US4385804A Expired / Lapsed US ⏱️ 0.0 years remaining

Mirror using transparent synthetic resin plate

Assignee: Marui Industrial Co Ltd
•
Filing: 1981-04-17
•
Granted: 1983-05-31
•
Expires: 2001-04-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A mirror which utilizes a transparent synthetic resin such as a polymethyl methacrylate resin in place of glass and is suitable, e.g., as an automobile inside rearview mirror. The back side of the resin plate is coated with a reflective metal film by vacuum deposition, and at least the front side of the resin plate is coated with a surface-hardening film, which is inevitably somewhat permeable to humidity. To prevent warping of the resin plate resulting from its moisture absorption and swelling only in its front region, the reflective film and a back-coat layer covering this film are both made permeable to humidity substantially equally to the surface-hardening film. Preferred material for the reflective film is a Sn--Cu--Cr ternary alloy having high reflectivity and excellent resistance to moisture.

Inventors

  • 👤 Takeo Tamura
  • 👤 Taiji Yamabe

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 08:40
CPC Classifications
G; G02; G02B; G02B5/00; G02B5/08; G02B5/0816; G02B5/0825; G02B5/0841; B; B29; B29D; B29D11/00; B29D11/00596; B60; B60R; B60R1/00; B60R1/02; C; C23; C23C; C23C14/00; C23C14/06; C23C14/14; C23C14/20; G02B1/00; G02B1/10; G02B1/105; G02B1/14; G02B27/00; G02B27/0006; G02B5/0808

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 72 words
A mirror comprising: a transparent plate of a synthetic resin; a surface-hardening film coated at least on a front surface of the resin plate; a reflective film of a metal resistant to moisture deposited on the back side of the resin plate; and a back-coat layer closely covering the outer surface of the reflective film, the surface-hardening film, the reflective film and the back-coat layer being all substantially equally permeable to humidity.
Claim 2
Dependent Claim 72 words
A mirror comprising: a transparent plate of a synthetic resin; a surface-hardening film coated at least on a front surface of the resin plate; a reflective film of a metal resistant to moisture deposited on the back side of the resin plate; and a back-coat layer closely covering the outer surface of the reflective film, the surface-hardening film, the reflective film and the back-coat layer being all substantially equally permeable to humidity.
Claim 3
Dependent Claim 34 words
A mirror according to claim 1, wherein said metal is a ternary alloy composed of 100 parts of Sn, 15 to 150 parts of Cu and 5 to 50 parts of Cr, by weight.
Claim 4
Dependent Claim 31 words
A mirror according to claim 2, wherein said reflective film is formed by vacuum deposition of said ternary alloy and has a thickness in the range from 0.025 to 0.10 microns.
Claim 5
Dependent Claim 21 words
A mirror according to claim 3, wherein said thickness is in the range from about 0.05 microns to about 0.06 microns.
Claim 6
Dependent Claim 15 words
A mirror according to claim 1, wherein said synthetic resin is a polymethyl methacrylate resin.
Claim 7
Dependent Claim 17 words
A mirror according to claim 1, wherein said surface-hardening film is formed essentially of an organosilicon polymer.
Claim 8
Dependent Claim 20 words
A mirror according to claim 1, wherein the entire surfaces of the resin plate are coated with said surface-hardening film.
Claim 9
Dependent Claim 24 words
A mirror according to claim 1, wherein said back-coat layer is a resin layer containing dispersed therein an inorganic filler material in powder form.
Claim 10
Dependent Claim 26 words
A mirror according to claim 1, wherein the front and back surfaces of the resin plate are both flat surfaces but are unparallel to each other.

References Cited (Backward Citations)

DE2423654A1 Cited
DE2923954A1 Cited
US4193668A Cited
DE2945780A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-05-30 1986-11-29 1987-05-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-05-30 1990-11-29 1991-05-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-05-30 1994-11-29 1995-05-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag