Patent US4411754A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4411754A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for preparing a polymer composition

Assignee: Japan Atomic Energy Agency
•
Filing: 1981-02-13
•
Granted: 1983-10-25
•
Expires: 2001-02-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A polymer composition containing a physiologically active substance which can be released at a controlled rate is prepared by contacting one or more polymerizable monomers with the physiologically active substance, making the monomers into a specific shape and then irradiating the shaped article with light or an ionizing radiation at a low temperature below room temperature to polymerize the polymerizable monomers.

Inventors

  • 👤 Isao Kaetsu
  • 👤 Masaru Yoshida
  • 👤 Minoru Kumakura

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 17:47
CPC Classifications
C; C08; C08F; C08F2/00; C08F2/44; A; A61; A61K; A61K9/00; A61K9/14; A61K9/16; A61K9/1605; A61K9/1629; A61K9/1635; A61K9/20; A61K9/2004; A61K9/2022; A61K9/2027; A61K9/70; A61K9/7007

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 120 words
A process for preparing a polymer composition containing a physiologically active substance, said composition capable of releasing said physiologically active substance at a controlled rate, characterized by mixing one or more polymerizable monomers and said physiologically active substance in the absence or presence of a crystallizable substance, intended to increase the surface area for elution of said substance, and wherein an adsorbent is added from the group consisting of active carbon, silica-gel, kaolin and ion exchange resins, to adsorb a solution of physiologically active substance when an elution medium permeates into the composition, and irradiating the resulting mixture with light or an ionizing radiation at a temperature below 0° C. to polymerize said polymerizable monomers, to yield said polymer composition.
Claim 2
Dependent Claim 120 words
A process for preparing a polymer composition containing a physiologically active substance, said composition capable of releasing said physiologically active substance at a controlled rate, characterized by mixing one or more polymerizable monomers and said physiologically active substance in the absence or presence of a crystallizable substance, intended to increase the surface area for elution of said substance, and wherein an adsorbent is added from the group consisting of active carbon, silica-gel, kaolin and ion exchange resins, to adsorb a solution of physiologically active substance when an elution medium permeates into the composition, and irradiating the resulting mixture with light or an ionizing radiation at a temperature below 0° C. to polymerize said polymerizable monomers, to yield said polymer composition.
Claim 3
Dependent Claim 114 words
A process for preparing a polymer composition having a function of releasing a physiologically active substance at a controlled rate which comprises dropping or injecting a mixture of one or more monomers vitrifiable at low temperatures containing 5 to 50%, by weight, of synthetic high molecular weight substance and said physiologically active substance into a medium at low temperatures to make it into a shape of spherical structure, and thereafter irradiating it with light or an ionizing radiation at a low temperature below room temperature to polymerize said monomers, to yield a composition capable of releasing said physiologically active substance at a controlled rate, and releasing said physiologically active substance at said controlled rate.
Claim 4
Dependent Claim 114 words
A process for preparing a polymer composition having a function of releasing a physiologically active substance at a controlled rate which comprises dropping or injecting a mixture of one or more monomers vitrifiable at low temperatures containing 5 to 50%, by weight, of synthetic high molecular weight substance and said physiologically active substance into a medium at low temperatures to make it into a shape of spherical structure, and thereafter irradiating it with light or an ionizing radiation at a low temperature below room temperature to polymerize said monomers, to yield a composition capable of releasing said physiologically active substance at a controlled rate, and releasing said physiologically active substance at said controlled rate.

References Cited (Backward Citations)

US3577512A Cited
US3767790A Cited
US3900559A Cited
US3901968A Cited
US3901967A Cited
US3901966A Cited
US4025391A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-10-24 1987-04-25 1987-10-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-10-24 1991-04-25 1991-10-25 $3760.00 Window Closed / Lapsed