Abstract

Abstract A single, thin walled corrugated electroplating barrel provided with laser formed extremely small perforations, designed and arranged so as to be suitable for handling bulk quantities of minute parts, with perforations performing a pumping action for constant agitation of the plating solution during plating operations.

Inventors

  • 👤 P. David Stutz
  • 👤 George J. Kuchta

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 22:06
CPC Classifications
C; C25; C25D; C25D17/00; C25D17/16; C25D17/18; C25D17/20

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 28 words
An electro-plating barrel comprising: (a) a thin continuous corrugated wall formed from a chemically inert high-tensile strength plastic having a thickness of less than 0.1875 of an inch,
Claim 2
Dependent Claim 28 words
An electro-plating barrel comprising: (a) a thin continuous corrugated wall formed from a chemically inert high-tensile strength plastic having a thickness of less than 0.1875 of an inch,
Claim 3
Dependent Claim 97 words
(b) a multiplicity of laser-formed perforations formed therein with said perforations arranged in longitudinal lines parallel to said corrugations with each line horizontally staggered with respect to each other, (c) each laser-formed perforation includes a slot-like oblong shaped opening formed on the exterior wall surface of said corrugations extending longitudinally thereof with the walls of said openings tapered inwardly to form a reduced oblong oppening on the interior wall surface of said corrugations resulting in a perforated area of not less than 15% and no greater than 30% of the total interior wall surface of the barrel.
Claim 4
Dependent Claim 97 words
(b) a multiplicity of laser-formed perforations formed therein with said perforations arranged in longitudinal lines parallel to said corrugations with each line horizontally staggered with respect to each other, (c) each laser-formed perforation includes a slot-like oblong shaped opening formed on the exterior wall surface of said corrugations extending longitudinally thereof with the walls of said openings tapered inwardly to form a reduced oblong oppening on the interior wall surface of said corrugations resulting in a perforated area of not less than 15% and no greater than 30% of the total interior wall surface of the barrel.
Claim 5
Independent Claim 130 words
A method of constructing an electroplating barrel consisting in the steps of moulding a flat thin sheet of plastic material having a thickness in the range of 0.080 inches to 0.1875 inches into a cylindrical corrugated surface, contacting the cylindrical surface with a focused coherent light energy laser beam to perforate the surface, moving and rotating the cylindrical surface in front of the beam to form rows of perforations, with the surface of the sheet around each perforation annealed by the beam, with each perforation having its walls tapered inwardly of the barrel so as to provide a large open area on the exterior surface of the barrel and a reduced open area on the interior wall surface in the range of 15% to 30% of the total wall surface.
Claim 6
Independent Claim 130 words
A method of constructing an electroplating barrel consisting in the steps of moulding a flat thin sheet of plastic material having a thickness in the range of 0.080 inches to 0.1875 inches into a cylindrical corrugated surface, contacting the cylindrical surface with a focused coherent light energy laser beam to perforate the surface, moving and rotating the cylindrical surface in front of the beam to form rows of perforations, with the surface of the sheet around each perforation annealed by the beam, with each perforation having its walls tapered inwardly of the barrel so as to provide a large open area on the exterior surface of the barrel and a reduced open area on the interior wall surface in the range of 15% to 30% of the total wall surface.

References Cited (Backward Citations)

US2243728A Cited
US3337442A Cited
US3563877A Cited
US3582526A Cited
US3549858A Cited
US3594261A Cited
US3668028A Cited
US4015831A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-05-01 1987-10-31 1988-05-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-05-01 1991-10-31 1992-05-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-05-01 1995-10-31 1996-05-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.