← Back to Patent Explorer
US4430807A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for drying water-wet membranes

Assignee: CYNARA COMPANY
•
Filing: 1982-05-17
•
Granted: 1984-02-14
•
Expires: 2002-05-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improved process for drying water-wet, cellulose ester membranes is described. It has been found that by contacting one side of the membrane with a liquid mixture of a water-miscible, volatile C 1 to C 6 hydrocarbon and a water-immiscible organic compound, while an inert gas stream or vacuum is maintained on the other surface of the membrane, water can be displaced from the membrane economically, rapidly and without adversely affecting the structure of the membrane. A 1 to 1 volume mixture of isopropanol and isooctane is particularly preferred in this step. The essentially water-free membrane is then dried by applying reduced pressure or an inert gas stream to produce a membrane having exceptional separation characteristics.

Inventors

  • 👤 Thomas E. Davis
  • 👤 Dana C. Overman, III

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 18:41
CPC Classifications
B; B01; B01D; B01D61/00; B01D61/36; B01D61/362; B01D67/00; B01D67/0081; B01D67/0095; F; F26; F26B; F26B5/00; F26B5/005; F26B7/00

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 289 words
A method for drying a water-wet, cellulose ester membrane, which comprises the steps of: (a) contacting a first side of the membrane with a liquid mixture compatible with the membrane, said liquid mixture comprising a first component which is a C 1 to C 6 hydrocarbon in which water is soluble to at least ten weight percent and a second component which is essentially immiscible in water, has a solubility parameter of no greater than about 9.5 (cal/cm 3 ) 0 .5 and exhibits poor hydrogen bonding, said contact with the liquid occurring while the other side of the membrane is swept with an inert gas or maintained at a reduced pressure relative to the first side of the membrane so as to maintain essentially continuously a lower chemical potential for the first component of the liquid mixture on the second side of the membrane, the composition of the liquid mixture being such that (1) the first component of said mixture pervaporates through the membrane more rapidly than the second component and (2) the liquid in contact with the membrane has a lower chemical potential for water than the membrane itself; (b) after a predominant amount of the water initially present in the water-wet membrane has been removed from the membrane, adjusting the composition of the liquid mixture in contact with the membrane so that the quantity of the second component which pervaporates through the membrane exceeds the quantity of the first component pervaporating through the membrane; (c) removing the liquid mixture from contact with the membrane after the membrane is essentially free of both water and the first component of the liquid mixture; and (d) treating the membrane to remove essentially all residual liquid remaining in the membrane.
Claim 2
Independent Claim 289 words
A method for drying a water-wet, cellulose ester membrane, which comprises the steps of: (a) contacting a first side of the membrane with a liquid mixture compatible with the membrane, said liquid mixture comprising a first component which is a C 1 to C 6 hydrocarbon in which water is soluble to at least ten weight percent and a second component which is essentially immiscible in water, has a solubility parameter of no greater than about 9.5 (cal/cm 3 ) 0 .5 and exhibits poor hydrogen bonding, said contact with the liquid occurring while the other side of the membrane is swept with an inert gas or maintained at a reduced pressure relative to the first side of the membrane so as to maintain essentially continuously a lower chemical potential for the first component of the liquid mixture on the second side of the membrane, the composition of the liquid mixture being such that (1) the first component of said mixture pervaporates through the membrane more rapidly than the second component and (2) the liquid in contact with the membrane has a lower chemical potential for water than the membrane itself; (b) after a predominant amount of the water initially present in the water-wet membrane has been removed from the membrane, adjusting the composition of the liquid mixture in contact with the membrane so that the quantity of the second component which pervaporates through the membrane exceeds the quantity of the first component pervaporating through the membrane; (c) removing the liquid mixture from contact with the membrane after the membrane is essentially free of both water and the first component of the liquid mixture; and (d) treating the membrane to remove essentially all residual liquid remaining in the membrane.
Claim 3
Dependent Claim 86 words
The method as described in claim 1 wherein the resulting dry cellulose ester membrane has a CO 2 permeation flux measured at a pressure differential of 50 psi between the feed gas and permeate of at least twice that attained with a membrane which is prepared from an identical water-wet membrane dried in the same manner except that a sweep gas or reduced pressure is not employed to maintain a lower chemical potential on the side of the membrane not in contact with the liquid mixture.
Claim 4
Dependent Claim 21 words
The method as described in claim 2 wherein the membrane is an asymmetric cellulose acetate, cellulose diacetate or cellulose triacetate membrane.
Claim 5
Dependent Claim 15 words
The method as described in claim 3 wherein the water-wet membrane is a spiral-wound membrane.
Claim 6
Dependent Claim 17 words
The method as described in claim 3 wherein the water-wet membrane is a bundle of hollow fibers.
Claim 7
Dependent Claim 31 words
The method as described in claim 3 wherein the first component of the liquid mixture is a C 1 to C 4 alkanol or C 2 to C 6 dialkyl ether.
Claim 8
Dependent Claim 20 words
The method as described in claim 6 wherein the second component of the liquid mixture is isooctane, n-hexane or n-heptane.
Claim 9
Dependent Claim 31 words
The method as described in claim 7 wherein the ratio of the first to the second component of the liquid mixture is in the range from 40:60 to 60:40 volume percent.

References Cited (Backward Citations)

US3415038A Cited
US3534528A Cited
US3842515A Cited
US4080743A Cited
US4080744A Cited
US4120098A Cited
US4068387A Cited
US4130403A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-02-13 1987-08-15 1988-02-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-02-13 1991-08-15 1992-02-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-02-13 1995-08-15 1996-02-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag