid medium has a normality between 2 and 9 N.
Claim 13
Dependent Claim
28 words
Method of hydrothermic de-aluminisation fof mordenite, according to claim 9, wherein in the hydrothermic treatment phase the mordenite is brought to a temperature between 600° and 650° C.
Claim 14
Dependent Claim
26 words
Method of hydrothermic de-aluminisation of mordenite, according to claim 9, wherein the concentration of steam by volume in the air-steam mixture is between 5 and 35%.
Claim 15
Dependent Claim
43 words
Method of hydrothermic de-aluminisation of mordenite, according to claim 10, wherein during the hydrothermic treatment phase the mordenite is brought to a temperature between 600° and 650° C., and wherein the air-steam mixture has a steam concentration by volume between 5 and 35%.
Claim 16
Dependent Claim
23 words
Doubly de-aluminised mordenite obtained by the method according to claim 9, 10, 11, 12, or 13 wherein the starting material is sodium mordenite.
Claim 17
Dependent Claim
24 words
Doubly de-aluminised mordenite obtained by the method according to claim 9, 10, 11, 12, or 13, wherein the starting material is ammonium form mordenite.