Stabilized thermosettable ethylenically unsaturated epoxy ester resin compositions

Assignee: DIAMOND TECHNOLOGY PARTNERSHIP Co
•
Filing: 1982-05-12
•
Granted: 1983-11-01
•
Expires: 2002-05-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract This invention is directed to thermosettable ethylenically unsaturated epoxy ester resin compositions having improved storage stability and to a method for improving the storage stability of such compositions by adding an anaerobically effective polymerization inhibitor to the resin composition. The resin composition comprises the reaction product of a bisphenol-base epoxy resin, a novolac-base epoxy resin, or a mixture thereof with an ethylenically unsaturated monocarboxylic acid dissolved in a polymerizable monomer containing a >C=CH2 group. The polymerization inhibitors of this invention are 4-chloro-2-nitrophenol, 2,4-dichloro-6-nitrophenol, or mixtures thereof.

Inventors

  • 👤 Raymond Koenig

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 21:27
CPC Classifications
C; C08; C08L; C08L63/00; C08L63/10; C08F; C08F299/00; C08F299/02; C08F299/026

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 60 words
A thermosettable ethylenically unsaturated epoxy ester resin composition having improved storage stability comprising the reaction product of a bisphenol-base epoxy resin, a novolac-base epoxy resin, or mixtures thereof with an ethylenically unsaturated monocarboxylic acid dissolved in a polymerizable monomer containing a >C═CH 2 group and an anaerobically effective polymerization selected from the group consisting of 4-chloro-2-nitrophenol, 2,4-dichloro-6-nitrophenol, and mixtures thereof.
Claim 2
Dependent Claim 60 words
A thermosettable ethylenically unsaturated epoxy ester resin composition having improved storage stability comprising the reaction product of a bisphenol-base epoxy resin, a novolac-base epoxy resin, or mixtures thereof with an ethylenically unsaturated monocarboxylic acid dissolved in a polymerizable monomer containing a >C═CH 2 group and an anaerobically effective polymerization selected from the group consisting of 4-chloro-2-nitrophenol, 2,4-dichloro-6-nitrophenol, and mixtures thereof.
Claim 3
Dependent Claim 31 words
The thermosettable resin composition of claim 1 wherein the polymerization inhibitor is present in the range of 10 to 5,000 parts by weight per million parts by weight of resin composition.
Claim 4
Dependent Claim 15 words
The thermosettable resin composition of claim 1 or 2 wherein the polymerization inhibitor is 4-chloro-2-nitrophenol.
Claim 5
Independent Claim 74 words
A method for improving the storage stability of thermosettable ethylenically unsaturated epoxy ester resin compositions by adding an anaerobically effective polymerization inhibitor selected from the group consisting of 4-chloro-2-nitrophenol, 2,4-dichloro-6-nitrophenol, and mixtures thereof to the thermosettable resin composition, the thermosettable resin composition comprising the reaction product of a bisphenol-base epoxy resin, a novolac-base epoxy resin, or mixtures thereof with an ethylenically unsaturated monocarboxylic acid dissolved in a polymerizable monomer containing a >C═CH 2 group.
Claim 6
Independent Claim 74 words
A method for improving the storage stability of thermosettable ethylenically unsaturated epoxy ester resin compositions by adding an anaerobically effective polymerization inhibitor selected from the group consisting of 4-chloro-2-nitrophenol, 2,4-dichloro-6-nitrophenol, and mixtures thereof to the thermosettable resin composition, the thermosettable resin composition comprising the reaction product of a bisphenol-base epoxy resin, a novolac-base epoxy resin, or mixtures thereof with an ethylenically unsaturated monocarboxylic acid dissolved in a polymerizable monomer containing a >C═CH 2 group.
Claim 7
Dependent Claim 30 words
The method of claim 4 wherein the polymerization inhibitor is employed in the range of from 10 to 5,000 parts by weight per million parts by weight of resin composition.
Claim 8
Dependent Claim 13 words
The method of claim 4 or 5 wherein the polymerization inhibitor is 4-chloro-2-nitrophenol.

References Cited (Backward Citations)

US3301743A Cited
US3524901A Cited
US4253918A Cited
US4309473A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-10-31 1987-05-02 1987-11-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-10-31 1991-05-02 1991-11-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-10-31 1995-05-02 1995-11-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag