Patent US4435455A successfully refreshed from Google Patents.
US4435455A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Compliant composite tubular liners of fiber reinforced glass/glass-ceramic having utility as gun barrel liners
Assignee: RTX Corp
•
Filing: 1983-01-10
•
Granted: 1984-03-06
•
Expires: 2003-01-10
Abstract
Abstract A compliant tubular liner particularly adapted to withstand brisant forces is disclosed. These liners comprising graphite or silicon carbide fiber reinforced glass or glass-ceramic have a high fracture toughness, a relatively low elastic modulus and a high temperature resistance. These articles are particularly useful as gun barrel liners.
Inventors
- 👤 Karl M. Prewo
- 👤 John J. Brennan
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-25 17:57
CPC Classifications
F; F41; F41A; F41A21/00; F41A21/02; C; C03; C03C; C03C14/00; C03C14/002; C03C2214/00; C03C2214/02; C03C2214/20; Y; Y10; Y10S; Y10S428/00; Y10S428/902; Y10T; Y10T428/00; Y10T428/13; Y10T428/131; Y10T428/1314; Y10T428/1317; Y10T428/29; Y10T428/2913; Y10T428/2918; Y10T428/2973; Y10T428/2978
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
46 words
A compliant tubular liner particularly adapted to withstand brisant forces comprising a fiber reinforced glass or glass-ceramic matrix having an elastic modulus less than 15×10 6 psi and high fracture toughness exemplified by a critical stress intensity factor greater than 5×10 3 psi (inch) 1/2 .
Claim 2
Dependent Claim
46 words
A compliant tubular liner particularly adapted to withstand brisant forces comprising a fiber reinforced glass or glass-ceramic matrix having an elastic modulus less than 15×10 6 psi and high fracture toughness exemplified by a critical stress intensity factor greater than 5×10 3 psi (inch) 1/2 .
Claim 3
Dependent Claim
55 words
A composite gun barrel comprising a fiber reinforced glass or glass/ceramic matrix liner surrounded by a metal outer sleeve, the liner having an elastic modulus less than 15×10 6 psi, a fracture toughness exemplified by a critical stress intensity factor greater than 5×10 3 psi (inch) 1/2 , and being capable of withstanding brisant forces.
Claim 4
Dependent Claim
55 words
A composite gun barrel comprising a fiber reinforced glass or glass/ceramic matrix liner surrounded by a metal outer sleeve, the liner having an elastic modulus less than 15×10 6 psi, a fracture toughness exemplified by a critical stress intensity factor greater than 5×10 3 psi (inch) 1/2 , and being capable of withstanding brisant forces.
Claim 5
Dependent Claim
15 words
An article of claims 1 or 2 wherein the fibers are silicon carbide or graphite.
Claim 6
Dependent Claim
16 words
An article of claims 1 or 2 wherein the fibers range in length from 0.25-0.75 inch.
Claim 7
Dependent Claim
29 words
An article of claims 1 or 2 wherein the matrix is comprised of a glass-ceramic selected from the group consisting of lithium aluminosilicate, magnesium aluminosilicate, or a combination thereof.
References Cited (Backward Citations)
US2915946A
Cited
US3025765A
Cited
US2977666A
Cited
US3517585A
Cited
CA952133A
Cited
US3742640A
Cited
US4260657A
Cited
US4265968A
Cited
US4263367A
Cited
US4324843A
Cited
US4341840A
Cited
US4370390A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-03-06 | 1987-09-05 | 1988-03-06 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-03-06 | 1991-09-05 | 1992-03-06 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-03-06 | 1995-09-05 | 1996-03-06 | $7700.00 | Window Closed / Lapsed |