Abstract

Abstract A method of coating uncoated portions of a coated optical fiber is disclosed. In this method a grooved split mold apparatus is used. This fiber, including coated portions of the fiber are placed within the groove and appropriately tensioned so as to prevent contact between the uncoated portions of the fiber and the mold. Injection molding techniques are then used to recoat the uncoated portions of the fiber.

Inventors

  • 👤 Arthur C. Hart, Jr.

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 11:56
CPC Classifications
G; G02; G02B; G02B6/00; G02B6/24; G02B6/255; G02B6/2558; B; B29; B29C; B29C45/00; B29C45/14; B29C45/14549; C; C03; C03C; C03C25/00; C03C25/10; C03C25/12; C03C25/18; B29C35/00; B29C35/02; B29C35/08; B29C35/0805; B29C2035/0827; B29C45/0053; B29C2045/0075; B29C2045/14557

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 168 words
A method of fabricating a continuously coated optical fiber comprising, aligning an uncoated portion of a coated optical fiber with a groove in an open, grooved, split mold, the groove extending beyond the uncoated portions of the fiber to the coated portion of the fiber which adjoins the end of the uncoated portion of the fiber, the groove having a diameter, D, greater than the diameter, d, of the coated portion of the optical fiber, tensioning the optical fiber, reducing the distance between the open mold and the fiber so that the coated portion of the fiber contacts the groove surface while the uncoated portions of the fiber do not contact the groove surface, aligning the groove in the second half of the split mold with the optical fiber, closing the split mold, injecting a curable coating material into the groove until the coating material flows at least to the coated portion of the fiber and, curing the coated material, whereby a continuously coated optical fiber is obtained.
Claim 2
Independent Claim 168 words
A method of fabricating a continuously coated optical fiber comprising, aligning an uncoated portion of a coated optical fiber with a groove in an open, grooved, split mold, the groove extending beyond the uncoated portions of the fiber to the coated portion of the fiber which adjoins the end of the uncoated portion of the fiber, the groove having a diameter, D, greater than the diameter, d, of the coated portion of the optical fiber, tensioning the optical fiber, reducing the distance between the open mold and the fiber so that the coated portion of the fiber contacts the groove surface while the uncoated portions of the fiber do not contact the groove surface, aligning the groove in the second half of the split mold with the optical fiber, closing the split mold, injecting a curable coating material into the groove until the coating material flows at least to the coated portion of the fiber and, curing the coated material, whereby a continuously coated optical fiber is obtained.
Claim 3
Dependent Claim 12 words
The method of claim 1 wherein the groove is semicircular or V-groove.
Claim 4
Dependent Claim 19 words
The method of claim 1 wherein the groove is semicircular and has a diameter, D, less than d+0.006 inches.
Claim 5
Dependent Claim 25 words
The method of claim 2 or 3 wherein the optical fiber is tensioned to a tension less than 10 pounds but greater than 0.1 pound.
Claim 6
Dependent Claim 18 words
The method of claim 4 wherein the curable coating material is essentially identical to the original coating material.
Claim 7
Dependent Claim 15 words
The method of claim 5 wherein the curable coating material is a UV curable material.
Claim 8
Dependent Claim 38 words
The method of claim 6 wherein the curable coating material is a UV curable coating material and wherein at least a portion of the mold is essentially transparent to UV radiation necessary to cure the UV curable material.

References Cited (Backward Citations)

US28028A Cited
US4091062A Cited
US3914145A Cited
US4217027A Cited
US4217027B1 Cited
US4049480A Cited
US4135587A Cited
US4152539A Cited
US4270021A Cited
US4201618A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-10-17 1987-04-18 1987-10-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-10-17 1991-04-18 1991-10-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-10-17 1995-04-18 1995-10-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag