US4386986A Expired / Lapsed US ⏱️ 0.0 years remaining

High power laser mirror repair

Assignee: RTX Corp
•
Filing: 1981-04-06
•
Granted: 1983-06-07
•
Expires: 2001-04-06
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of bonding a laser mirror faceplate to a substrate involves the use of chemical vapor deposition within coolant passages 12 to form a mechanically strong bond 28 between the faceplate 10 and the substrate 16. The method may also be used for the repair of disbonded sections of laser mirrors without disassembling the faceplate from the substrate.

Inventors

  • 👤 John H. Bluege

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 15:44
CPC Classifications
G; G02; G02B; G02B7/00; G02B7/18; G02B7/181; G02B7/1815; C; C23; C23C; C23C16/00; C23C16/04; C23C16/045; H; H01; H01S; H01S3/00; H01S3/05; H01S3/08; H01S3/08059; Y; Y10; Y10S; Y10S359/00; Y10S359/90; Y10T; Y10T29/00; Y10T29/49; Y10T29/49718; Y10T29/49746

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 158 words
A method of bonding first and second members of a cooled mirror for high power lasers comprising the steps of: placing a first member, having a first bonding surface including a plurality of coolant channels having channel surfaces, said channels being separated by land members having land surfaces disposed toward said second member, said coolant surfaces and said land surfaces together comprising a portion of said first bonding surface, in close proximity with a second member having a second bonding surface with portions of said second bonding surface disposed with a predetermined relationship to said land surfaces; passing a bonding medium of predetermined composition only through said plurality of coolant channels; and depositing a bonding chemical from said bonding medium on portions of said first bonding surface and second bonding surface, said bonding chemical being chemically and thermally compatible with said first and second members, in sufficient amount to form a bond joining said first and second members.
Claim 2
Independent Claim 158 words
A method of bonding first and second members of a cooled mirror for high power lasers comprising the steps of: placing a first member, having a first bonding surface including a plurality of coolant channels having channel surfaces, said channels being separated by land members having land surfaces disposed toward said second member, said coolant surfaces and said land surfaces together comprising a portion of said first bonding surface, in close proximity with a second member having a second bonding surface with portions of said second bonding surface disposed with a predetermined relationship to said land surfaces; passing a bonding medium of predetermined composition only through said plurality of coolant channels; and depositing a bonding chemical from said bonding medium on portions of said first bonding surface and second bonding surface, said bonding chemical being chemically and thermally compatible with said first and second members, in sufficient amount to form a bond joining said first and second members.
Claim 3
Dependent Claim 26 words
A method according to claim 1, in which said bonding chemical is deposited from a chemical vapor bonding medium by the process of chemical vapor deposition.
Claim 4
Dependent Claim 64 words
A method according to either claim 1 or claim 2, in which the deposition of said chemical is restricted to predetermined portions of said first and second bonding surfaces by means of a further step of applying a barrier coating, before said step of passing said medium, to those portions of said first and second bonding surfaces for which chemical deposition is not desired.
Claim 5
Independent Claim 185 words
A method of repairing a partially disbonded cooled mirror consisting of first and second members, said first member, having a first bonding surface including a plurality of coolant channels having channel surfaces, said channels being separated by land members having land surfaces disposed toward said second member, said coolant surfaces and said land surfaces together comprising a portion of said first bonding surface and a second member, in close proximity with said first member and having a second bonding surface with portions of said second bonding surface disposed with a predetermined relationship to said land surfaces; a portion of said first and second bonding surfaces being separated in a disbond area traversed by a plurality of disbond coolant channels, comprising the steps of: passing a bonding medium of predetermined composition only through said plurality of disbond coolant channels; and depositing a bonding chemical from said bonding medium on portions of said first bonding surface and second bonding surface, said bonding chemical being chemically and thermally compatible with said first and second members, in sufficient amount to form a bond joining said first and second members.
Claim 6
Independent Claim 185 words
A method of repairing a partially disbonded cooled mirror consisting of first and second members, said first member, having a first bonding surface including a plurality of coolant channels having channel surfaces, said channels being separated by land members having land surfaces disposed toward said second member, said coolant surfaces and said land surfaces together comprising a portion of said first bonding surface and a second member, in close proximity with said first member and having a second bonding surface with portions of said second bonding surface disposed with a predetermined relationship to said land surfaces; a portion of said first and second bonding surfaces being separated in a disbond area traversed by a plurality of disbond coolant channels, comprising the steps of: passing a bonding medium of predetermined composition only through said plurality of disbond coolant channels; and depositing a bonding chemical from said bonding medium on portions of said first bonding surface and second bonding surface, said bonding chemical being chemically and thermally compatible with said first and second members, in sufficient amount to form a bond joining said first and second members.
Claim 7
Dependent Claim 26 words
A method according to claim 4, in which said bonding chemical is deposited from a chemical vapor bonding medium by the process of chemical vapor deposition.

References Cited (Backward Citations)

US3841737A Cited
SU518315A1 Cited
US4042163A Cited
US4314742A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-06-06 1986-12-06 1987-06-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-06-06 1990-12-06 1991-06-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-06-06 1994-12-06 1995-06-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag