Abstract
Abstract New liquid developers for electrophotography comprise (a) a coloring agent, (b) a charge control agent and (c) one or more of a polyethylene, a polypropylene, an ethylene copolymer and a propylene copolymer, with or without (d) a hydrocarbon resin soluble in a hydrocarbon solvent and containing a 1,3-pentadiene moiety, in an electro-insulating liquid. These developers have an excellent etching resistance and a high dispersion stability.
Inventors
- 👤 Akio Iwaki
- 👤 Toyoki Nishijima
- 👤 Akio Iijima
- 👤 Tatsuya Sasazawa
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-29 09:38
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/12; G03G9/135; G03G9/122; G03G9/13; G03G9/131; G03G9/1355
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
59 words
A liquid developer for electrophotography which comprises (a) a coloring agent, (b) a charge control agent, (c) at least one polymer selected from the group consisting of a polyethylene, a polypropylene, an ethylene copolymer and a propylene copolymer in an electro-insulating liquid and (d) a hydrocarbon resin that is soluble in a hydrocarbon solvent and contains a 1,3-pentadiene moiety.
Claim 2
Dependent Claim
59 words
A liquid developer for electrophotography which comprises (a) a coloring agent, (b) a charge control agent, (c) at least one polymer selected from the group consisting of a polyethylene, a polypropylene, an ethylene copolymer and a propylene copolymer in an electro-insulating liquid and (d) a hydrocarbon resin that is soluble in a hydrocarbon solvent and contains a 1,3-pentadiene moiety.
Claim 3
Dependent Claim
135 words
A developer according to claim 1 wherein said coloring agent (a) is selected from the group consisting of carbon black, copper phthalocyanine, phthalocyanine green, Malachite Green, Rhodamine, Victoria Blue and Oil Black; said charge control agent (b) is selected from the group consisting of lecithin. a metal salt of naphthenic acid, an alkylbenzenesulfonate, a dialkylnaphthalenesulfonate, a mono- or dialkylsulfosuccinate, a dialkylphosphate, linseed oil, soybean oil and an alkyd resin; said polymer (c) is selected from the group consisting of a polyethylene, a polypropylene, a copolymer of ethylene with a copolymerizable monomer therewith and a copolymer of propylene with a copolymerizable monomer therewith; and said electro-insulating liquid is selected from the group consisting of an aliphatic hydrocarbon, an aromatic hydrocarbon and a halogenated hydrocarbon, said hydrocarbon having an electrical resistance of at least 10 9 Ωcm.
Claim 4
Dependent Claim
81 words
A developer according to claim 1 wherein said coloring agent (a) is in an amount of 0.01 to 1.00 part by weight based upon 100 parts by weight of said insulating liquid, said charge control agent (b) is in an amount sufficient to bring the electrical resistance of said developer to at least 10 9 Ωcm and said polymer (c) is in an amount of 0.01 to 5 parts by weight based upon 100 parts by weight of said insulating liquid.
Claim 5
Dependent Claim
57 words
A developer according to claim 1 wherein said coloring agent (a) is in an amount of 0.01 to 0.1 part by weight based upon 100 parts by weight of said insulating liquid and said polymer (c) is in an amount of 0.1 to 2 parts by weight based upon 100 parts by weight of said insulating liquid.
Claim 6
Dependent Claim
32 words
A developer according to claim 1 wherein said hydrocarbon resin (d) is in an amount of 0.01 to 5 parts by weight based upon 100 parts by weight of said insulating liquid.
Claim 7
Dependent Claim
32 words
A developer according to claim 5 wherein said hydrocarbon resin (d) is in an amount of 0.1 to 2 parts by weight based upon 100 parts by weight of said insulating liquid.
References Cited (Backward Citations)
US3993483A
Cited
US4060493A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-01-09 | 1987-07-11 | 1988-01-10 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-01-09 | 1991-07-11 | 1992-01-10 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-01-09 | 1995-07-11 | 1996-01-10 | $7700.00 | Window Closed / Lapsed |