Abstract

Abstract A paper printing ink is disclosed composed of a pigment, an alkyd resin binder modified with a long-chain fatty acid and which optionally contains conventional components, such as, lubricants, solvents, and viscosity modifiers, wherein the alkyd resin is a non-drying resin modified with oils, fatty acids, or fatty alcohols having an iodine number less than about 20. The inks of the present invention possess good printability properties and pigment wetting capability. This results in high gloss abrasion-resistant printing films which are free from contact yellowing and odor formation. Moreover, the inks of the present invention can be readily removed from the paper, thereby facilitating recycling of the paper. Methods for utilizing the inks as well as products printed with the inks are disclosed.

Inventors

  • 👤 Albert Uhlemayr
  • 👤 Heinrich Traitteur

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 07:42
CPC Classifications
C; C09; C09D; C09D11/00; C09D11/02; C09D11/10; C09D11/102; C09D11/104; C09D11/105; Y; Y10; Y10S; Y10S260/00; Y10S260/38

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 74 words
In a method for printing paper wherein ink is applied to paper using the offset printing process, the improvement which comprises said ink being composed of pigment, an alkyd resin binder, wherein the alkyd resin is non-drying and has a weight average molecular weight (M w ) of from 12,000 to 22,000 and is modified with oils, fatty acids or fatty alcohols with an iodine number less than about 20 and additional conventional additives.
Claim 2
Dependent Claim 74 words
In a method for printing paper wherein ink is applied to paper using the offset printing process, the improvement which comprises said ink being composed of pigment, an alkyd resin binder, wherein the alkyd resin is non-drying and has a weight average molecular weight (M w ) of from 12,000 to 22,000 and is modified with oils, fatty acids or fatty alcohols with an iodine number less than about 20 and additional conventional additives.
Claim 3
Dependent Claim 14 words
The method of claim 1 wherein the alkyd resin is modified with coconut oil.
Claim 4
Dependent Claim 20 words
The method of claim 1 or 2 wherein the alkyd resin has a corrected OH number greater than about 10.
Claim 5
Dependent Claim 20 words
The method of claim 1 or 2 wherein the alkyd resin has a corrected OH number greater than about 15.
Claim 6
Dependent Claim 24 words
The method of claim 1 or 2 wherein the alkyd resin has a corrected OH number in the range from about 20 to 35.
Claim 7
Dependent Claim 32 words
The method of claim 1 or 2 wherein the non-drying alkyd resin has a viscosity in the range from 2000 dPa X sec (20° C.) to the consistency of a solid resin.
Claim 8
Dependent Claim 19 words
The method of claim 1 or 2 wherein the alkyd resin has an acid number less than about 25.
Claim 9
Dependent Claim 20 words
The method of claim 1 or 2 wherein the alkyd resin has an acid number from about 6 to 12.
Claim 10
Dependent Claim 25 words
The method of claim 1 or 2 wherein the alkyd resin has a weight average molecular weight (M w ) of from 9000 to 30,000.
Claim 11
Dependent Claim 24 words
The method of claim 1 or 2 wherein the alkyd resin has a number average molecular weight (M n ) of 3000 to 5000.
Claim 12
Dependent Claim 25 words
The method of claim 1 or 2 wherein the alkyd resin has a number average molecular weight (M n ) of about 3500 to 4500.
Claim 13
Dependent Claim 25 words
The method of claim 1 or 2 wherein the alkyd resin as a dispersion factor (M w /M n ) of from 3 to 6.
Claim 14
Dependent Claim 25 words
The method of claim 1 or 2 wherein the alkyd resin has a dispersion factor (M w /M n ) of from 3.5 to 5.
Claim 15
Dependent Claim 27 words
The method of claim 1 or 2 wherein the amount of modifier in the alkyd resin is in the range from about 40 to 70 weight percent.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-05-16 1986-11-15 1987-05-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-05-16 1990-11-15 1991-05-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-05-16 1994-11-15 1995-05-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag