Method of making an electrochemical cell having a safety vent closure

Assignee: Edgewell Personal Care Brands LLC
•
Filing: 1982-02-02
•
Granted: 1984-03-20
•
Expires: 2002-02-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A safety blow-out vent closure for galvanic cells, such as nonaqueous oxyhalide cells, which comprises the employment of a conductive tubular member secured to the cell's housing and surrounding a vent orifice in the cell's housing and wherein a deformable member is force-fitted in said vent orifice and adapted to at least partially be ejected from the vent orifice upon the build up of a predetermined internal gas pressure within the cell. The invention is also directed to a method for assembling an electrochemical cell with the above-described safety vent closure.

Inventors

  • 👤 Ronald L. Zupancic

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 06:47
CPC Classifications
H; H01; H01M; H01M50/00; H01M50/30; H01M50/342; Y; Y02; Y02E; Y02E60/00; Y02E60/10; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49108; Y10T29/4911

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 334 words
A method for assembling an electrochemical cell having a safety vent closure which comprises the steps: (a) providing a metal cell housing comprising a container having an open end, a closed end and an upstanding circumference; (b) inserting a cathode collector shell into said container, said cathode collector being in contact with the inner upstanding circumference of the container thereby adapting the container as the positive terminal of the cell; (c) disposing a separator within and in contact with the inner circumference of the cathode collector shell; (d) inserting a multimember anode comprised of a first half-cylindrical annular member and a second half-cylindrical annular member, each of said members have an inert electrically conductive metal screen disposed against their inner surface wall, said first and second cylindrical half annular members being disposed in an opposing fashion such that an axial cavity is formed therebetween; (e) disposing an electrically conductive spring strip into the axial cavity between the screen-backed anode members such that said strip resiliently biases the two anode members via said strip so as to provide a substantially uniform and continuous pressure contact over the inner wall of the anode members; (f) securing a first metal cover over the open end of said housing, said first cover having at least one vent orifice; (g) securing a second metal cover to the open end of the cell's housing and placing said second metal cover over said first metal cover wherein at least one metal tubular member is secured to said second cover and surrounds the vent orifice defined in said first cover; (h) feeding the liquid cathode/electrolyte of the cell through the vent orifice into the housing; (i) force fitting a deformable member into the vent orifice thereby providing a fluid-tight seal over said vent orifice; and (j) placing a layer of sealant having adhesion to metal within said metal tubular member over the deformable member and the area of the first metal cover defining the vent orifice and surrounded by the tubular member.
Claim 2
Independent Claim 334 words
A method for assembling an electrochemical cell having a safety vent closure which comprises the steps: (a) providing a metal cell housing comprising a container having an open end, a closed end and an upstanding circumference; (b) inserting a cathode collector shell into said container, said cathode collector being in contact with the inner upstanding circumference of the container thereby adapting the container as the positive terminal of the cell; (c) disposing a separator within and in contact with the inner circumference of the cathode collector shell; (d) inserting a multimember anode comprised of a first half-cylindrical annular member and a second half-cylindrical annular member, each of said members have an inert electrically conductive metal screen disposed against their inner surface wall, said first and second cylindrical half annular members being disposed in an opposing fashion such that an axial cavity is formed therebetween; (e) disposing an electrically conductive spring strip into the axial cavity between the screen-backed anode members such that said strip resiliently biases the two anode members via said strip so as to provide a substantially uniform and continuous pressure contact over the inner wall of the anode members; (f) securing a first metal cover over the open end of said housing, said first cover having at least one vent orifice; (g) securing a second metal cover to the open end of the cell's housing and placing said second metal cover over said first metal cover wherein at least one metal tubular member is secured to said second cover and surrounds the vent orifice defined in said first cover; (h) feeding the liquid cathode/electrolyte of the cell through the vent orifice into the housing; (i) force fitting a deformable member into the vent orifice thereby providing a fluid-tight seal over said vent orifice; and (j) placing a layer of sealant having adhesion to metal within said metal tubular member over the deformable member and the area of the first metal cover defining the vent orifice and surrounded by the tubular member.
Claim 3
Dependent Claim 40 words
The method of claim 1 wherein the liquid cathode/electrolyte added in step (h) comprises at least one liquid oxyhalide selected from the group consisting of thionyl chloride, sulfuryl chloride, phosphorous oxychloride, thionyl bromide, chromyl chloride, vanadyl tribromide and selenium oxychloride.
Claim 4
Dependent Claim 26 words
The method of claim 2 wherein the solid anode inserted in step (d) is selected from the group consisting of lithium, sodium, calcium, potassium and aluminum.

References Cited (Backward Citations)

US660051A Cited
US2412169A Cited
US3398026A Cited
US3415690A Cited
US3664878A Cited
US4164070A Cited
US4032696A Cited
US4207385A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-03-20 1987-09-19 1988-03-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-03-20 1991-09-19 1992-03-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-03-20 1995-09-19 1996-03-20 $7700.00 Window Closed / Lapsed