Paper-coating compositions

Assignee: BASF SE
•
Filing: 1981-08-31
•
Granted: 1983-05-17
•
Expires: 2001-08-31
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improved paper-coating composition which contains, per 100 parts by weight of a finely divided pigment, from 5 to 25 parts by weight of a copolymer A, in the form of an aqueous dispersion, as a binder, and from 0.5 to 10 parts by weight of a copolymer B, containing (a) from 20 to 70% by weight of copolymerized units of hydroxy-C2-C4-alkyl acrylates or hydroxy-C2-C4-alkyl methacrylates, (b) from 10 to 50% by weight of copolymerized units of acrylic acid, methacrylic acid, maleic acid and/or monoesters of maleic acid and (c) from 5 to 50% by weight of copolymerized units of acrylonitrile, methacrylonitrile, C1-C4-alkyl acrylates of C1-C4-alkyl methacrylates, or vinyl esters of saturated C2-C4-carboxylic acids as the co-binder, with or without from 0.1 to 2.0 parts by weight of an optical brightener which is activated by the co-binder. The paper-coating composition has high water retention.

Inventors

  • 👤 Kurt Wendel
  • 👤 Gunter Hirsch

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 17:27
CPC Classifications
D; D21; D21H; D21H19/00; D21H19/36; D21H19/44; D21H19/56; D21H19/58; D21H19/60

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 183 words
A paper coating composition which contains, 100 parts by weight of a finely divided pigment, from 5 to 25 parts by weight of a copolymer A having a glass transition temperature of from -40° to +50° C., in the form of an aqueous dispersion, and from 0.5 to 10 parts by weight of one or more high molecular weight-containing copolymers B, wherein the improvement comprises using, as the copolymer B a copolymer having a K value of 60-140, which is prepared by solution copolymerization, and which contains: (a) from 20 to 70% by weight of copolymerized units of hydroxy-C 2 -C 4 -alkyl acrylates or hydroxy-C 2 -C 4 -alkyl methacrylates; (b) from 10 to 50% by weight of copolymerized units of compounds selected from the group comprising acrylic acid, methacrylic acid, maleic acid and monoesters of maleic acid; and (c) from 5 to 50% by weight of copolymerized units of compounds selected from the group comprising acrylonitrile, methacrylonitrile, C 1 -C 4 -alkyl acrylates or C 1 -C 4 -alkyl methacrylates, or vinyl esters of saturated C 2 -C 4 -carboxylic acids.
Claim 2
Dependent Claim 183 words
A paper coating composition which contains, 100 parts by weight of a finely divided pigment, from 5 to 25 parts by weight of a copolymer A having a glass transition temperature of from -40° to +50° C., in the form of an aqueous dispersion, and from 0.5 to 10 parts by weight of one or more high molecular weight-containing copolymers B, wherein the improvement comprises using, as the copolymer B a copolymer having a K value of 60-140, which is prepared by solution copolymerization, and which contains: (a) from 20 to 70% by weight of copolymerized units of hydroxy-C 2 -C 4 -alkyl acrylates or hydroxy-C 2 -C 4 -alkyl methacrylates; (b) from 10 to 50% by weight of copolymerized units of compounds selected from the group comprising acrylic acid, methacrylic acid, maleic acid and monoesters of maleic acid; and (c) from 5 to 50% by weight of copolymerized units of compounds selected from the group comprising acrylonitrile, methacrylonitrile, C 1 -C 4 -alkyl acrylates or C 1 -C 4 -alkyl methacrylates, or vinyl esters of saturated C 2 -C 4 -carboxylic acids.
Claim 3
Dependent Claim 54 words
An improved paper-coating composition as claimed in claim 1, wherein copolymer B contains (a) from 30 to 55% by weight of hydroxypropyl acrylate units, (b) from 15 to 40% by weight of acrylic acid or methacrylic acid units and (c) from 20 to 40% by weight of acrylonitrile, methyl acrylate and/or ethyl acrylate units.
Claim 4
Dependent Claim 22 words
An improved paper-coating composition as claimed in claim 1, which contains from 0.1 to 2.0 parts by weight of an optical brightener.

References Cited (Backward Citations)

US3892675A Cited
US3985698A Cited
US4102843A Cited
US4157995A Cited
US4258104A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-05-16 1986-11-15 1987-05-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-05-16 1990-11-15 1991-05-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-05-16 1994-11-15 1995-05-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag