Method of making organophilic clays

Assignee: Covia Holdings LLC
•
Filing: 1980-11-12
•
Granted: 1983-09-06
•
Expires: 2000-11-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A substantially dry method for making organophilic clays. Smectite clays, having a moisture content of less than 12% by weight are sprayed with an activator substance comprising about 1-10% by weight of the clay of a hydrophobic radical including those obtained from an "onium" base selected from a class consisting of ammonium, oxonium, sulfonium, arsonium, stibonium and telluronium. Organic amines and ammonium salts are preferred sources for the hydrophobic radical, and a substituted, hydrogenated tallow ammonium chloride is particularly preferred. The pretreated clay is then subjected to mechanical working such as by compaction to activate the clay. The subject method avoids the addition of water or other solvent to the clay when adding the activator substance, and therefore avoids the added cost of later removing the water, or other solvent. The physical properties of the dry processed organophilic clay are superior in some respects to organophilic clays made by the prior art methods. The organophilic clay made by the subject method can be used for gelling oils and oil-muds to suspend solids in a fluid when the fluid is static. It can also be used to impart cuttings-carrying ability to oil well drilling muds.

Inventors

  • 👤 George R. Alther

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 21:50
CPC Classifications
C; C01; C01B; C01B33/00; C01B33/20; C01B33/36; C01B33/38; C01B33/44; C09; C09K; C09K8/00; C09K8/02; C09K8/04; C09K8/14; C09K8/145; Y; Y10; Y10S; Y10S507/00; Y10S507/901

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 111 words
A substantially dry process for making an organophilic clay from a smectite clay comprising first adding to said smectite clay 1-10% by weight of an activator substance having a hydrophobic radical and being selected from the group consisting of aliphatic and alicyclic amine acid-addition and quaternary ammonium salts, said smectite clay having a maximum moisture content of about 12% by weight, thoroughly mixing said activator substance with said clay, and then compacting said clay activator substance mixture into a compacted mass having an apparent density of from about 60-94% of the apparent density of the clay before it is ground, whereby the organophilic properties of said treated clay are substantially improved.
Claim 2
Dependent Claim 111 words
A substantially dry process for making an organophilic clay from a smectite clay comprising first adding to said smectite clay 1-10% by weight of an activator substance having a hydrophobic radical and being selected from the group consisting of aliphatic and alicyclic amine acid-addition and quaternary ammonium salts, said smectite clay having a maximum moisture content of about 12% by weight, thoroughly mixing said activator substance with said clay, and then compacting said clay activator substance mixture into a compacted mass having an apparent density of from about 60-94% of the apparent density of the clay before it is ground, whereby the organophilic properties of said treated clay are substantially improved.

References Cited (Backward Citations)

US2531427A Cited
US2531440A Cited
US2859234A Cited
US4105578A Cited
US4193806A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-09-05 1987-03-07 1987-09-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-09-05 1991-03-07 1991-09-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-09-05 1995-03-07 1995-09-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag