Abstract

Abstract Water repellent treating compositions are based upon olefin and paraffin materials containing a substantial proportion of compounds containing from 20 to 24 carbon atoms. The treating compositions are especially useful for application to wood. Additives such as wood preservatives, alkyd resins and, in especially preferred compositions, organic ionizable compounds are included. The preferred compositions are useful for application to wood substrates which are subsequently electrostatically sprayed with a topcoating.

Inventors

  • 👤 John F. Grunewalder

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 18:43
CPC Classifications
C; C09; C09K; C09K3/00; C09K3/18; B; B05; B05D; B05D1/00; B05D1/02; B05D1/04; B05D1/045; B05D7/00; B05D7/06; B05D7/08; B27; B27K; B27K3/00; B27K3/02; B27K3/0278; B27K3/15; B27K3/34; B27K3/36; B27K3/50; B27K5/00; B27K5/001; C08; C08L; C08L97/00; C08L97/02; C09D; C09D191/00; C09D191/06; B27K2240/00; B27K2240/70; C08L67/00; C08L67/08

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 152 words
A method of treating wood so as to provide the wood with water-repellency, comprising the steps of: (a) applying to wood a water-repellent composition, said composition consisting essentially of; (i) from about 1% to about 50% of an alpha olefin having from 20 to 24 carbon atoms, a narrow cut alpha olefin blend, a narrow cut paraffin blend, or a mixture thereof, wherein said olefin blend and paraffin blend consists essentially of a mixture of compounds of which at least about 50% have from 20 carbon atoms to 24 carbon atoms; (ii) from about 0% to about 6% of a wood preservative; (iii) from about 0% to about 20% of an alkyd resin; (iv) from about 0% to about 5% of an organic ionizable compound; and (v) from about 45% to about 98% of an organic solvent, and (b) drying the wood of step (a) so as to produce the treated wood.
Claim 2
Independent Claim 152 words
A method of treating wood so as to provide the wood with water-repellency, comprising the steps of: (a) applying to wood a water-repellent composition, said composition consisting essentially of; (i) from about 1% to about 50% of an alpha olefin having from 20 to 24 carbon atoms, a narrow cut alpha olefin blend, a narrow cut paraffin blend, or a mixture thereof, wherein said olefin blend and paraffin blend consists essentially of a mixture of compounds of which at least about 50% have from 20 carbon atoms to 24 carbon atoms; (ii) from about 0% to about 6% of a wood preservative; (iii) from about 0% to about 20% of an alkyd resin; (iv) from about 0% to about 5% of an organic ionizable compound; and (v) from about 45% to about 98% of an organic solvent, and (b) drying the wood of step (a) so as to produce the treated wood.
Claim 3
Dependent Claim 31 words
The method of claim 1 wherein the wood is treated with the alpha olefin blend consisting essentially of at least about 70% of compounds having from 20 to 24 carbon atoms.
Claim 4
Dependent Claim 31 words
The method of claim 1 wherein the wood is treated with the alpha olefin blend consisting essentially of at least about 90% of compounds having from 20 to 24 carbon atoms.
Claim 5
Independent Claim 23 words
The method of claims 2 or 3 wherein from about 0.5% to about 6% of the wood preservative is used in the composition.
Claim 6
Independent Claim 23 words
The method of claims 2 or 3 wherein from about 1% to about 20% of the alkyd resin is used in the composition.
Claim 7
Independent Claim 24 words
The method of claims 2 or 3 wherein from about 1% to about 5% of the organic ionizable compound is used in the composition.
Claim 8
Dependent Claim 21 words
The method of claim 6 further comprising the step of electrostatically depositing a coating onto the treated wood of step (a).
Claim 9
Dependent Claim 27 words
The method of claim 7 wherein the treated wood, after being electrostatically coated, is dried at a temperature ranging from about 5° C. to about 65° C.
Claim 10
Dependent Claim 54 words
The method of claim 6 wherein the alpha olefin blend consists essentially of at least about 96% of compounds having between 20 and 24 carbon atoms in the chain, less than about 3% of compounds having less than 20 carbon atoms and less than about 1% of compounds having more than 24 carbon atoms.
Claim 11
Dependent Claim 30 words
The method of claim 9 wherein the organic ionizable compound is an organic acid, base or salt and is used at a level ranging from about 1% to about 2%.
Claim 12
Dependent Claim 15 words
The method of claim 10 wherein the organic ionizable compound is a quaternary ammonium sulfate.
Claim 13
Dependent Claim 29 words
The method of claim 1 wherein the treating composition contains the alpha olefin, alpha olefin blend or paraffin blend at a level of from about 1% to about 15%.
Claim 14
Dependent Claim 36 words
The method of claim 12 wherein the treating composition is further characterized in being capable of providing the wood substrate with wood repellency at a level of at least about 40% efficiency as determined under NWMA-M-2-70.
Claim 15
Dependent Claim 23 words
The method of claim 13 wherein the treating composition is capable of providing water-repellency at a level of at least about 50% efficiency.
Claim 16
Dependent Claim 23 words
The method of claim 14 wherein the treating composition is capable of providing water-repellency at a level of at least about 60% efficiency.
Claim 17
Dependent Claim 26 words
The method of claim 1 wherein the wood is treated with the paraffin blend and said paraffin blend is further characterized as being comprised of n-paraffins.

References Cited (Backward Citations)

US3061508A Cited
US3236679A Cited
US3881940A Cited
US4183757A Cited
US4265663A Cited
US4360385A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-09-12 1987-03-14 1987-09-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-09-12 1991-03-14 1991-09-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-09-12 1995-03-14 1995-09-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag