Claims Analysis
Total Claims: 26
Claim 1
Independent Claim
140 words
In a no base hair relaxer composition comprising a continuous water phase having dispersed therein about 3 to about 50 weight percent oleaginous material, about 7 to about 25 percent by weight emulsifier and containing a water soluble organic base in sufficient quantity to provide a pH of said composition at about 12-14, wherein the improvement comprises said composition being stabilized against phase separation by about 2 to about 30 weight percent lipophilic, organically modified hectorite clay gellant comprised of hectorite modified with a quaternized nitrogen-containing compound containing at least one C 8 -C 20 long chain substituent on the quaternary nitrogen atom, propylene carbonate and an organic liquid, said weight percents being based upon the total weight of the composition, said oleaginous material, emulsifier and gellant together comprising no more than about 65 percent by weight of the composition.
Claim 2
Dependent Claim
140 words
In a no base hair relaxer composition comprising a continuous water phase having dispersed therein about 3 to about 50 weight percent oleaginous material, about 7 to about 25 percent by weight emulsifier and containing a water soluble organic base in sufficient quantity to provide a pH of said composition at about 12-14, wherein the improvement comprises said composition being stabilized against phase separation by about 2 to about 30 weight percent lipophilic, organically modified hectorite clay gellant comprised of hectorite modified with a quaternized nitrogen-containing compound containing at least one C 8 -C 20 long chain substituent on the quaternary nitrogen atom, propylene carbonate and an organic liquid, said weight percents being based upon the total weight of the composition, said oleaginous material, emulsifier and gellant together comprising no more than about 65 percent by weight of the composition.
Claim 3
Dependent Claim
33 words
The no base hair relaxer composition of claim 1 wherein said organic base is guanidine and is prepared just before use of said composition by the reaction of calcium hydroxide and guanidine carbonate.
Claim 4
Dependent Claim
181 words
In an emulsified composition suitable as a component of a no base hair relaxer composition and comprising a continuous water phase having dispersed therein about 3 to about 50 weight percent oleaginous material, about 7 to about 25 percent by weight emulsifier and containing a sufficient amount of an alkaline earth hydroxide to produce a pH between about 12 and about 14 when said composition is blended with an aqueous solution of the salt of a strong organic base with an anion capable of being precipitated by the ion of said alkaline earth, wherein the improvement comprises said composition being stabilized against phase separation by about 2 to about 30 weight percent lipophilic, organically modified hectorite clay gellant comprised of hectorite modified with a quaternized nitrogen containing compound containing at least one C 8 -C 20 long chain substituent on the quaternary nitrogen atom, propylene carbonate and an organic liquid, said weight percents being based upon the total weight of the composition, said oleaginous material, emulsifier and gellant together comprising no more than about 65 percent by weight of the composition.
Claim 5
Dependent Claim
181 words
In an emulsified composition suitable as a component of a no base hair relaxer composition and comprising a continuous water phase having dispersed therein about 3 to about 50 weight percent oleaginous material, about 7 to about 25 percent by weight emulsifier and containing a sufficient amount of an alkaline earth hydroxide to produce a pH between about 12 and about 14 when said composition is blended with an aqueous solution of the salt of a strong organic base with an anion capable of being precipitated by the ion of said alkaline earth, wherein the improvement comprises said composition being stabilized against phase separation by about 2 to about 30 weight percent lipophilic, organically modified hectorite clay gellant comprised of hectorite modified with a quaternized nitrogen containing compound containing at least one C 8 -C 20 long chain substituent on the quaternary nitrogen atom, propylene carbonate and an organic liquid, said weight percents being based upon the total weight of the composition, said oleaginous material, emulsifier and gellant together comprising no more than about 65 percent by weight of the composition.
Claim 6
Dependent Claim
29 words
The composition of claim 3 wherein said alkaline earth hydroxide is present in an amount from about 0.5 weight percent to about 20 weight percent of said emulsified composition.
Claim 7
Dependent Claim
26 words
The hair relaxer of claim 4 wherein said oleaginous material is selected from the group consisting of petrolatum, mineral jelly and mineral oil and mixtures thereof.
Claim 8
Dependent Claim
24 words
The hair relaxer of claim 4 wherein said emulsifier is selected from the group consisting of anionic, amphoteric and non-ionic emulsifiers and mixtures thereof.
Claim 9
Dependent Claim
50 words
The hair relaxer of claim 4 wherein said quaternized nitrogen-containing compound is selected from the group consisting of stearalkonium chloride and dimethyl-di-(hydrogenated tallow)ammonium chloride and said organic liquid is selected from the group consisting of mineral oil, castor oil, mineral spirits, and a mixture of lanolin oil and isopropyl palmitate.
Claim 10
Dependent Claim
37 words
The hair relaxer of claim 4 wherein said emulsifier comprises about 0.25 to about 10 weight percent 2-heptadecyl-1-carboxymethyl-1-(2-hydroxyethyl)-2-imidazolinium chloride and about 0.05 to about 8 weight percent of a quaternary polymer prepared by polymerizing a diallyldimethylammonium salt.
Claim 11
Dependent Claim
190 words
In a no-base hair relaxer composition comprising a continuous water phase having dispersed therein about 3 to about 50 weight percent oleaginous material selected from the group consisting of petrolatum, mineral jelly and mineral oil; about 7 to about 25 weight percent emulsifier selected from the group consisting of anionic, amphoteric and non-ionic emulsifiers; about 0.25 to about 20 weight percent of calcium hydroxide, said composition having a pH of about 12 to about 14 when blended with an aqueous solution of guanidine carbonate; wherein the improvement comprises said composition being stabilized against phase separation by about 2 to about 30 weight percent of a lipophilic modified hectorite clay gellant comprised of hectorite modified by propylene carbonate, a quaternized nitrogen containing compound selected from the group consisting of stearalkonium chloride and dimethyl-di-(hydrogenated tallow) ammonium chloride and an organic liquid selected from the group consisting of mineral oil, castor oil, mineral spirits and a mixture of lanolin and isopropyl palmitate; said weight percents being based upon the total weight of said composition, and said oleaginous material, emulsifier and gellant together comprising no more than about 65 weight percent of said composition.
Claim 12
Dependent Claim
190 words
In a no-base hair relaxer composition comprising a continuous water phase having dispersed therein about 3 to about 50 weight percent oleaginous material selected from the group consisting of petrolatum, mineral jelly and mineral oil; about 7 to about 25 weight percent emulsifier selected from the group consisting of anionic, amphoteric and non-ionic emulsifiers; about 0.25 to about 20 weight percent of calcium hydroxide, said composition having a pH of about 12 to about 14 when blended with an aqueous solution of guanidine carbonate; wherein the improvement comprises said composition being stabilized against phase separation by about 2 to about 30 weight percent of a lipophilic modified hectorite clay gellant comprised of hectorite modified by propylene carbonate, a quaternized nitrogen containing compound selected from the group consisting of stearalkonium chloride and dimethyl-di-(hydrogenated tallow) ammonium chloride and an organic liquid selected from the group consisting of mineral oil, castor oil, mineral spirits and a mixture of lanolin and isopropyl palmitate; said weight percents being based upon the total weight of said composition, and said oleaginous material, emulsifier and gellant together comprising no more than about 65 weight percent of said composition.
Claim 13
Dependent Claim
62 words
The hair relaxer of claim 9 wherein said oleaginous material is present at about 15 to about 25 weight percent and is a petrolatum-mineral oil mixture containing at least about 80 weight percent petrolatum; said lipophilic hectorite gellant is present at about 8 to about 20 weight percent; and said calcium hydroxide is present at about 5 to about 10 weight percent.
Claim 14
Dependent Claim
57 words
The hair relaxer of claim 10 wherein said emulsifier is comprised of about 7 to about 16 weight percent C 12 -C 18 fatty alcohols, about 0.5 to about 12 weight percent polyoxyethylene (75) lanolin, about 0.05 to about 1.5 weight percent polyoxyethylene (20) oleyl ether phosphate, and about 1 to about 10 weight percent propylene glycol.
Claim 15
Dependent Claim
25 words
The hair relaxer of claim 9 additionally comprising about 0.5 to about 2 weight percent of a quaternary homopolymer prepared by polymerizing a diallyldimethylammonium salt.
Claim 16
Dependent Claim
60 words
The hair relaxer of claim 12 wherein said oleaginous material comprises a petrolatum-mineral oil mixture containing at least about 80 weight percent petrolatum and is present at about 15 to about 25 weight percent; said calcium hydroxide is present at about 5 to about 10 weight percent; and said emulsifier comprises about 0.25 to about 5 weight percent 2-heptadecyl-1-carboxymethyl-1-(2-hydroxyethyl)-2-imidazolinium chloride.
Claim 17
Dependent Claim
55 words
The hair relaxer of claim 13 wherein said emulsifier comprises about 7 to about 16 weight percent C 12 -C 18 fatty alcohols, about 0.05 to about 1.5 weight percent polyoxyethylene (3) oleyl ether phosphate, about 1 to about 10 weight percent propylene glycol, and about 0.5 to about 12 weight percent polyoxyethylene (75) lanolin.
Claim 18
Independent Claim
264 words
A method of preparing an emulsified composition stable against phase separation and capable of producing a hair relaxer upon admixture with an aqueous solution of guanidine carbonate comprising the steps of: (A) heating and agitating a mixture of about 3 to about 50 weight percent of an oleaginous material and about 2 to about 30 weight percent of lipophilic modified hectorite clay gellant comprised of hectorite modified with a quaternized nitrogen-containing compound containing at least one C 8 -C 20 long chain substituent on the quaternary nitrogen atom at about 80° C. until a substantially uniform dispersion results, said weight percents being based upon the total weight of the composition; (B) admixing emulsifying agents of low water solubility thereto while maintaining said agitation and temperature to thereby form the oil phase of said composition; (C) heating and agitating water, calcium hydroxide and emulsifiers of high water solubility in a separate container at about 80° C. to thereby form the bulk of the aqueous phase of said composition, all of said emulsifiers comprising about 7 to about 25 weight percent of said composition; and said emulsifiers, oleaginous material and gellant together comprising no more than about 65 percent by weight of said composition; (D) slowly admixing said bulk of the aqueous phase into said oil phase at about 80° C.; (E) thereafter mixing said admixture for about 15 minutes; (F) cooling said admixture to about 50° C. and adding perfume; (G) thereafter mixing said composition for about 15 minutes, and then force cooling said composition to about 25° C.; and H. homogenizing said cooled composition.
Claim 19
Independent Claim
264 words
A method of preparing an emulsified composition stable against phase separation and capable of producing a hair relaxer upon admixture with an aqueous solution of guanidine carbonate comprising the steps of: (A) heating and agitating a mixture of about 3 to about 50 weight percent of an oleaginous material and about 2 to about 30 weight percent of lipophilic modified hectorite clay gellant comprised of hectorite modified with a quaternized nitrogen-containing compound containing at least one C 8 -C 20 long chain substituent on the quaternary nitrogen atom at about 80° C. until a substantially uniform dispersion results, said weight percents being based upon the total weight of the composition; (B) admixing emulsifying agents of low water solubility thereto while maintaining said agitation and temperature to thereby form the oil phase of said composition; (C) heating and agitating water, calcium hydroxide and emulsifiers of high water solubility in a separate container at about 80° C. to thereby form the bulk of the aqueous phase of said composition, all of said emulsifiers comprising about 7 to about 25 weight percent of said composition; and said emulsifiers, oleaginous material and gellant together comprising no more than about 65 percent by weight of said composition; (D) slowly admixing said bulk of the aqueous phase into said oil phase at about 80° C.; (E) thereafter mixing said admixture for about 15 minutes; (F) cooling said admixture to about 50° C. and adding perfume; (G) thereafter mixing said composition for about 15 minutes, and then force cooling said composition to about 25° C.; and H. homogenizing said cooled composition.
Claim 20
Dependent Claim
97 words
The method of claim 15 wherein said oleaginous material is selected from the group consisting of mineral oil, petrolatum and mineral jelly and mixtures thereof; said lipophilic modified hectorite clay gellant is a hectorite modified with propylene carbonate, a quaternized nitrogen-containing compound selected from the group consisting of stearalkonium chloride and dimethyl-di-(hydrogenated tallow)-ammonium chloride, and an organic liquid selected from the group consisting of mineral oil, castor oil, mineral spirits and a mixture of lanolin oil and isopropyl palmitate; and said emulsifiers are selected from the group consisting of anionic, amphoteric and non-ionic emulsifiers and mixtures thereof.
Claim 21
Dependent Claim
40 words
The method of claim 15 wherein the bulk of said aqueous phase comprises about 0.25 to about 10 weight percent 2-heptadecyl-carboxymethyl-1-(2-hydroxyethyl)-2-imidazolinium chloride; and about 0.05 to about 8 weight percent of a quaternary polymer prepared by polymerizing a diallyldimethylammonium salt.
Claim 22
Independent Claim
309 words
A method of preparing an emulsified composition stable against phase separation and capable of producing a hair relaxer upon admixture with an aqueous solution of guanidine carbonate comprising the steps of: (A) heating and agitating a mixture of about 3 to about 50 weight percent of an oleaginous material selected from the group consisting of petrolatum, mineral oil and mineral jelly, and about 2 to about 30 weight percent lipophilic modified hectorite clay gellant comprising hectorite modified with propylene carbonate, a quaternized nitrogen-containing compound selected from the group consisting of stearalkonium chloride and dimethyl-di-(hydrogenated tallow)ammonium chloride, and an organic liquid selected from the group consisting of mineral oil, castor oil, mineral spirits and a mixture of lanolin oil and isopropyl palmitate, at about 80° C. until a substantially uniform dispersion results, said weight percents being based upon the weight of said composition. (B) admixing emulsifying agents of low water solubility thereto while maintaining said agitation and temperature to thereby form the oil phase of said composition; (C) heating and agitating water, calcium hydroxide and emulsifiers of high water solubility in a separate container at about 80° C. to thereby form the bulk portion of the aqueous phase of said composition, all of said emulsifiers comprising about 7 to about 25 weight percent of said composition, and being selected from the group consisting of anionic, amphoteric and non-ionic emulsifiers, said emulsifiers, oleaginous material and gellant together comprising no more than about 65 weight percent of said composition; (D) slowly admixing said bulk portion of the aqueous phase into said oil phase at about 80° C.; (E) thereafter mixing said admixture for about 15 minutes; (F) cooling said admixture to about 50° C. and adding perfume; (G) thereafter mixing said composition for about 15 minutes, and then force cooling said composition to about 25° C.; and (H) homogenizing said cooled composition.
Claim 23
Independent Claim
309 words
A method of preparing an emulsified composition stable against phase separation and capable of producing a hair relaxer upon admixture with an aqueous solution of guanidine carbonate comprising the steps of: (A) heating and agitating a mixture of about 3 to about 50 weight percent of an oleaginous material selected from the group consisting of petrolatum, mineral oil and mineral jelly, and about 2 to about 30 weight percent lipophilic modified hectorite clay gellant comprising hectorite modified with propylene carbonate, a quaternized nitrogen-containing compound selected from the group consisting of stearalkonium chloride and dimethyl-di-(hydrogenated tallow)ammonium chloride, and an organic liquid selected from the group consisting of mineral oil, castor oil, mineral spirits and a mixture of lanolin oil and isopropyl palmitate, at about 80° C. until a substantially uniform dispersion results, said weight percents being based upon the weight of said composition. (B) admixing emulsifying agents of low water solubility thereto while maintaining said agitation and temperature to thereby form the oil phase of said composition; (C) heating and agitating water, calcium hydroxide and emulsifiers of high water solubility in a separate container at about 80° C. to thereby form the bulk portion of the aqueous phase of said composition, all of said emulsifiers comprising about 7 to about 25 weight percent of said composition, and being selected from the group consisting of anionic, amphoteric and non-ionic emulsifiers, said emulsifiers, oleaginous material and gellant together comprising no more than about 65 weight percent of said composition; (D) slowly admixing said bulk portion of the aqueous phase into said oil phase at about 80° C.; (E) thereafter mixing said admixture for about 15 minutes; (F) cooling said admixture to about 50° C. and adding perfume; (G) thereafter mixing said composition for about 15 minutes, and then force cooling said composition to about 25° C.; and (H) homogenizing said cooled composition.
Claim 24
Dependent Claim
46 words
The method of claim 18 wherein said emulsifier of high water solubility includes about 0.25 to about 5 weight percent 2-heptadecyl-1-carboxymethyl-1-(2-hydroxyethyl)-2-imidazolinium chloride and said composition is also comprised of about 0.5 to about 2 weight percent of a quaternary polymer prepared by polymerizing a diallyldimethylammonium salt.
Claim 25
Dependent Claim
45 words
In the method of treating human hair with a no-base relaxer composition in which the relaxer is applied to the hair, the hair physically smoothed, rinsed, shampooed, set and dried, the improvement which comprises using as the relaxer the hair relaxer composition of claim 1.
Claim 26
Dependent Claim
45 words
In the method of treating human hair with a no-base relaxer composition in which the relaxer is applied to the hair, the hair physically smoothed, rinsed, shampooed, set and dried, the improvement which comprises using as the relaxer the hair relaxer composition of claim 2.