Abstract An arc welding method in which with a welding electrode being oscillated within the groove in the width direction thereof, the movement of the electrode in the upright or vertical direction is controlled to always maintain the arc length constant. The groove of a predetermined shape is subjected to arc welding with predetermined welding speed and wire feed speed so that when a half cycle of the electrode oscillation is completed, the height direction displacement of the electrode is integrated over the time to obtain a cross-sectional area S o described by the electrode and also an oscillation stroke X o made by the electrode is obtained, thus storing the cross-sectional area S o and the oscillation stroke X o . When the next half cycle is completed, a cross-sectional area S and an oscillation stroke X are similarly obtained so that the welding speed or the wire feed speed is controlled to vary and thereby to vary the cross-sectional area of metal deposition by an amount ΔS which is determined by the following equation ##EQU1## The deposition rate is controlled in accordance with the actual cross-sectional area of the groove and thus a weld bead of a uniform height or level is produced.
Inventors
👤 Hirokazu Nomura
👤 Yuji Sugitani
👤 Yasuo Suzuki
Bibliographic Details
Application Number—
JurisdictionUS
Data Sourcegoogle_patents
Last Synchronized2026-10-26 02:34
CPC Classifications
B; B23; B23K; B23K9/00; B23K9/02; B23K9/0216
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
173 words
In an arc welding method of the type in which while oscillating a welding electrode in a width direction within a groove of a pair of metals to be welded, the vertical movement of said electrode is controlled so as to always maintain an arc length constant, the improvement comprising the steps of: arc welding said groove of a predetermined shape by using a predetermined welding speed and wire feed speed; upon completion of a half cycle of oscillation of said electrode, integrating a vertical displacement of said electrode over a period of time to obtain a cross-sectional area S o described by said electrode and also obtaining an oscillation stroke x o of said electrode; storing said cross-sectional area S and said oscillation stroke in memory means; similarly obtaining a cross-sectional area S and an oscillation stroke x for the next half cycle of oscillation of said electrode; and varying a cross-sectional area of metal deposition by an amount ΔS given by ##EQU5## whereby providing a weld bead having a uniform level.
Claim 2
Dependent Claim
173 words
In an arc welding method of the type in which while oscillating a welding electrode in a width direction within a groove of a pair of metals to be welded, the vertical movement of said electrode is controlled so as to always maintain an arc length constant, the improvement comprising the steps of: arc welding said groove of a predetermined shape by using a predetermined welding speed and wire feed speed; upon completion of a half cycle of oscillation of said electrode, integrating a vertical displacement of said electrode over a period of time to obtain a cross-sectional area S o described by said electrode and also obtaining an oscillation stroke x o of said electrode; storing said cross-sectional area S and said oscillation stroke in memory means; similarly obtaining a cross-sectional area S and an oscillation stroke x for the next half cycle of oscillation of said electrode; and varying a cross-sectional area of metal deposition by an amount ΔS given by ##EQU5## whereby providing a weld bead having a uniform level.
Claim 3
Dependent Claim
54 words
An arc welding method according to claim 1, wherein the wire feed speed V f is maintained constant and the welding speed V is controlled in accordance with a relation ##EQU6## where A is a cross-sectional area of metal deposition obtained before controlling said welding speed V to vary, and C is a constant.
Claim 4
Dependent Claim
35 words
An arc welding method according to claim 2, wherein said welding speed V is controlled to vary, and wherein a welding current I is controlled to make the same proportional to said welding speed V.
Claim 5
Dependent Claim
52 words
An arc welding method according to claim 1, wherein the welding speed V is maintained constant, and the wire feed speed V f is increased in accordance with a relation ΔV f =V·C·ΔS, where C is a constant and ΔV f is an increment of said wire feed speed V f .
Claim 6
Dependent Claim
40 words
An arc welding method according to claim 4, wherein said wire feed speed V f is controlled to vary, and wherein a welding current I is controlled to make the same proportional to said wire feed speed V f .