Patent US4410468A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4410468A Expired / Lapsed US ⏱️ 0.0 years remaining

Hot press-forging of an optical body with dynamic constraint by crystal powder

Assignee: Solon Technologies Inc
•
Filing: 1981-07-06
•
Granted: 1983-10-18
•
Expires: 2001-07-06
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method is disclosed for hot press-forging a normally frangible optically integral crystalline mass ("optical body") in a closed die, by directly pressing a surface of the mass while it is peripherally surrounded by a crystal powder the amount of which is computed from the deformation ratio desired and the geometry of the die. The crystal powder is compacted by the nonuniformly directed forces transmitted to it by the optical body, and eventually the crystal powder is sufficiently dense so as dynamically to constrain the optical body at its peripheral surface. The dynamic constraint of the optical body while it is being forged is effected in such a way as to permit deformation of the optical body without fracturing it, and, without affecting its optical integrity. Hot press-forging the optical body by peripherally surrounding it with the crystal powder produces a stress environment in which the forces applied in a first stage, to the optical body by the ram of the forging press and, in a second stage, by the crystal powder, are non-uniform both in magnitude as well as in direction. The result is that the optical body may be deformed and forged to obtain a deformation ratio greater than 1.0 so as to obtain a fine-grain structure free of peripheral fissures and "veiling". Typically, a melt-grown essentially single macrocrystal of an ionic salt or of an optical oxide of magnesium including certain optical mixed oxides such as bismuth germanium oxide, cadmium tungstate and lithium niobate, is hot press-forged while it is surrounded by a crystal powder of the same ionic salt or oxide. A polycrystalline extrudate of a melt-grown macrocrystal may also be hot press-forged in an analogous manner.

Inventors

  • 👤 Herbert Packer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 20:28
CPC Classifications
G; G02; G02B; G02B1/00; G02B1/02; C; C30; C30B; C30B29/00; C30B29/10; C30B29/12; C30B29/60; C30B29/62; C30B33/00

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 249 words
A two-stage process for hot press-forging an optical body, comprising, (a) maintaining said optical body at an elevated temperature below its melting point in a die cavity so as to provide an annular space therein, (b) peripherally surrounding said optical body with a crystal powder placed in said annular space, said crystal powder consisting essentially of an inorganic material having essentially the same coefficient of thermal expansion as that of said optical body, the volume of said crystal powder being equal to or less than that of said annular space, (c) gradually press-forging said optical body at said temperature between opposed spaced-apart surfaces in solid-to-solid contact with opposed surfaces of said optical body, essentially free from contact with said crystal powder therebetween, (d) exerting, in a first stage of said press-forging sufficient pressure on said opposed surfaces to move one surface closer to the other so as to impart a radially outward essentially unconstrained movement of the peripheral surfaces of said optical body, (e) transmitting, in a second stage of said press-forging, sufficient force from walls of said die cavity to compact said crystal powder and dynamically constrain radially outward movement of said peripheral surfaces, and (f) providing a deformation ratio greater than 1 without changing the density of said optical body, so as to effect a change of its shape due to said press-forging and to obtain a forged optical body essentially free from surface defects and fissures near its periphery, yet maintaining its physical and optical integrity.
Claim 2
Dependent Claim 249 words
A two-stage process for hot press-forging an optical body, comprising, (a) maintaining said optical body at an elevated temperature below its melting point in a die cavity so as to provide an annular space therein, (b) peripherally surrounding said optical body with a crystal powder placed in said annular space, said crystal powder consisting essentially of an inorganic material having essentially the same coefficient of thermal expansion as that of said optical body, the volume of said crystal powder being equal to or less than that of said annular space, (c) gradually press-forging said optical body at said temperature between opposed spaced-apart surfaces in solid-to-solid contact with opposed surfaces of said optical body, essentially free from contact with said crystal powder therebetween, (d) exerting, in a first stage of said press-forging sufficient pressure on said opposed surfaces to move one surface closer to the other so as to impart a radially outward essentially unconstrained movement of the peripheral surfaces of said optical body, (e) transmitting, in a second stage of said press-forging, sufficient force from walls of said die cavity to compact said crystal powder and dynamically constrain radially outward movement of said peripheral surfaces, and (f) providing a deformation ratio greater than 1 without changing the density of said optical body, so as to effect a change of its shape due to said press-forging and to obtain a forged optical body essentially free from surface defects and fissures near its periphery, yet maintaining its physical and optical integrity.
Claim 3
Dependent Claim 25 words
The hot press-forging process of claim 1 wherein said optical body is selected from the group consisting of an ionic salt and an optical oxide.
Claim 4
Dependent Claim 21 words
The hot press-forging process of claim 1 wherein said crystal powder is derived from the same material as said optical body.
Claim 5
Dependent Claim 21 words
The hot press-forging process of claim 1 wherein said deformation ratio is in the range from about 1.2 to about 10.
Claim 6
Dependent Claim 26 words
The process of claim 2 wherein said ionic salt is selected from the group consisting of the alkali metal halides and the alkaline earth metal halides.
Claim 7
Dependent Claim 26 words
The process of claim 2 wherein said optical oxide is selected from the group consisting of magnesium oxide, bismuth germanium oxide, cadmium tungstate, and lithium niobate.
Claim 8
Dependent Claim 22 words
The process of claim 3 wherein said crystal powder is in the size range from about 20 microns to about 250 microns.

References Cited (Backward Citations)

US4071372A Cited
US3892835A Cited
US3933970A Cited
US4217318A Cited
US4171400A Cited
US4081505A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-10-17 1987-04-18 1987-10-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-10-17 1991-04-18 1991-10-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-10-17 1995-04-18 1995-10-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag