US4396077A Expired / Lapsed US ⏱️ 0.0 years remaining

Drill bit with carbide coated cutting face

Assignee: Diamant Boart Stratabit USA Inc
•
Filing: 1981-09-21
•
Granted: 1983-08-02
•
Expires: 2001-09-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A drill bit for connection on a drill string has a hollow tubular body with an end cutting face provided with a tungsten carbide coated surface and an exterior peripheral stabilizer surface with cylindrical sintered carbide inserts positioned therein. Nozzle passages extend from the interior of the bit body through the cutting face for receiving a removable and interchangeable nozzle member therein. The cutting face has a plurality of recesses therein which receive, by an interference fit, a plurality of cutting elements of the type known as STRATAPAX, consisting of a cylindrical stud having an angular supporting surface with a cutting disc bonded thereon consisting of sintered carbide having a cutting surface of polycrystalline diamond. The recesses in the cutting face have milled offset recesses adjacent to the edges thereof which are sized and positioned to permit the cutting discs to be partially recessed and to restrain the cutting elements from rotation during use. The cutting face is coated with tungsten carbide to a thickness of 0.012-0.040 in. by means of a high-velocity, high-temperature plasma coating process after the cutting elements are assembled in the bit body. This process coats the steel bit body with tungsten carbide without coating or otherwise affecting the cutting inserts. The coating is metallurgically bonded to the steel bit body and protects against wear during drilling for periods of several hundred hours.

Inventors

  • 👤 Robert P. Radtke

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 06:55
CPC Classifications
E; E21; E21B; E21B10/00; E21B10/46; E21B10/56; E21B10/567; C; C23; C23C; C23C4/00; C23C4/04; C23C4/10; E21B10/60

Claims Analysis

Total Claims: 21
Claim 1
Independent Claim 141 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface.
Claim 2
Independent Claim 141 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface.
Claim 3
Dependent Claim 67 words
A method according to claim 1 in which said tungsten carbide coating is applied by dispersing fine tungsten carbide particles into a plasma arc at a temperature sufficient to melt said particles, and projecting said molten particles onto said cutting face at a high linear velocity such that said molten particles solidify as a coating thereon which is dense, coherent, non-porous and metallurgically bonded to said surface.
Claim 4
Dependent Claim 42 words
A method according to claim 2 in which said plasma arc heats said tungsten carbide particles to a temperature of about 6,000° F. and the gas flow therethrough carries said molten tungsten carbide at a linear velocity in excess of 4,000 ft./sec.
Claim 5
Dependent Claim 23 words
A method according to claim 1 in which said tungsten carbide coating is built up in layers to a thickness of 40-50 mils.
Claim 6
Dependent Claim 55 words
A method according to claim 3 in which said plasma arc is produced by passing an arc through an inert gas stream to produce an ionized gas at a temperature of about 30,000° F., and ejecting the heated gas stream with the tungsten particles entrained therein at a linear velocity in excess of 4,000 ft./sec.
Claim 7
Independent Claim 213 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface said cutting elements each comprising a cylindrical supporting stud of sintered carbide having an angularly oriented supporting surface with a disc shaped element bonded thereon comprising a sintered carbide disc having a cutting surface comprising polycrystalline diamond, each of said cutting elements being positioned in one of said recesses by an interference fit, and said tungsten carbide coating being only on said cutting face, said cutting elements being free of said coating.
Claim 8
Independent Claim 213 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface said cutting elements each comprising a cylindrical supporting stud of sintered carbide having an angularly oriented supporting surface with a disc shaped element bonded thereon comprising a sintered carbide disc having a cutting surface comprising polycrystalline diamond, each of said cutting elements being positioned in one of said recesses by an interference fit, and said tungsten carbide coating being only on said cutting face, said cutting elements being free of said coating.
Claim 9
Independent Claim 312 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface each of said recesses having a milled offset recess at its surface opening edge, of circular curvature in section and intersecting the circumferential edge of said recess for substantially less than 180° of the circumference thereof, said cutting elements each comprising a cylindrical supporting stud of sintered carbide having an angularly oriented supporting surface with a disc shaped element bonded thereon comprising a sintered carbide disc having a cutting surface comprising polycrystalline diamond, each of said cutting elements being positioned in one of said recesses by an interference fit with said disc shaped element partially recessed in and abutting said milled offset recess at the surface opening thereof, said milled offset recesses each being positioned to orient said discs with their cutting surfaces facing the direction of rotation of the bit and being of a size relieving stresses on said supporting studs during cutting operation and resisting twisting movement of said studs, and said tungsten carbide coating being only on said cutting face, said cutting elements being free of said coating.
Claim 10
Independent Claim 312 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface each of said recesses having a milled offset recess at its surface opening edge, of circular curvature in section and intersecting the circumferential edge of said recess for substantially less than 180° of the circumference thereof, said cutting elements each comprising a cylindrical supporting stud of sintered carbide having an angularly oriented supporting surface with a disc shaped element bonded thereon comprising a sintered carbide disc having a cutting surface comprising polycrystalline diamond, each of said cutting elements being positioned in one of said recesses by an interference fit with said disc shaped element partially recessed in and abutting said milled offset recess at the surface opening thereof, said milled offset recesses each being positioned to orient said discs with their cutting surfaces facing the direction of rotation of the bit and being of a size relieving stresses on said supporting studs during cutting operation and resisting twisting movement of said studs, and said tungsten carbide coating being only on said cutting face, said cutting elements being free of said coating.
Claim 11
Independent Claim 184 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface, said bit body including a plurality of passages extending through said cutting face, a plurality of removable and replaceable nozzles positioned one in each of said passages, and said tungsten carbide coating covering said cutting face extending into and coating said nozzle-containing passages.
Claim 12
Independent Claim 184 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface, said bit body including a plurality of passages extending through said cutting face, a plurality of removable and replaceable nozzles positioned one in each of said passages, and said tungsten carbide coating covering said cutting face extending into and coating said nozzle-containing passages.
Claim 13
Independent Claim 174 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface, said peripheral stabilizer surface having a plurality of recesses therein, and flat ended tungsten carbide inserts positioned one in each of said last named recesses to provide wear protection for said stabilizer surface.
Claim 14
Independent Claim 174 words
A method of producing a drill bit which comprises providing a drill body of a steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface, said peripheral stabilizer surface having a plurality of recesses therein, and flat ended tungsten carbide inserts positioned one in each of said last named recesses to provide wear protection for said stabilizer surface.
Claim 15
Independent Claim 140 words
A method of producing a drill bit comprising providing a drill body of 4130 steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface.
Claim 16
Independent Claim 140 words
A method of producing a drill bit comprising providing a drill body of 4130 steel alloy having a hollow tubular body adapted to be connected to a drill string, said drill body having an exterior peripheral stabilizer surface and an end cutting face, said end cutting face having a plurality of recesses spaced therearound in a selected pattern, positioning a plurality of cutting elements one in each of said recesses and extending outward from said end cutting face, applying a coating of tungsten carbide on said cutting face, after assembly of said cutting elements therein, in a plasma arc spray without raising the temperature of the bit body above about 200° F. or raising the temperature of said cutting elements above about 1300° F., to a thickness in excess of 12 mils, dense, non-porous, and metallurgically bonded to said surface.
Claim 17
Dependent Claim 10 words
A drill bit produced by the method of claim 1.
Claim 18
Dependent Claim 10 words
A drill bit produced by the method of claim 2.
Claim 19
Dependent Claim 10 words
A drill bit produced by the method of claim 3.
Claim 20
Dependent Claim 10 words
A drill bit produced by the method of claim 4.
Claim 21
Dependent Claim 10 words
A drill bit produced by the method of claim 5.

References Cited (Backward Citations)

US3298451A Cited
US3286334A Cited
US4246977A Cited
US4285410A Cited
US4265324A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-08-01 1987-01-31 1987-08-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-08-01 1991-01-31 1991-08-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-08-01 1995-01-31 1995-08-02 $7700.00 Window Closed / Lapsed