Catalysts for the production of maleic anhydride by the oxidation of butane

Assignee: BP Corp North America Inc
•
Filing: 1982-05-26
•
Granted: 1983-11-22
•
Expires: 2002-05-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for the manufacture of a phosphorus/vanadium/metal oxide catalyst suitable for the oxidation of butane to maleic anhydride can be prepared by reacting in an aqueous medium a vanadium compound, inorganic acid and metal oxide, then adding orthophosphoric acid to form a soluble vanadium phosphorus metal oxide catalyst, removing the acidified water and adding an aliphatic alcohol, removing the alcohol and recovering under vacuum the solid phosphorus vanadium metal oxide catalyst.

Inventors

  • 👤 Carl A. Udovich
  • 👤 Robert C. Edwards

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 07:48
CPC Classifications
C; C07; C07C; C07C51/00; C07C51/16; C07C51/21; C07C51/215; B; B01; B01J; B01J23/00; B01J23/002; B01J27/00; B01J27/14; B01J27/186; B01J27/195; B01J27/198; B01J2523/00

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 94 words
A process for the manufacture of a phosphorus/vanadium/metal oxide catalyst suitable for use in the manufacture of maleic anhydride which process comprises reacting in an aqueous medium, a vanadium compound and inorganic acid and metal oxide, then adding orthophosphoric acid to form a soluble vanadium phosphorus metal oxide catalyst removing the acidified water and adding an aliphatic alcohol having 1 to 8 carbon atoms, removing the alcohol and drying the catalyst syrup under vacuum of about 0 to 300 mm Hg at a temperature of 90° to 120° C. to produce the solid catalyst.
Claim 2
Dependent Claim 94 words
A process for the manufacture of a phosphorus/vanadium/metal oxide catalyst suitable for use in the manufacture of maleic anhydride which process comprises reacting in an aqueous medium, a vanadium compound and inorganic acid and metal oxide, then adding orthophosphoric acid to form a soluble vanadium phosphorus metal oxide catalyst removing the acidified water and adding an aliphatic alcohol having 1 to 8 carbon atoms, removing the alcohol and drying the catalyst syrup under vacuum of about 0 to 300 mm Hg at a temperature of 90° to 120° C. to produce the solid catalyst.
Claim 3
Dependent Claim 12 words
The process of claim 1 wherein the vanadium compound is vanadium pentoxide.
Claim 4
Dependent Claim 27 words
The process of claim 2 wherein the alcohol is methanol and the inorganic acid is HCl and the orthophosphoric acid is 85 to 95 percent orthophosphoric acid.
Claim 5
Dependent Claim 12 words
The process of claim 3 wherein the vanadium compound is vanadium pentoxide.
Claim 6
Dependent Claim 98 words
A process for the manufacture of a phosphorus/vanadium/molybdenum oxide catalyst suitable for use in the manufacture of maleic anhydride which process comprises reacting in an aqueous medium vanadium compound and inorganic acid and molybdenum oxide, then adding orthophosphoric acid to form a soluble vanadium phosphorus molybdenum oxide catalyst, removing the acidified water and adding an aliphatic alcohol having 1 to 8 carbon atoms, removing the alcohol and drying the catalyst syrup under vacuum of about 0 to 300 mm Hg at a temperature of about 90° to 120° C. to produce the solid vanadium phosphorus molybdenum oxide catalyst.
Claim 7
Dependent Claim 98 words
A process for the manufacture of a phosphorus/vanadium/molybdenum oxide catalyst suitable for use in the manufacture of maleic anhydride which process comprises reacting in an aqueous medium vanadium compound and inorganic acid and molybdenum oxide, then adding orthophosphoric acid to form a soluble vanadium phosphorus molybdenum oxide catalyst, removing the acidified water and adding an aliphatic alcohol having 1 to 8 carbon atoms, removing the alcohol and drying the catalyst syrup under vacuum of about 0 to 300 mm Hg at a temperature of about 90° to 120° C. to produce the solid vanadium phosphorus molybdenum oxide catalyst.
Claim 8
Dependent Claim 10 words
The process of claim 4 wherein the alcohol is methanol.
Claim 9
Dependent Claim 11 words
The process of claim 6 wherein the inorganic acid is HCl.
Claim 10
Dependent Claim 16 words
The process of claim 7 wherein the orthophosphoric acid is 85 to 95 percent orthophosphoric acid.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-11-21 1987-05-23 1987-11-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-11-21 1991-05-23 1991-11-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-11-21 1995-05-23 1995-11-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag